Indonesia’s MHP route was preferred by companies over traditional routes such as briquettes and matte, while tightening MHP supply was linked to sulfur prices, high-capacity operation, maintenance and reduced operations.
PT Huafei Nickel Cobalt planned to suspend lines from May 1, 2026, with an estimated production impact of about 50%, as sulfur prices rose and plants operated near capacity [S2].
Why MHP and Matte Supply Differentiate Battery Nickel
MHP and matte are distinct intermediate feed routes for nickel sulfate: MHP contains mixed hydroxide precipitate from laterite processing, while matte is a separate nickel intermediate produced for subsequent refining [S3].
MHP output was expected to reach 113,500 tonnes in 2022, an increase of 1,691% from 2011, as Indonesian laterite-based production expanded [S1]. Fastmarkets found MHP producers increasingly preferred the material over LME-grade nickel briquettes and nickel matte for sulfate conversion [S1].
The nickel alloy reference is relevant to downstream material selection because nickel sulfate feed chemistry determines the composition of purified nickel compounds used in battery precursors.
How the 2026 MHP Constraints Stack Up
Sulfur supply shortages and sharply higher sulfur prices contributed to tightening MHP supply. This reagent intensity explains why sulfur availability can constrain MHP output even when nickel ore remains available.
MHP Versus Matte, Briquettes and Sulfate Feed

MHP versus matte differ across four decision criteria: feed availability, conversion route, pricing exposure and operational dependency. Companies were choosing MHP over traditional routes such as nickel metal briquettes and nickel matte.
Feed availability: MHP depends on laterite ore quotas, HPAL maintenance and sulfur imports. Matte avoids direct dependence on the MHP refining stage but still requires stable mining, smelting and conversion capacity, while the research does not quantify the 2026 matte supply share at unit level [S2].
Conversion route: MHP requires dissolution and purification before sulfate production, whereas briquettes are dissolved or refined and matte is refined into marketable products [S1][S6]. FPX Nickel described sulfate production as based primarily on dissolving LME-grade nickel briquettes or refining nickel intermediates [S6].
Pricing exposure: historical Chinese EXW nickel sulfate pricing tracked LME Class I nickel with a 4% monthly statistical discrepancy before March 2022, after which the discrepancy increased more than fivefold to 21% as alternative mechanisms expanded [S5]. Some contracts outside China moved toward pricing linked to the MHP-to-sulfate chain rather than LME [S5].
Operational dependency: a converter selecting MHP inherits HPAL restart risk and sulfur intensity, whereas a briquette buyer accepts a different conversion burden and often pays an LME premium [S1]. For conversion plants, the relevant alloy steel equipment specifications must therefore be assessed against the selected feed route rather than a generic nickel-feed assumption.
Payables Show the Market Price of Feed Scarcity
MHP payables had recently risen to 95% for nickel and 92% for cobalt, significantly higher than earlier levels, as MHP supply tightened.
Payables are linked to exchange cash prices and vary with destination and nickel content, so procurement contracts should separate the LME base, payable percentage, assay, freight and conversion charges [S1].
Concentration Makes Conversion Supply a Strategic Variable

Stainless steel represented more than 68% of global nickel demand, according to Benchmark’s Nickel Forecast. This concentration gives Indonesian MHP and Chinese sulfate conversion links outsized importance in battery-material planning.
A trade-flow study found that the precursor-linked system was highly concentrated around China’s conversion capacity and Indonesian MHP and matte supply [S4].
Stainless steel represented more than 68% of global nickel demand, so LME prices continued to reflect stainless-steel fundamentals rather than the battery chemical chain alone [S5]. For converters, this supports separating the nickel-metal benchmark from MHP payables, sulfate conversion economics and precursor demand when evaluating contract coverage.
Procurement Limits and Failure Modes
MHP supply is vulnerable to the interaction of three constraints: nickel ore quota reductions, sulfur shortages and HPAL operating interruptions [S2]. Suspended or restarted projects do not immediately restore full output because production systems require time to restart and stabilize, while alternative ore can increase logistics costs and reduce quality consistency [S2].
High payable rates do not guarantee low all-in sulfate cost. Fastmarkets noted that MHP’s underlying cost can be lower than the briquette route, but higher impurities can increase dissolution and conversion costs [S1]. Contracts therefore need explicit limits for nickel content, cobalt content, relevant impurities, moisture, delivery basis and rejection provisions.
Matte and briquettes remain relevant alternatives for converters whose equipment, impurity tolerance or contracted feed economics do not fit MHP [S1][S6]. However, neither route removes all supply-chain risk: matte remains exposed to mining, smelting and refinery continuity, while briquettes carry the added metal premium associated with LME sales [S1].
Signals Buyers Can Track

Three operational indicators can be monitored without relying on directional price forecasts: Indonesian annual ore quotas, HPAL utilization and maintenance schedules, and sulfur import availability.
Buyers should also separate three price signals in their contracts: LME nickel, MHP payable terms and the sulfate conversion margin. MHP payables had recently risen to 95% for nickel and 92% for cobalt as MHP supply tightened, while the nickel sulphate market’s increased use of alternative pricing mechanisms showed why a single benchmark may not represent the full delivered cost.