A tape-cast titanium porous transport layer using a 60:40 Ti:PMMA ratio and 60 μm PMMA beads delivered a 62 mV lower cell voltage at 4 A/cm² than a commercial powder-based titanium PTL [S1].
Commercial supply extends beyond laboratory coupons to sheet-based titanium PTLs, coated structures, laser-cut formats, and custom components, but buyers must qualify porosity, thickness, coating, and gas-removal behavior for the assembled cell [S3][S4].
Why the PEM Anode PTL Controls Cell Losses
The PTL in a PEM electrolyzer occupies the interface between the catalyst layer and flow field, where it must conduct electrons while distributing water and removing oxygen [S4]. Its functions include water and oxygen mass transfer, thermal management, electrical conduction, and corrosion-resistant mechanical support [S4].
Titanium is the normal material choice for acidic, oxidative PEM anodes, while nickel and stainless steel are associated with alkaline AEM systems [S4]. A titanium PTL therefore combines structural conductivity with resistance to the anode environment, but material compatibility alone does not establish cell performance.
For procurement, the relevant article is the hydrogen electrolyzer, because the PTL must be evaluated as part of the membrane-electrode assembly, flow field, catalyst layer, operating pressure, and production rate rather than as a standalone filter.
Compare PTL Structures by Pore Size, Porosity, and Contact
A 2023 tape-casting study varied titanium loading and PMMA poreformer bead size, then characterized the structures by SEM and synchrotron X-ray computed tomography [S1]. The best reported formulation used a 60:40 Ti:PMMA ratio and 60 μm PMMA beads and outperformed the standard commercial titanium powder PTL by 62 mV at 4 A/cm² [S1].
Increasing titanium loading improved contact at the catalyst-layer/PTL interface, but it also produced severe mass-transport losses caused by gas bubbles [S1]. Large poreformer beads created a more open structure with improved gas removal while retaining mechanical integrity, showing that maximum solid loading is not the same as maximum cell performance [S1].
Match Porosity and Thickness to the Stack Design

Bekaert states that PEM electrolyzers typically use titanium PTLs, while AEM electrolyzers use nickel and stainless steel.
Thickness adaptation changes porosity, so a dimensional tolerance cannot be specified independently of the pore network [S4]. A buyer should require the proposed material to demonstrate both electrical contact at the catalyst layer and adequate transport of feed water and oxygen under the intended operating condition.
Specify Coatings Without Confusing Support and Surface Function
A commercially listed titanium PTL measures 150 × 150 mm and carries an iridium coating at 0.2 mg/cm² for PEM water electrolysis [S7]. The coating specification is distinct from the substrate requirement: the product is identified as an iridium-coated titanium PTL intended for oxygen-evolution-side use [S7].
U.S. Department of Energy funding documentation identifies Mott Corporation as the recipient for the project titled “Advanced Porous Transport Layer Design and Manufacturing for PEM Electrolyzers.”
Coating loading, uniformity, adhesion, and performance after assembly require separate qualification rather than substitution from the datasheet.
Wettability and Build Quality Can Shift Transport Losses

A 2021 study established that PTL wettability affects mass transport in PEM electrolyzers and used that relationship to guide next-generation PTL design [S5]. This matters because a hydrophilic surface changes how liquid water occupies the porous structure, while gas-phase pathways still determine oxygen evacuation from the reaction zone.
Higher titanium loading cannot be treated as a universal improvement because the 2023 study linked it to better catalyst-layer contact and worse bubble-driven mass-transport loss [S1]. The structural design must balance compression, contact resistance, liquid distribution, gas permeability, and enough rigidity to avoid damage during assembly.
Such products still require verification against the stack's compression, sealing, and pressure conditions.
Separate Commercial Availability from Cell Qualification
Bekaert states that PEM electrolyzers typically use titanium PTLs, while AEM electrolyzers use nickel and stainless steel.
These offerings establish manufacturing breadth, not interchangeability. Procurement should require a supplier to identify whether the quoted layer is titanium sheet, fiber paper, powder-based material, tape-cast material, or an additively manufactured structure, because each route uses a different pore-control mechanism [S1][S3][S6][S8].
The qualification package should include substrate grade, thickness tolerance, porosity method, pore-size distribution, basis weight where applicable, coating material and loading, flatness, contact-pressure behavior, in-plane electrical resistance, gas permeability, and cell-test results at the intended current density [S1][S2][S7].
Qualification Criteria for a Production PTL Purchase

A technically defensible titanium PTL purchase combines four controls: a validated pore structure, stable catalyst-layer contact, corrosion-compatible titanium construction, and evidence at the intended operating current density [S1][S4]. The 4 A/cm² result for the 60:40 Ti:PMMA tape-cast structure provides a useful comparison point, but it does not replace testing the final cell architecture [S1].
Buyers should separate commercial dimensions from performance criteria. Bekaert's 0.15–0.50 mm coated-titanium range and 210 × 290 mm or 430 × 580 mm standard formats define available geometry [S4]. The 150 × 150 mm iridium-coated product and its 0.2 mg/cm² loading define a different commercial specification [S7].
Near-term sourcing can be tracked through three measurable items: commercial orders for titanium PTLs with defined coating loading, supplier disclosure of porosity and thickness tolerances, and cell-test data reporting voltage at a stated current density. These signals distinguish a specified component from a generic porous metal sheet [S1][S2][S3][S4][S7].