Use full-wave rectification for routine flaw detection because it combines positive and negative RF lobes on one positive baseline, while RF preserves phase information required for thin specimens, boundary analysis, and signal-origin diagnosis [S1][S2].
The decision is based on information content, threshold behavior, and inspection purpose: RF shows the received waveform with both half-waves, whereas full-wave rectification simplifies amplitude interpretation but removes direct visibility of echo polarity [S1][S2][S5].
Display Modes and Signal Content
A conventional A-scan places received signal amplitude on the vertical axis and ultrasonic travel time on the horizontal axis. In linear amplification, vertical excursion is proportional to signal amplitude; logarithmic amplification presents amplitude on a logarithmic scale [S5]. The A-scan may show unrectified RF, positive half-wave, negative half-wave, full-wave rectified, or filtered rectified information [S1][S2][S4][S5].
RF retains both positive and negative waveform peaks. Positive half-wave rectification keeps positive peaks, negative half-wave rectification keeps negative peaks and flips them above the baseline, and full-wave rectification displays both lobes above the baseline [S1][S2]. These transformations are display operations: the underlying received echo still contains the waveform information unless the instrument stores only a processed representation.
RF Versus Full-Wave: Decision Matrix
RF provides the highest diagnostic information of these two modes because phase and polarity remain visible, but it requires more careful interpretation because multiple signals, back-wall skips, water-path effects, and wave conversion can appear as complex waveforms [S2][S5]. Full-wave rectification reduces that interpretive burden, presents both echo lobes as positive amplitude, and is the common format for general flaw detection [S1].
Recommended Display by Inspection Objective

Use RF as the starting mode when diagnosing a weak, complex, or unexpected echo, particularly on thin test pieces or when phase and polarity determine whether a signal originated at a boundary, interface, or flaw. An RF display is necessary for investigation of signal phase shift, such as at boundaries [S5]. It is also required when investigating signal phase shift, including boundary-related behavior [S5].
Use full-wave rectification for routine flaw detection, amplitude evaluation, and gate positioning when the objective is to identify and measure an echo without interpreting the signs of its individual lobes [S1]. This is the practical default for many inspections, but it should not replace RF when the suspected mechanism depends on waveform polarity.
For precise thickness work, half-wave positive or half-wave negative mode can be more suitable because measurements are made consistently on lobes of the same polarity. One experienced NDT discussion specifies an illustrative resolution distinction: full-wave may be acceptable when a measurement requirement of about 0.005 to 0.010 in is immaterial, while pen-probe or small-diameter high-frequency work benefits from half-wave mode [S1]. These values illustrate the principle rather than establish a universal acceptance criterion.
Limits, Failure Modes, and Interpretation Traps
The main failure mode of full-wave display is false simplification. Once positive and negative lobes are combined above the baseline, the operator cannot tell which lobe crossed a threshold, making it impossible to distinguish their polarity directly [S1]. This can mask phase relationships and make a complex waveform appear to be a single echo.
The main limitation of RF display is interpretive complexity. Echoes may overlap, multiple signals may be present, back-wall skips may occur, and wave conversion may alter the observed signal. RF therefore benefits from digital functions such as averaging, echo filtering, maximum hold, and a frozen A-scan [S5]. These functions improve readability, but they do not justify ignoring the raw waveform when phase is diagnostically important.
Half-wave rectification can reduce spurious peaks in some setups and thereby improve signal-to-noise, while full-wave processing combines both lobes rather than selecting one polarity [S1][S2]. Do not treat this as a guaranteed improvement: the usable result still depends on transducer selection, pulse width, damping, gain, filtering, and the material under test. Evident lists typical pulser voltages of 100–400 V or greater and PRF values from 10–1000 Hz or greater [S2].
Instrument Workflow and Data Reuse

A defensible inspection workflow starts in RF, identifies the meaningful lobe and any phase shift, selects the appropriate rectification mode, and then calibrates the gate and amplitude criteria on a consistent waveform [S1]. Full-wave is a processed display, not a different ultrasonic frequency and not an alternative to the RF acquisition.
Digital storage can separate acquisition from presentation. This capability supports review of RF-to-rectified display choices without requiring a second scan, provided the original RF data were acquired and retained.
For broader inspection workflows, an ultrasonic flaw detector may also produce B-scan and C-scan views. B-scan records echo depth along a scan line, while C-scan maps indication amplitude over an area, but neither replaces the A-scan waveform when phase or polarity determines the diagnosis [S6].
Document the selected mode, probe, pulse width or frequency, damping, gain, filter, threshold, and calibration reference for every data set. Before final acceptance, reproduce the stored A-scan in both RF and full-wave form where the equipment permits, and verify that the selected gate follows the intended lobe rather than an unrelated crossing [S1][S3].