Six-inch SiC substrate prices fell below US$500 per wafer from mid-2024 through Q4 2024, with some Chinese-made wafers priced around US$200–300 by June 2026 [S5][S8].
By Q3 2026, supplier capacity exits and depleted inventories had tightened SiC wafer supply, with prices turning upward as demand recovered across key sectors [S1].
SiC substrate price reversal in 2026
The 2026 market did not continue a straight decline. Six-inch prices bottomed in July 2026 after a two-year oversupply cycle, then strengthened through Q3 as smaller producers stopped output and distributors drew down inventories [S1].
This makes a single annual price estimate misleading: the low point and the exit price occurred within the same calendar year.
Price benchmarks by wafer diameter
The useful benchmark ranges in 2026 are US$200–300 for some Chinese-made 150 mm substrates, around US$400 or less for mainstream 6-inch quotations in the 2025 price war, and below US$500 per wafer for much of mid-2024 through Q4 2024 [S5][S8].
These are transaction or quotation benchmarks, not a universal list price. Diameter, defect density, conductivity type, thickness, surface finish, epitaxial readiness, contract volume and qualification status can place two nominally identical 6-inch wafers in different price bands.
Why the 150 mm price decline occurred

The main cause of declining 150 mm substrate prices was excess crystal-growth and processing capacity, amplified by aggressive expansion by Chinese manufacturers [S2][S3]. Mainstream 6-inch quotes fell by more than 20% from mid-2024 to Q4 2024 and reached about US$400 or less during 2025, with some suppliers offering material close to cost [S5].
Raw-material pricing moved in the opposite direction. Bulk black and green SiC powders and grains traded around CNY 6,271 per metric ton in November 2025, a 0.21% weekly increase attributed to firm feedstock costs, downstream demand and supply adjustments [S2]. The divergence matters because a low substrate price can still sit above rising upstream input costs, squeezing supplier margins.
Harder slicing and polishing, slow crystal growth, energy demand and defect-control requirements explain why oversupply initially reduced prices faster than the cost base [S4].
Why buyers were not paying the headline price
SiC substrate selection is governed by usable device yield rather than wafer diameter or purchase price alone. Effective device cost depends on total wafer processing cost divided by the number of electrically good dies, so defect density, geometry and lot consistency can outweigh a small nominal price discount [S3].
A substrate may still require epitaxial growth, photolithography, implantation, high-temperature annealing, metallization, thinning, dicing, packaging and electrical testing [S3]. A wafer with lower purchase cost can therefore be more expensive if its defects reduce downstream yield or delay qualification.
For procurement, the comparison should therefore include at least four criteria: purchase price per wafer, good-die yield, lot-to-lot consistency and downstream qualification effort. A lower-cost 150 mm wafer is unattractive if it fails a customer’s defect specification or interrupts an already qualified device flow.
150 mm versus 200 mm economics

Moving from 150 mm to 200 mm increases usable wafer area by approximately 78%, raising the theoretical number of die per wafer and reducing cost per device [S7]. The gain is not automatic because larger SiC boules require tighter control of the thermal field, material transport, stress and crystal interfaces [S3].
200 mm also raises qualification demands. The investment case is strongest where device footprints scale with wafer area, processing yields are proven and the customer can use the larger die population without creating excess inventory. It is weaker for isolated low-volume programs that cannot amortize qualification or where edge losses, yield loss and machining constraints offset the area advantage.
The comparison below explains why a 200 mm wafer can remain scarce and firmer even while commodity 150 mm material has moved through a price war.
Demand sectors and price sensitivity
AI server power supplies and solar inverter exports supported the Q3 2026 recovery in SiC substrate prices, while electric-vehicle high-voltage demand remained softer than expected [S1]. That mix explains why supply tightened without producing equal strength across every end market.
SiC substrates support electric-vehicle traction inverters, renewable-energy systems, industrial power supplies and aerospace electronics because the material offers higher thermal conductivity, greater breakdown voltage, lower switching losses and better high-temperature operation than conventional silicon [S1]. However, a weak EV market can delay volume orders, while AI and solar demand can tighten supply for smaller product segments.
These applications also differ from SiC’s proposed thermal-carrier use in high-performance computing, where SiC is being evaluated for AI chipset heat dissipation and advanced packaging [S2][S5]. Such emerging demand should not be treated as proof that conventional power-device substrate pricing will follow the same cycle.
Cost drivers, total ownership and sourcing strategy

The purchase price is driven by wafer diameter, material quality, crystal yield, process complexity, supplier capacity, qualification requirements and order volume. Raw powder and grain costs form one input, but crystal growth above 2,000°C, boule yield, slicing, polishing and defect control determine how much usable area reaches the customer [S1][S4].
Certification and qualification raise the effective cost of moving beyond commodity material. Automotive-qualified production, repeatability testing, customer audits and line requalification are less easily replaced by a lower purchase quote. A near-cost 150 mm offer may therefore produce a higher total cost if it increases wafer sort losses or fails qualification.
Total cost of ownership must include substrate purchase, incoming inspection, epitaxy, processing yield, wafer-handling changes, dicing, packaging, test and qualification delay. For a production line, the economically relevant calculation is the cost of good devices and good modules, not the invoice price per wafer [S3].
Buyers should split 2026 procurement into three lanes: qualified 150 mm material with contractual price protection, new 150 mm capacity offered near US$200–300 per wafer, and 200 mm material linked to a specific device roadmap [S1][S8]. Avoid using the US$200–300 benchmark as a universal ceiling for qualified automotive or industrial material.
Standards, qualification and contract controls
SiC substrate procurement is principally controlled through the customer’s device qualification and incoming-quality specification, including defect density, thickness, bow, warp, surface roughness, off-notch, conductivity type and epitaxial compatibility [S3]. There is no single universal standard that turns a spot-price listing into a qualified automotive wafer.
For qualification, the supplier should provide material traceability, defect maps, surface specifications, lot consistency data and evidence from downstream processing. Contract terms should define the quality tier, wafer diameter, electrical and geometrical tolerances, delivery window, price-adjustment formula and remedies for lot rejection.
The defensible 2026 benchmark is therefore a range with conditions. Some Chinese 150 mm wafers traded around US$200–300 in June, mainstream quotes were around US$400 or less during the price-war phase, and established 6-inch prices then recovered from a July 2026 trough as inventories tightened [S1][S5][S8]. Track July-to-September price direction, qualified supplier capacity and 200 mm availability as the next sourcing signals.