REQUEST FOR QUOTE → Request a quote
SpecForge Editorial Team

Cross-Reference AS568 EPDM O-Rings by Size and Cord

Table of Contents
  1. What the AS568 Dash Number Identifies
  2. Dash Number Series and Cross-Sections
  3. Selected AS568 Cross-Reference Dimensions
  4. Fractional Labels Can Misidentify a Ring
  5. Metric Cross-References Need Conversion Discipline
  6. EPDM Selection Criteria Beyond Size
  7. Metric, AS568 and Custom Sizes Compared
  8. Inspection and Procurement Checks
Cross-Reference AS568 EPDM O-Rings by Size and Cord

AS568 covers inch-based O-ring sizes with inside diameters from 0.029 in for -001 to 25.940 in for -475 and cross-sections from 0.040 in to 0.275 in [S2][S5].

Each dash number identifies a nominal inside diameter, cross-section and tolerance series, so an EPDM ring can be ordered without relying on a rounded fraction or an outside-diameter label [S1][S3].

What the AS568 Dash Number Identifies

SAE AS568 defines an O-ring through its inside diameter, cross-section, dimensional tolerances and dash-number identification code [S1][S2]. The dash number is not a hardness or material code, so an order such as AS568-210 identifies geometry only.

AS568 dash numbers identify o-ring sizes, with dimensions specified by inside diameter and cross-section. A complete purchase specification should therefore combine the AS568 number with a Shore A durometer and elastomer designation [S2].

For an EPDM component, the size code should be followed by the required hardness and compound, such as 70 Shore A EPDM. Available hardness in the referenced ordering system runs from 20 to 90 Shore A, with a standard tolerance of ±5 durometer points [S2].

Dash Number Series and Cross-Sections

Both inside diameter and cross-section are needed to identify an o-ring size because two rings can have nearly the same ID but different cross-sections.

AS568-004 has a 0.070 in cross-section, and AS568-110 has a 0.103 in cross-section.

AS568-210 has a 0.139 in cross-section, and AS568-318 has a 0.210 in cross-section.

AS568-001, AS568-002, and AS568-003 have cross-sections of 0.040 in, 0.050 in, and 0.060 in, respectively.

Selected AS568 Cross-Reference Dimensions

EPDM O-ring size chart AS568 dash number cross reference - Selected AS568 Cross-Reference Dimensions
EPDM O-ring size chart AS568 dash number cross reference - Selected AS568 Cross-Reference Dimensions

AS568-210 has a nominal ID of 0.734 in and a 0.139 in cross-section, producing a calculated OD of 1.012 in [S3]. The OD follows the geometry of an unstretched round ring: OD = ID + 2 × CS [S3].

AS568-214 has a nominal ID of 0.984 in, a 0.139 in CS and an ID tolerance of ±0.010 in. AS568-318 has a nominal ID of 0.975 in, a 0.210 in CS and the same ±0.010 in ID tolerance [S3]. Their nominal IDs differ by only 0.009 in, while the -318 cord is 0.071 in thicker, about 51% [S3].

The reference table also places -001 at 0.029 in ID, 0.040 in CS and 0.109 in OD; -004 at 0.070 in ID, 0.070 in CS and 0.210 in OD; and -110 at 0.362 in ID, 0.103 in CS and 0.568 in OD [S4]. These dimensions demonstrate why an O-ring cross-reference must include both ID and CS rather than fitting by nominal bore alone.

Fractional Labels Can Misidentify a Ring

AS568-210 has an ID of 0.734 in with an ID tolerance of ±0.010 in, giving an allowed range of 0.724–0.744 in. A ring measured at 0.750 in ID is therefore outside that tolerance range despite matching the nominal fraction label.

This distinction matters during inspection and cross-reference work. Record the measured ID and CS independently, compare both against the specified tolerances, and then confirm the complete dash number. Two rings can have overlapping ID ranges but different cord sections, as demonstrated by -214 and -318 [S3].

For nonstandard rings, specify inside diameter and cross-section directly, and order o-rings by size, hardness, and material.

Metric Cross-References Need Conversion Discipline

EPDM O-ring size chart AS568 dash number cross reference - Metric Cross-References Need Conversion Discipline
EPDM O-ring size chart AS568 dash number cross reference - Metric Cross-References Need Conversion Discipline

Metric O-rings are commonly written as ID × CS in millimeters, while AS568 dash numbers identify inch-series dimensions [S3]. A direct cross-reference requires conversion at 1 in = 25.4 mm, with rounding only after the dimensional comparison is complete.

The 0.070, 0.103, 0.139, 0.210 and 0.275 in cross-sections correspond approximately to 1.78, 2.62, 3.53, 5.33 and 6.99 mm [S3]. Rounded millimeter values are useful for catalog searches, but purchasing tolerance should remain tied to the governing AS568 dimensions and their inch-based tolerances.

Do not treat a rounded metric size as an exact AS568 equivalent. A supplier’s metric cross-reference can identify a likely candidate, but the purchase order should state the dash number, hardness and material when interchangeability matters. The referenced size system covers both fractional and decimal inch dimensions with tolerances [S2].

EPDM Selection Criteria Beyond Size

An AS568 size chart establishes geometry, not chemical compatibility, temperature capability or compression performance. The referenced EPDM rubber must still be qualified for the actual fluid, temperature range, pressure and service life, while the O-ring must be sized against the groove and shaft or bore geometry. [S5]

These figures belong to the listed gland design, not to the AS568 size code itself.

Material selection also affects installation and service. EPDM O-rings should not be selected for petroleum oils or mineral-oil service merely because the dash number matches; elastomer compatibility must be confirmed separately from size [S1][S2].

Metric, AS568 and Custom Sizes Compared

EPDM O-ring size chart AS568 dash number cross reference - Metric, AS568 and Custom Sizes Compared
EPDM O-ring size chart AS568 dash number cross reference - Metric, AS568 and Custom Sizes Compared

The three common sizing routes differ in control, interchangeability and procurement risk. The correct choice depends on whether the drawing specifies a standard code, a metric seal or a controlled nonstandard geometry. [S8]

AS568 sizing provides a dash number linked to inch-based ID, CS and tolerances, which makes it suitable for repeat orders and legacy drawings [S1][S2]. Metric ID × CS sizing is useful for international or metric designs, but rounded values and conversion practices can complicate direct interchange with an AS568 drawing [S3]. Custom ID × CS sizing offers dimensional flexibility, although it requires tighter drawing control because no standard dash number identifies the seal [S2].

For interchangeability, compare nominal ID, CS, tolerance and gland conditions rather than code alone. For repeat procurement, preserve the full description: quantity, AS568 dash number, hardness and material. Apple Rubber illustrates this structure with 10,000 pieces of AS568-110 in 70 Shore A silicone, expressed as “10,000 AS568-110 70SL” [S2].

Inspection and Procurement Checks

Inspect the ring’s ID and CS rather than its OD alone, because the same OD can be produced by different ID and CS combinations [S3]. For example, AS568-210 at 0.734 in ID and 0.139 in CS gives 1.012 in OD, so a diameter reading must be evaluated against the correct geometric pair.

Cross-section tolerance is not interchangeable with ID tolerance. The -210 reference uses a 0.139 in CS with a ±0.004 in tolerance, while -318 uses a 0.210 in CS with a ±0.005 in tolerance [S3]. A caliper measurement can therefore reveal a size mismatch that an ID-only check misses.

Record the complete procurement line as quantity, size, hardness and material. Standard durometer options in the referenced specification span 20 to 90 Shore A, with ±5 points tolerance and a 70 Shore A standard for most elastomers [S2]. Add the material designation required by the drawing, such as EPDM, without using the compound code as a substitute for the AS568 geometry code.

For equivalent EPDM replacements, capture the original AS568 dash number, measured ID, measured CS, hardness and groove details before ordering. Compare those values with the supplier’s tolerance table, then verify the new ring’s material and hardness against the service specification rather than accepting a match based on the dash number alone.

Frequently asked questions

What dimensions and tolerance define an AS568-210 EPDM O-ring?

AS568-210 has a nominal inside diameter of 0.734 in, a cross-section of 0.139 in, and a calculated outside diameter of 1.012 in. Its specified ID range is 0.724–0.744 in, so a 3/4 in ID measurement is not an acceptable substitute.

Which AS568 series should be selected for a 0.139 in cross-section?

The 200 series uses a 0.139 in cross-section, approximately 3.53 mm, with a ±0.004 in tolerance. Individual dash numbers in the -201 through -284 range identify the nominal inside diameter and tolerance series.

Can a metric ID × cross-section label be treated as an exact AS568 equivalent?

No. Convert metric dimensions using 1 in = 25.4 mm and complete the dimensional comparison before rounding; a rounded metric size may only identify a likely AS568 candidate. Specify the governing dash number, hardness and material when interchangeability matters.

What compound and hardness should accompany AS568-210 on a purchase order?

Specify the geometry together with the elastomer and Shore A durometer, for example 70 Shore A EPDM with AS568-210. The dash number identifies geometry only, and the referenced hardness range is 20–90 Shore A with a standard tolerance of ±5 durometer points.

8 sources
  1. AS568 Size Chart
  2. AS568 Standard O-Rings
  3. O-Ring Size Chart: Selected AS568 Sizes and Metric Cross ... (Oct 30, 2026)
  4. AS568 O-Ring Size Chart & Dimensions
  5. O-Ring Size Chart: Standard and Metric Dimensions Guide
  6. O-Ring Size Chart (AS568): Dash Numbers, ID & CS
  7. O-RING REFERENCE AS568 SIZES
  8. O-Ring Specification Chart | AS568, ISO 3601 Size Tables

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI