Specify EPDM Flange Gaskets at 60–70 Shore A

Table of Contents
  1. 60–70 Shore A: Baseline Hardness for Metal Flanges
  2. Hardness Options Compared by Seal Duty
  3. Set Compression at 25–40% for Solid EPDM
  4. Match the Compound to Medium and Temperature
  5. Account for Cure, Compression Set and Geometry
  6. Limits, Failure Modes and Purchase Controls
Specify EPDM Flange Gaskets at 60–70 Shore A

EPDM flange gaskets for metallic pipe joints are normally specified at 60–70 Shore A, with installation compression typically targeted at 25–40% of free thickness [S1][S2].

This hardness band suits general static sealing across water, steam, weather, dilute acids, strong bases, glycols, ketones and alcohols, but it does not make EPDM suitable for petroleum oils or mineral fuels [S1].

60–70 Shore A: Baseline Hardness for Metal Flanges

For standard metallic pipe flanges, specify 60–70 Shore A and 3 mm thickness [S1]. A 3 mm gasket thickness is also identified as a normal starting point for that flange configuration, although flange geometry and design rules still govern final thickness [S1].

The wider EPDM family spans approximately 40–90 Shore A, so hardness alone does not identify a suitable compound [S1]. Published EPDM data includes a closed-cell EPDM sheet with a durometer rating of 15 Shore C (2024-05) [S5].

For purchase documentation, state Shore A hardness together with the EPDM grade, cure system, temperature rating and compression requirement. A 65 Shore A rating, for example, appears in a chemical-grade, 1 inch thermoplastic-piping flange gasket supplied as 65–66 Durometer A, but that dimensional product should not be treated as a universal flange-seal specification [S7].

Hardness Options Compared by Seal Duty

Low, medium and high hardness EPDM grades should be compared against conformability, installed compression and pressure duty rather than selected by durometer alone.

These are selection categories, not pressure ratings for every flange.

Set Compression at 25–40% for Solid EPDM

EPDM gasket hardness range for flange sealing applications - Set Compression at 25–40% for Solid EPDM
EPDM gasket hardness range for flange sealing applications - Set Compression at 25–40% for Solid EPDM

Solid EPDM gaskets typically target 25–40% compression of free thickness, with approximately 10–15% as a lower design boundary and approximately 50% as the upper limit [S2]. The calculation is [(free thickness minus compressed thickness) divided by free thickness] multiplied by 100; compressing a 3 mm gasket to 2.1 mm therefore produces 30% compression [S2].

Compression percentage is a geometry and installation parameter rather than a material property [S2]. A general rubber-gasket guide gives a typical compression range of 10–30% of original thickness and states that 40 Shore A material is easier to compress and conforms to irregular surfaces [S8]. For solid EPDM flange joints, the more specific 25–40% design target remains the controlling specification because the joint design, flange closure and compound formulation determine the final result [S2].

Under-compression can leave gaps across surface irregularities, while excessive compression can cause permanent deformation and loss of recovery [S2]. Compression percentage is an assembly parameter rather than an intrinsic material property, so changing Shore A hardness does not replace control of gasket height, groove depth, flange flatness and bolt torque [S2].

Match the Compound to Medium and Temperature

EPDM is suited to water, steam, weather, glycols, ketones, alcohols, dilute acids and strong bases, but it is not the correct material for petroleum oils [S1]. For steam service or continuous operation above 120°C, peroxide-cured compound or a special heat grade should be evaluated; EPDM’s overall working envelope extends from about -50°C to +150°C, with the upper limit dependent on cure system [S1].

Specify peroxide-cured compound for steam or continuous heat above 120°C [S1]. A published EPDM family range of -50°C to +150°C is compatible with the design guidance that lists EPDM from -50°C to +150°C for water, steam, alcoholic solvents and automotive brake fluids [S1][S4].

Do not extend that compatibility into hydrocarbon service by inference. If mineral oil, petroleum oil or fuel is present, nitrile rubber or fluororubber is the appropriate direction for comparison, while EPDM rubber remains the choice for compatible aqueous, steam and weathering service [S1]. Detailed medium-specific limits for EPDM alcohol and ketone resistance should be checked before a compound is approved.

Account for Cure, Compression Set and Geometry

EPDM gasket hardness range for flange sealing applications - Account for Cure, Compression Set and Geometry
EPDM gasket hardness range for flange sealing applications - Account for Cure, Compression Set and Geometry

Elastomer hardness is only one property of the gasket compound.

Compression set must be separated from installation compression. Compression set describes permanent deformation remaining after load removal and is evaluated under controlled deflection, temperature and recovery conditions under ASTM D395 Method B [S2].

For flange design, use 1–3 mm gaskets only where both flanges are smooth and rigid, and consider 3–6 mm where rougher or less regular surfaces require more conformity [S4]. The same guidance recommends a flange finish of approximately 125–250 microinches and controlled torque to avoid over-compression [S4].

Limits, Failure Modes and Purchase Controls

A 60–70 Shore A EPDM gasket can fail through assembly errors even when the durometer is correct: insufficient compression leaves leakage paths, excess compression promotes permanent set, and poor alignment creates local stress [S2][S4]. Thermal cycling, bolt-torque variation, surface roughness and material hardness all alter the contact stress developed at the gasket-flange interface [S2].

The apparent hardness tolerance also matters. A product advertised at 65–66 Durometer A is tighter than the general 60–70 Shore A pipe-flange band, while a commercial 60A sheet is listed at 55–65 Shore A [S7][S5]. Specifications should therefore define the test method and acceptance tolerance, not just write “EPDM 60A.”

EPDM compounds can be supplied as sheet, O-rings, extrusions or die-cut shapes, and the exact grade datasheet governs the final limits [S1]. For a flange package, the defensible purchase line is EPDM, 60–70 Shore A, approximately 25–40% installed compression, an identified cure system, a stated continuous-temperature rating, and verification of medium compatibility [S1][S2].

Two trackable checks close the specification loop: measure installed compression from gasket free thickness and the compressed joint, then confirm the purchased compound against ASTM D395 compression-set requirements and the stated service temperature [S2].

Frequently asked questions

What EPDM hardness should be specified for standard metallic pipe flange gaskets?

Specify 60–70 Shore A EPDM as the starting point for metallic pipe flanges because it balances conformability with resistance to excessive extrusion and permanent deformation. Control installation compression at 25–40% of the gasket’s free thickness.

What gasket thickness and compression should be used for a 3 mm EPDM flange gasket?

A 3 mm thickness is a normal starting point for metallic flange configurations, subject to flange geometry and applicable design rules. If assembly compresses it to 2.1 mm, the compression is 30%, calculated as [(3 − 2.1) ÷ 3] × 100.

Can 60–70 Shore A EPDM be used for petroleum oil and mineral fuel service?

No. EPDM is suited to water, steam, weather, glycols, ketones, alcohols, dilute acids and strong bases, but it is not suitable for petroleum oils or mineral fuels. Compare nitrile rubber or fluororubber when mineral oil, petroleum oil or fuel is present.

What EPDM compound and temperature details should be required in purchase documentation?

State Shore A hardness together with the EPDM grade, cure system, continuous-service temperature rating and required installation compression. For steam service or continuous operation above 120°C, evaluate peroxide-cured or special heat-grade EPDM; the overall EPDM working envelope is approximately -50°C to +150°C, depending on cure system.

8 sources
  1. EPDM Rubber Gasket Material - Hydraulic Cylinder (Jan 18, 2026)
  2. EPDM Gasket Compression Percentage Guide and Specifications (May 25, 2026)
  3. What are the standards for EPDM Gasket? - Blog (Oct 8, 2026)
  4. Rubber Gasket Design Guidelines - Custom rubber products.
  5. All About EPDM Gasket Properties (Oct 2, 2024)
  6. Neoprene vs EPDM vs Nitrile | Gasket Material Guide
  7. 1" Chemical Grade EPDM Flange Gasket
  8. Compression Rates in Rubber Gaskets : Solid vs. Foam/Sponge (Sep 2, 2025)

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI