Table of Contents
  1. Permeation rate calculation for FKM seals
  2. What FKM can and cannot deliver
  3. Compare FKM, butyl, and FFKM for gas service
  4. Design variables that change the calculated loss
  5. Refrigerant-specific testing and sourcing
  6. Failure modes and acceptance criteria
FKM Seal Permeation for Refrigerant Gas Service

FKM seal permeation is governed by the refrigerant-specific coefficient, pressure differential, exposed area, and seal thickness, rather than by a single universal FKM rate.

For refrigerant service, the material decision must combine permeation, chemical compatibility, temperature, compression set, and the permitted system leak rate.

Permeation rate calculation for FKM seals

The steady-state permeation rate is calculated as Q = K·A·(P1 − P2)/D, where Q is the gas transfer rate, K is the permeation coefficient for the specific gas and elastomer, A is the exposed seal area, P1 − P2 is the pressure differential, and D is the seal thickness or diffusion-path length [S3][S4].

Permeation is gas transfer through the elastomer, not leakage around the sealing interface.

These figures demonstrate gas dependence, but they are not refrigerant coefficients and must not be substituted for one.

What FKM can and cannot deliver

FKM offers excellent chemical resistance and is commonly used for heat, oils, and chemicals, with material temperature resistance extending to approximately +200 °C [S8]. That resistance does not make every FKM compound gas-tight, because permeability is controlled separately by the refrigerant and compound formulation [S4].

FKM is suited to applications where refrigerant compatibility and temperature resistance dominate, including many static gland arrangements. It is less suitable where the allowable permeation rate is exceptionally low, the gas is a strong FKM permeant, or a metal seal can be justified by the service economics.

The material portfolio comparison is clear: FKM provides strong chemical resistance but only moderate, gas-specific permeation; butyl commonly provides lower gas permeability in dry vacuum service; and FFKM is generally used where low outgassing or demanding vacuum performance justifies its cost [S4]. FKM should therefore be specified as a performance-balanced elastomer, not as a universal refrigerant barrier.

Compare FKM, butyl, and FFKM for gas service

FKM seal permeation rate for refrigerant gas service - Compare FKM, butyl, and FFKM for gas service
FKM seal permeation rate for refrigerant gas service - Compare FKM, butyl, and FFKM for gas service

For severe service conditions, the comparison moves beyond material families. The EPDM option may suit water and steam exposure, but it does not replace a refrigerant-compatible compound simply because it has low permeability in another gas. Seal geometry, pressure, and compound-specific data must be evaluated together [S3][S4].

Design variables that change the calculated loss

Increasing seal thickness reduces permeation because it increases the diffusion path, while reducing exposed area reduces the transmission area in the governing equation [S4]. Deeper glands and larger cross-sections can therefore reduce gas transport through the seal without changing the compound.

Higher hardness, greater squeeze, swelling, and elevated temperature can alter the permeation result.

Neither value is an FKM refrigerant rate, but both show why the test gas, humidity, geometry, and units must be retained in the calculation record.

Refrigerant-specific testing and sourcing

FKM seal permeation rate for refrigerant gas service - Refrigerant-specific testing and sourcing
FKM seal permeation rate for refrigerant gas service - Refrigerant-specific testing and sourcing

A valid refrigerant-service calculation requires a permeability coefficient measured or published for the actual refrigerant, compound, and service temperature. Test literature commonly covers sheet permeation up to 400 K and can include measurements at about 600–700 K, but those conditions do not automatically match a compressor or refrigeration-system seal [S6].

For automotive-style fuel data, a Viton FKM comparison lists permeation rates at 23 °C for fuel C and a blend of 90% fuel C with 10% ethanol, demonstrating that the test fluid composition must be identified rather than generalized as hydrocarbon service [S7]. Refrigerant qualification should follow the same discipline, using the exact refrigerant identity, concentration, temperature, pressure, and elastomer grade.

Request a material-specific permeation coefficient, test method, temperature, humidity where applicable, pressure differential, and unit system from the compound or seal supplier. Use industrial adhesive data only for the relevant sealing system and test conditions, not as a substitute for elastomer permeation data. A generic certificate stating “FKM” or “Viton” is insufficient for a loss calculation.

Failure modes and acceptance criteria

Three failure modes should be separated during acceptance: leakage around the seal caused by poor fit or compression, permeation through the elastomer, and outgassing from the elastomer and surrounding surfaces. Permeation continues while a pressure differential exists, whereas outgassing generally declines as pumping time increases [S4].

A zero-interface helium leak result does not establish low total system loss. The equipment builder must define an acceptance limit that combines the permitted refrigerant loss, the calculated permeation rate, environmental exposure, operating temperature, and any applicable emission or safety requirement.

For rotating equipment, additional checks are required for wear, friction, heat, and compression set. The comparison in FKM vs NBR dynamic seals is relevant when the FKM element is dynamic rather than a static refrigeration seal. Dynamic seals require a different qualification because wear-generated leakage can dominate material permeation.

The next engineering action is to define the refrigerant, concentration, operating and worst-case temperatures, pressure differential, gland area, seal thickness, and maximum permissible loss. Request the compound-specific coefficient in compatible units, then calculate Q and verify the result through a seal-level gas-loss test.

Frequently asked questions

What formula should be used to calculate FKM seal permeation for a specific refrigerant?

Use Q = K·A·(P1 − P2)/D, where K is the refrigerant- and compound-specific permeation coefficient, A is the exposed seal area, P1 − P2 is the pressure differential, and D is the seal thickness or diffusion-path length. The resulting Q is the gas transfer rate through the elastomer.

Can published FKM coefficients for helium, hydrogen, nitrogen, or carbon dioxide be used for refrigerant service?

No. The cited coefficients—1–2 for helium, 40 for hydrogen, 0.05–0.7 for nitrogen, and 5 for carbon dioxide—are expressed in units of 10⁻⁸ sccm·cm/(s·cm²·atm), but they are not refrigerant coefficients. Request a coefficient measured or published for the exact refrigerant, FKM compound, and service temperature.

How do seal thickness and exposed area affect calculated FKM permeation?

Permeation decreases as seal thickness or diffusion-path length increases, because Q is inversely proportional to D. It also decreases when exposed seal area is reduced, because Q is directly proportional to A; deeper glands and larger cross-sections can therefore reduce transmission through the seal.

Does a zero-interface helium leak test prove that an FKM refrigeration seal has an acceptable total loss rate?

No. A zero-interface helium result addresses leakage around the sealing interface but does not establish low refrigerant permeation through the elastomer or control outgassing. Acceptance should separately assess interfacial leakage, calculated permeation, and outgassing against the permitted system loss.

9 sources
  1. O-Ring Permeation Chart
  2. Question: How much does permeation through elastomer O-rings ...
  3. Vacuum Permeation in O-ring Polymers
  4. O-Rings in Vacuum: Outgassing, Permeation & Seal Selection (Oct 11, 2026)
  5. Low Permeability - Seal Design Guide
  6. PERMEATION THROUGH ELASTOMERIC 0-RING SEALS*
  7. Viton™ Resistance To Reduce Emissions
  8. FKM O-rings: heat- and fluid-resistant (Oct 6, 2026)
  9. Materials in Vacuum Technology - Know-How | Pfeiffer Global

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI