US ferrous scrap reached $404 per tonne on November 19, 2026, while the October 2026 nonferrous scrap producer-price index stood at 723.393 [S2][S5].
Ferrous material is commonly quoted per ton and non-ferrous metal per pound, with copper, brass and aluminum commanding higher unit prices than steel and iron [S3].
What the 2026 Scrap Price Index Measures
The US scrap market has no single exchange price covering every grade and location. It combines commodity indices, regional ferrous benchmarks and dealer quotations, each serving a different purpose [S3][S4][S5].
The BLS producer-price series for nonferrous scrap, WPU1023, uses an index base of 1982=100 and is not seasonally adjusted. The FRED nonferrous scrap index (WPU1023) recorded an observation of 723.393 in October 2026 [S2]. The broader BLS metals and metal products index reached 395.633 in October 2026, versus 337.898 in October 2025 [S1].
For ferrous material, RMDAS reports regional aggregated spot prices in USD per gross ton. Values are derived from participants’ actual order data processed by the 20th of each buy month and then rounded to whole integers [S4]. These are market benchmarks, not universal prices for every load.
Ferrous Scrap Trend and Price Benchmarks
Ferrous scrap stood at $404/t on November 19, 2026, up 1.00% from the preceding day, 2.54% over a shorter comparison period and 13.48% against the corresponding prior-year period [S5].
Reported RMDAS regional aggregated spot-market ferrous scrap prices are based on participants' actual order data processed as of the 20th of each respective buy month and rounded to whole integers [S4]. These series cannot be treated as interchangeable without checking their geographic and commodity definitions.
Ferrous pricing is usually expressed per ton because steel and iron have lower value per unit weight than copper, brass or aluminum [S3]. The practical result is that a heavy ferrous load can still produce substantial gross proceeds even when its quoted rate per pound is much lower.
Non-Ferrous Scrap Pricing and Metal Ranking
Approximate 2026 sector ranges place copper at $2.00–$4.00+ per pound, brass at $1.50–$3.00, aluminum at $0.40–$0.80, stainless steel at $0.30–$0.60, lead at $0.30–$0.50, and steel and iron at $0.05–$0.15 [S3].
Non-ferrous material is usually priced per pound because smaller quantities can carry high value [S3]. Clean bright copper and #1 copper occupy the upper end of the commercial range, while oxidized #2 copper and insulated wire receive lower rates because recovery costs and contaminants reduce recoverable value [S3].
The FRED nonferrous scrap index (WPU1023), indexed to 1982=100 and not seasonally adjusted, recorded an observation of 723.393 in October 2026 [S2].
Comparing Ferrous and Non-Ferrous Pricing
Non-ferrous grades offer much higher revenue per pound, but ferrous grades remain the volume business. The comparison is straightforward on unit value: copper at $2.00–$4.00+ per pound can exceed steel and iron at $0.05–$0.15 by a very large multiple [S3].
On price stability, the two segments require different reference points. Ferrous buyers track regional gross-ton benchmarks and monthly RMDAS values, while non-ferrous sellers track commodity-linked dealer rates and grades [S3][S4]. On logistics, non-ferrous earns a higher rate per pound and is more sensitive to contamination and recovery yield, whereas ferrous value depends more heavily on weight, bulk handling and transport cost [S3].
On suitability, a fabrication shop buying scrap for remelting should separate material by grade and negotiate on the relevant benchmark. A scrapyard or industrial buyer seeking a price signal should compare WPU1023 for nonferrous scrap with a geographically matched ferrous benchmark rather than treating a brass dealer quote and an RMDAS steel value as directly comparable [S2][S4].
Who Benefits from Each Pricing Method
Large generators, demolition contractors and fabrication plants can use ferrous indices to estimate the value of high-volume steel and iron before transport. This works best when the buyer can segregate clean heavy metal from material with excessive coatings, plastics or mixed grades that increase processing costs [S3][S4].
Non-ferrous buyers fit a different use case. Cable generators, HVAC contractors, valve and fitting users, and aluminum processors can evaluate material by grade and unit weight because copper, brass and aluminum carry substantially higher value per pound [S3].
These methods are less suitable for informal loads containing several alloys. A blended load can produce a misleading estimate because an apparent ferrous rate may include copper, aluminum or stainless content, while a non-ferrous average can conceal lower-value contamination [S3]. Such loads require material sampling, weight reconciliation and a grade-specific settlement statement.
Cost Drivers Behind Scrap Prices
The largest cost driver for a scrap seller is not the headline index but the gap between benchmark value and the net settlement received. That gap includes freight, sorting, processing, assay or contamination deductions, and the minimum-volume requirements imposed by the buyer [S3][S4].
Material quality ranks next. Clean copper, sorted brass and aluminum free of steel attachments command better settlement rates than mixed or contaminated streams [S3]. For ferrous material, grade, quantity, density, freight and the buyer’s processing costs determine the discount from the regional benchmark [S4].
Volume tier also affects price because larger, consistent loads reduce handling and assay costs, while small quantities face more fixed charges per pound. Total cost of ownership therefore includes purchase price plus inbound transport, sorting labor, processing charges, carry-inventory time and the yield loss from contamination. A higher unit price can still produce a lower net return if freight and processing costs rise proportionally.
Practical Limits of the Price Benchmarks
Each benchmark carries a scope limitation. WPU1023 is an index with a 1982=100 base, not a dollar price, and its October 2026 value of 723.393 must not be interpreted as $723.393 per pound [S2].
RMDAS values apply to specified regional aggregated commodities and depend on transactions expected during the reported buy month [S4]. A national scrap-steel quote of $404/t is a separate market measure and may differ from RMDAS values because of geography, grade, timing and transaction terms [S4][S5].
The quoted per-pound ranges for copper, brass, aluminum, stainless steel, lead and ferrous metal are approximate 2026 sector estimates rather than guaranteed offers [S3].
Track monthly WPU1023 and WPU10 movements alongside the next regional ferrous benchmark and day-specific dealer quotes. A change in the nonferrous index, ferrous gross-ton value and seller’s material mix will provide a more defensible estimate than any single 2026 price point [S1][S2][S4].