REQUEST FOR QUOTE → Request a quote
SpecForge Editorial Team

ESD vs EN ISO 20345 Antistatic A-Marking: Resistance Ranges Compared

Table of Contents
  1. Antistatic A Marking Under EN ISO 20345
  2. ESD Resistance Band Under EN 61340-4-3:2018
  3. Decision Matrix: Antistatic A vs ESD for Specific Roles
  4. Who Each Type Is For, and Who It Is Not For
  5. Failure Modes and Common Specification Errors
  6. Standards and Sourcing Reference
ESD vs EN ISO 20345 Antistatic A-Marking: Resistance Ranges Compared

EN ISO 20345 antistatic (A marking) safety footwear is specified with a contact resistance between 100 kΩ and 1,000 MΩ, while ESD-rated footwear tightens that band to 0.1–100 MΩ under EN 61340-4-3:2018 [S2][S5]. The two are not different technologies; ESD is the stricter sub-range of the same dissipative family, defined by the electronics protection standard rather than by EN ISO 20345.

The distinction matters at the procurement stage: A-marked antistatic footwear is mandatory from class S1 upward, whereas ESD-marked footwear is specified by EPA programme owners who need controlled charge decay to protect components sensitive to discharges as low as 100 V [S4][S8].

Antistatic A Marking Under EN ISO 20345

EN ISO 20345 divides all safety footwear into three electrical classes: conductive (below 100 kΩ), antistatic (A), and electrically insulating (above 1,000 MΩ) [S1]. The antistatic A marking covers contact resistance from 1×10⁵ Ω to 1×10⁹ Ω, measured per EN ISO 20344 [S4]. This 100 kΩ lower bound prevents the footwear from being too conductive, which would otherwise expose the wearer to mains-frequency shock, while the 1,000 MΩ upper bound still bleeds off body charge fast enough to prevent spark ignition in flammable atmospheres [S1][S2].

Footwear of class S1, S2, S3, S4, S5, S6, and S7 under EN ISO 20345 must meet the antistatic requirement by default; only SB (basic) rated shoes may omit the A marking [S4][S8]. The resistance test itself is conducted on a conditioned sample with a defined contact pressure, voltage and humidity envelope defined in EN ISO 20344, not the more stringent EN 61340-4-3:2018 protocol used for true ESD certification [S4][S5].

ESD Resistance Band Under EN 61340-4-3:2018

ESD (Electrostatic Dissipative) safety footwear is tested to BS EN IEC 61340-4-3:2018 and must sit between 0.1 MΩ and 100 MΩ (1×10⁵ to 1×10⁸ Ω) [S5]. That narrower window is a deliberate carve-out of the lower part of the EN ISO 20345 antistatic range, where the resistance is low enough to suppress human-body-model events capable of damaging HBM Class 1A devices but not so low as to bypass the dissipative decay profile an EPA floor is engineered for [S2][S5].

Some manufacturers, including Rock Fall, voluntarily test to a tighter internal ceiling of 35 MΩ carried over from EN 61340-5-1:2007, even though the current 2018 standard permits up to 100 MΩ [S4]. In practice, the 100 MΩ cap is the published acceptance limit, and pair-to-floor system resistance (shoe plus sole plus floor plus grounding) is what an EPA auditor measures, not the shoe alone [S4][S7].

Decision Matrix: Antistatic A vs ESD for Specific Roles

ESD footwear vs EN ISO 20345 antistatic A marking resistance ranges - Decision Matrix: Antistatic A vs ESD for Specific Roles
ESD footwear vs EN ISO 20345 antistatic A marking resistance ranges - Decision Matrix: Antistatic A vs ESD for Specific Roles

Use the A marking when the hazard is spark ignition of a flammable atmosphere and the operator does not touch ESD-sensitive devices. The 100 kΩ–1,000 MΩ band meets EN ISO 20345 and is the default for S1–S7 footwear, costing no premium over standard safety shoes [S1][S8].

Use true ESD footwear (EN 61340-4-3:2018, 0.1–100 MΩ) when the worker is inside an EPA handling bare PCBAs, Class 0 ESDS devices, or backplane components, because 100 V human-body discharges can destroy parts the operator will not feel [S4]. For combined hazards (explosive atmosphere plus electronics assembly), specify ESD shoes on a verified ESD floor and accept that the A marking is also implicitly satisfied because the ESD band sits inside the antistatic band [S2][S7].

Who Each Type Is For, and Who It Is Not For

A-marked antistatic footwear is for the general industrial worker on S1 or above rated shoes, including petrochemical, pharmaceutical, paint-shop, flour mill, and ATEX zone operators who need spark-ignition control but are not handling exposed electronics [S1][S4][S8]. It is not for live electrical work, where EH-rated ASTM boots (rated to 600 V AC only) or dielectric footwear are specified instead, and it is not for personnel who rely on a strict EPA system resistance envelope below 35 MΩ [S5].

ESD footwear is for electronics assembly operators, field service engineers handling exposed boards, and any operator inside an EPA whose role description includes handling of ESDS items at 100 V HBM or below [S4][S7]. It is not a substitute for EH or dielectric protection in HV environments, and it is not a stand-alone solution: an ESD shoe without an ESD floor, an ESD smock, and a verified wrist-strap or foot-grounding path does not meet EN 61340-5-1 [S4].

Failure Modes and Common Specification Errors

ESD footwear vs EN ISO 20345 antistatic A marking resistance ranges - Failure Modes and Common Specification Errors
ESD footwear vs EN ISO 20345 antistatic A marking resistance ranges - Failure Modes and Common Specification Errors

The most common procurement error is specifying "ESD safety shoes" without naming EN 61340-4-3:2018 or quoting a resistance range, which lets suppliers deliver any antistatic A-marked boot in the 100 kΩ–1,000 MΩ window and pass it off as ESD [S5][S9]. The reverse error is specifying a sub-35 MΩ ceiling for an EPA that was never designed for it, producing shoes that pass the resistance test but feel "dead" to the wearer, signal false ground, and trigger ESD floor monitoring alarms outside the expected band [S4][S7].

Contamination is the second failure mode: any insulating film (oils, hydrocarbon splashes, midsole delamination, winter road salt residue) can push an in-spec ESD shoe above 100 MΩ, so verification on a body-voltage or foot-grounding tester is required at the EPA entry point, not just at issue [S4][S5]. EN 61340-4-3:2018 testing is performed under controlled humidity, which means a shoe that passes the lab test can still fail on the shop floor if the EPA humidity drifts outside the 12–50% RH envelope many programmes quote for the standard [S4].

Standards and Sourcing Reference

EN ISO 20345 defines the antistatic A marking and the 100 kΩ–1,000 MΩ window, with the test method in EN ISO 20344 [S1][S2][S4]. The ESD window of 0.1–100 MΩ is governed by BS EN IEC 61340-4-3:2018, while the EPA system envelope (shoe + floor + garment + grounding) is set by EN 61340-5-1 [S4][S5]. For explosive atmospheres the EU framework is ATEX 2014/34/EU for equipment and 1999/92/EC for worker protection, both of which reference antistatic footwear as one ignition-risk control measure [S1][S2].

For a deeper cut on the EPA system envelope and the 10⁶–10⁹ Ω window where most dissipative equipment actually sits, the companion piece on the SourceBySpec editorial site 10⁶ to 10⁹ Ω: where static dissipative ESD equipment actually lives extends the same resistance-band logic across mats, flooring, and garments.

Trackable signals to watch on the 2026-10-21 cycle: any revision of EN 61340-4-3 that tightens or widens the 100 MΩ ceiling, and any update to EN ISO 20345's class table that adds an explicit ESD letter code rather than relying on the A marking plus a separate EN 61340 certificate.

Frequently asked questions

What is the exact resistance range for ESD footwear under EN 61340-4-3:2018?

EN 61340-4-3:2018 specifies ESD safety footwear resistance between 0.1 MΩ and 100 MΩ (1×10⁵ to 1×10⁸ Ω), which is a narrower carve-out of the lower end of the EN ISO 20345 antistatic band. Some manufacturers, including Rock Fall, voluntarily tighten their internal ceiling to 35 MΩ per the older EN 61340-5-1:2007 guidance.

9 sources
  1. The difference between antistatic and ESD (Sep 25, 2015)
  2. ESD Footwear Standards: EN ISO 20345 Markings and ...
  3. Antistatic Safety Footwear: Standards and A Marking (Sep 1, 2026)
  4. A Guide to Anti-Static and ESD Safety Footwear (3 days ago)
  5. Electrical Hazard (EH), Anti-Static & Electrostatic ...
  6. EN ISO 20345 Explained - Safety Footwear Standard (Dec 19, 2018)
  7. How Do I Identify ESD-rated Footwear? (Nov 28, 2025)
  8. Antistatic vs ESD Footwear: What's the Difference? (Oct 12, 2026)
  9. ESD Safety Shoes: ESD vs Antistatic Explained - TrustGear (3 days ago)

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI