  1. Defining an Acceptable Outgassing Requirement
  2. Comparing Common Engineering-Plastic Families
  3. Moisture, Additives and Contamination Risk
  4. Temperature, Bake-Out and Service Limits
  5. Where Plastic Components Are and Are Not Suitable
  6. Procurement, Preparation and Validation
Engineering Plastic Outgassing Requirements for Vacuum Parts

Engineering-plastic vacuum components should be selected from grade-specific ASTM E595 data, with 24-hour TML and CVCM results checked against the chamber's pressure and contamination limits.

The ASTM E595 test described in [S4] exposes a plastic to a vacuum of 5 × 10⁻⁶ Torr for 24 hours at 257°F and reports total mass loss, collected volatile condensable materials, and water vapor regained.

Defining an Acceptable Outgassing Requirement

An engineering-plastic outgassing requirement should state the polymer grade, manufacturer, finished-part configuration, maximum test temperature, exposure duration, vacuum level and acceptance limits. A generic statement such as "low-outgassing plastic" is not auditable because additives, reinforcement, surface condition and processing history can alter behavior [S5].

ASTM E595 measures three outputs under a defined vacuum exposure: total mass loss, or TML, in percent; collected volatile condensable material, or CVCM, in percent; and water-vapor regain, or WVR, in percent. NASA's database uses this method to substantiate material suitability for spaceflight vacuum environments [S1].

The test provides a material screen rather than a direct guarantee of chamber pressure. Outgassing depends on the polymer, temperature, time under vacuum, surface condition and prior exposure [S5]. For process equipment, the procurement specification should therefore combine laboratory limits with finished-part qualification, including the actual chamber geometry and bake-out cycle.

Comparing Common Engineering-Plastic Families

These figures are screening values for listed grades, not universal properties for every member of a resin family [S4]. Compare candidates on four criteria: TML for total volatile release, CVCM for condensable contamination, WVR for moisture retention, and maximum service or bake-out temperature. That comparison must also account for electrical insulation behavior, which is discussed in Engineering Plastic Insulation Resistance vs Temperature.

Moisture, Additives and Contamination Risk

engineering plastic outgassing requirement for vacuum chamber components - Moisture, Additives and Contamination Risk
engineering plastic outgassing requirement for vacuum chamber components - Moisture, Additives and Contamination Risk

The cited engineering comparison states that many plastics are hydroscopic and absorb water of hydration in the bulk of the plastic [S2]. Water held inside a plastic must diffuse to the surface before it can be pumped, extending the release period after chamber evacuation.

Moisture is only one source of contamination. Plastics may release unpolymerized monomers, plasticizers, stabilizers and other additives, and these species can deposit on optical components, semiconductor surfaces or other sensitive hardware [S2]. Higher-purity feedstock reduces the available impurity burden, but grade-specific test evidence remains necessary because processing and formulation affect the finished component [S4].

CVCM deserves particular attention where a condensable film would damage a product. TML measures total mass loss, while CVCM quantifies volatile material collected on a nearby test surface; the difference cannot be inferred from TML alone [S1][S4].

Temperature, Bake-Out and Service Limits

Vacuum-service plastics must tolerate both their operating temperature and the chamber's bake-out schedule. These figures describe cited material limits, not permission to operate every component at its maximum temperature.

The standard screening condition of 125°C for 24 hours supplies a common comparison point, but it does not reproduce every process condition [S2][S4]. A part that will see a 200°C bake, a heated deposition source or repeated thermal cycling needs confirmation that its polymer, adhesive, coating and joining method remain acceptable at the actual peak temperature.

Vacuum components can also create thermal constraints beyond the polymer rating. Current-carrying wires lose convective cooling under vacuum, requiring current-capacity derating, while electrical insulation and engineering plastics must remain compatible with the intended voltage, temperature and geometry [S2].

Where Plastic Components Are and Are Not Suitable

engineering plastic outgassing requirement for vacuum chamber components - Where Plastic Components Are and Are Not Suitable
engineering plastic outgassing requirement for vacuum chamber components - Where Plastic Components Are and Are Not Suitable

Engineering plastics are justified for electrical isolation, complex machined geometry, thermal isolation and wiring support when their measured outgassing and temperature limits fit the process [S2]. They can also prevent eddy currents in applications where a metal part would create unacceptable interference.

They are a poor default for chambers requiring the lowest possible pressure, long uninterrupted pump-down or maximum bake-out temperature. Porous surfaces retain adsorbed water, while the polymer matrix may retain water and volatile constituents [S2]. For applications requiring strict contamination control, metals and ceramics may remain the safer default unless a plastic component has completed finished-part qualification.

Elastomeric seals require their own evidence rather than substitution of plastic data. Material families such as EPDM rubber, nitrile rubber and fluororubber should be checked for vacuum compatibility, compression set, temperature and extractables before use.

Procurement, Preparation and Validation

The procurement specification should require ASTM E595 data for the exact resin grade and, where available, the finished component. A supplier should identify fillers, pigments, adhesives, lubricants and processing aids, because a low-outgassing base resin does not establish the performance of a compound containing unspecified additives. [S4]

Preparation is part of the requirement. Suitable plastic selection, careful handling, cleaning, and bake-out can reduce chamber outgassing, while adsorbed gases must become gaseous before pumps can remove them [S7][S9]. A vacuum-compatible assembly also needs a controlled bake-out schedule matched to the polymer's thermal limit.

Acceptance should follow two stages. First, compare ASTM E595 TML, CVCM and WVR against procurement limits. Second, pump the assembled chamber with production heaters, seals, cables and fixtures present, then record pressure versus time, pressure-rise rate after isolation, and any visible condensate on witness surfaces. This finished-part test exposes effects that a coupon result cannot [S1][S5].

A traceable engineering-plastic outgassing requirement is therefore grade-specific and risk-based: name the polymer and formulation, set ASTM E595 limits, require temperature and bake-out compatibility, and validate the completed assembly. Track the qualified material, supplier change, finished-part test date and any production bake cycle as the next set of control points.

Frequently asked questions

What ASTM E595 data should an engineering-plastic vacuum-part specification require?

Require 24-hour TML, CVCM and WVR results for the exact polymer grade and finished-part configuration, together with the vacuum level, test temperature, exposure duration and acceptance limits. The ASTM E595 reference condition is 5 × 10⁻⁶ Torr for 24 hours at 125°C, and a generic designation such as “low-outgassing plastic” is not auditable.

Which cited engineering-plastic grades have the lowest listed TML and CVCM values?

Among the listed grades, PPS is reported at 0.04% TML and 0.00% CVCM, while PTFE is at 0.05% TML and 0.00% CVCM. PEEK is listed at 0.26% TML and 0.00% CVCM, so the CVCM value alone does not establish the lowest total volatile release.

What maximum temperatures are cited for PTFE, Vespel, PEEK and Kapton in vacuum service?

The cited material limits are 260°C for PTFE and Vespel, 177°C for PEEK, and 400°C for Kapton. A component exposed to a 200°C bake or repeated thermal cycling must also be qualified for its actual peak temperature, including adhesives, coatings and joining methods.

Which engineering-plastic families require particular attention to moisture uptake in vacuum chambers?

Nylon, polycarbonate and acrylic are identified as hydroscopic, whereas polyethylene, polypropylene, FEP, PTFE, PFA and PVC are described as non-hydroscopic. Internal moisture must diffuse to the surface before evacuation and can extend the release period after pump-down.

9 sources
  1. Outgassing Database (Jul 11, 2025)
  2. Plastics in Vacuum Applications
  3. Understanding Outgassing for Semiconductor Plastics Guide (Nov 25, 2023)
  4. Outgassing Plastic Materials for Semiconductor (Apr 11, 2023)
  5. Outgassing: significance in vacuum environments
  6. Understanding Outgassing Requirements: Importance & ... (Feb 3, 2025)
  7. Basic Outgassing Concepts
  8. Materials for use in vacuum
  9. Outgassing in Vacuum Deposition (Jul 27, 2026)

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI