A PQ² diagram matches a die to a die casting machine by comparing the die’s pressure and flow demand with the machine’s injection performance envelope.
The PQ² diagram relates the injection unit’s ability to deliver energy during cavity filling to filling flow, gate velocity, plunger diameter, and die resistance.
What the PQ² Axes Represent
The PQ² diagram expresses the relationship between pressure P, the pressure applied through the injection plunger, and flow rate Q, which determines metal velocity during cavity filling [S1][S2].
The graph is more informative than a machine’s headline tonnage because it shows how injection capability changes as flow demand rises. A cold chamber die casting machine may offer substantial force, but the usable operating point still depends on plunger diameter, hydraulic circuit, accumulators, valve behavior, and the resistance created by the die and casting [S2].
Metal generally moves through the gates at a speed of a few tens of metres per second during the short filling interval, and the casting is shaped and much of its quality determined within that brief phase [S2]. The PQ² diagram therefore helps assess the machine’s capability during the second injection phase, not merely its ability to hold a static load.
Construct the Die Demand Curve
The die requirement must be expressed as a curve of required pressure against Q², with each point representing an operating condition during filling [S3]. The die’s estimated resistance depends on the gating system and casting geometry, while the required flow follows from the shot volume and target filling time [S3].
Target filling time and estimated freezing time are critical parameters in die design because they connect gating calculations to the period in which the casting must be filled before solidification compromises the process [S3]. The analysis should also account for static back pressure imposed by the die’s air-exhaust system when calculating the pressure needed to produce the casting [S3].
Gate velocity is the practical bridge between the calculated demand and machine performance. If the die is assigned a target gate velocity and the calculated Q for that target does not produce enough pressure to overcome resistance, the machine-die pairing is unsuitable without changes to gating, dimensions, materials, or process parameters [S1][S3].
Read the Machine Performance Envelope

The machine performance envelope on the PQ² diagram is the permitted operating region established by the injection unit, and the die requirement curve must fit within it [S3].
This trade-off means a die curve that lies beyond the machine envelope cannot be corrected simply by selecting a longer fill time. The required point lacks either the necessary flow, the necessary pressure, or both.
Machine construction changes the envelope. The injection unit described by the PQ² diagram consists of accumulators and a hydraulic cylinder that manages the movement of the injection plunger. Comparing envelopes from different machines is therefore more meaningful than comparing a single maximum-pressure or maximum-tonnage figure.
Compare Options on Four Decision Criteria
Machine selection should compare pressure availability, flow capacity, die resistance, and hardware configuration rather than rely on one nominal rating. The same four criteria also explain why hot chamber and cold chamber systems cannot be judged with a common unconverted headline figure. [S1]
Pressure availability concerns whether the injection unit can overcome gate, runner, and cavity resistance. Flow capacity concerns whether it can supply the required Q within the intended filling interval. Die resistance concerns the geometry and gating condition represented by the die demand curve. Hardware configuration concerns plunger diameter, shot sleeve, hydraulic circuit, accumulators, and valve control, all of which shape the PQ² envelope [S1][S2].
The correct choice is therefore the machine whose full envelope encloses the die demand, not the machine with the largest single endpoint. Engineers should also confirm whether the proposed machine is a hot chamber machine or cold chamber machine before applying a supplied performance curve.
Identify Where the Match Fails

A failed match occurs when the die demand curve crosses outside the machine performance envelope, commonly because the target flow requires more pressure than the unit can produce or because the calculated resistance exceeds the available injection pressure [S3]. The operating point must also be checked for controllability, because theoretical capability is of little value if valve response cannot regulate the intended intermediate point.
Three implementation errors can distort the comparison. First, using Q instead of Q² misstates the horizontal position of every operating point [S2]. Second, treating the dry maximum-flow endpoint as a production point ignores the pressure needed to move liquid metal [S2]. Third, comparing only machine pressure ignores that flow capability falls as demanded pressure rises [S1][S2].
The plunger and shot sleeve remain central to the check. Their dimensions influence both the maximum flow and the resistance encountered by the metal, while hydraulic design and accumulator performance determine how the machine traverses the envelope during filling [S1][S2]. For machine-family context, a shot sleeve should be reviewed together with the injection unit rather than selected as an isolated component.
Turn the Diagram into a Purchase Decision
The final machine-die match requires three records: the die pressure-flow demand curve, the OEM’s machine PQ² performance envelope, and the intended operating point for the qualified casting and alloy. The demand curve is derived from die calculations that include filling time, freezing time, gating flow, resistance, and exhaust-system back pressure [S3].
Before releasing the machine, verify that the operating point remains inside the envelope across the full filling sequence, that the gate velocity target is met, and that the plunger and shot-sleeve configuration is the one represented by the curve [S1][S2]. If the operating point lies outside, compare alternatives across pressure capability, flow capability, die resistance, and hardware configuration rather than accepting a larger machine without checking its actual envelope.
The trackable engineering result is the signed overlap between the die demand curve and the specific machine configuration envelope. A completed match identifies the proposed operating point, the margin to the machine limits, and the gating and hardware assumptions that produced it.