Where movement joints are required, they must extend through both the tile and its substrate, with minimum widths of 6 mm for interior tile and 10 mm for exterior tile.
The joint must occur at the junction of horizontal and vertical surfaces, around floor perimeters, where tile meets other hard materials, and at changes in direction, with widths increasing where exposure and movement are greater [S3][S6].
Wall-to-Floor Transition Requirements
Expansion joints are required in both floors and walls and must extend through both the tile and the substrate to accommodate continuing structural movement caused by thermal expansion, contraction, and other effects over the building life [S3].
Movement joints accommodate differential movement between horizontal and vertical tile fields. The tile contractor should align the tile joint with the designated substrate joint and fill the opening with an appropriate sealant rather than grout [S3][S4].
A movement joint should extend through the tile, setting material, and substrate rather than end at the tile surface.
Joint Width and Spacing by Exposure
Interior tile control joints are specified at 4,878 mm to 6,098 mm in each direction with a minimum 6 mm width [S3]. Areas exposed to moisture or direct sunlight use 2,439 mm to 3,659 mm spacing in each direction, also with a minimum 6 mm width [S3].
Exterior tile requires a minimum 10 mm joint width at 2,439 mm to 3,659 mm spacing in each direction. Where the difference between summer highs and winter lows exceeds 40°C, the minimum joint width increases to 13 mm [S3].
These are movement-joint design values, not grout-joint spacing rules. The interval applies to the tile field, while the width controls the opening reserved for sealant and movement.
Compare Detail Types

The main comparison is between a sealant-only tile joint, a prefabricated expansion joint, and a double metal or plastic strip with sealant. For interior installations, the tile joint must extend through the setting material and into the substrate, while interior expansion joints may use prefabricated profiles or double metal or plastic strips with a suitable sealant [S3].
The comparison criterion is not appearance. It is the ability to extend through the tile assembly, remain compatible with the exposure, and receive a sealant suitable for the joint geometry. Exterior expansion and control joints are to be caulked with suitable sealants, and some prefabricated products are recommended by their manufacturers only for exterior use [S3].
Use Cases Across Building Types
Movement joints apply to residential rooms, commercial interiors, exterior installations, tiled walls, tiled floors, and assemblies where tile meets another hard material.
Typical movement-joint locations include door sills, transitions to walls, floor perimeters, columns, corridors, and changes in direction.
For a wet room or other moisture-exposed area, reduce the control-joint spacing to 2,439 mm to 3,659 mm in each direction and retain a minimum 6 mm width [S3]. Locate the tile control joint above the substrate control joint or above a construction cold joint, including where a membrane is used.
Coordinate Tile, Substrate, and Sealant

A wall-to-floor movement joint is a coordinated detail because the tile joint, substrate joint, sealant, and adjoining materials must operate as one assembly [S1][S3]. The consultant is responsible for locating expansion and control joints, while the tile contractor installs the joint in the tile opening under the caulking and sealant requirements of the specification [S3].
Apply concrete control-joint saw cuts within the first 12 hours of concrete placement. Saw cutting of the slab is not the responsibility of the tile contractor [S3]. A tile control joint should be located over a substrate control joint or construction cold joint; where a crack-isolation membrane is used, the tile joint should remain as close as possible to the underlying cold joint [S3].
The sealant must replace grout in the movement opening, while ordinary grout continues in the field joints.
Limits and Failure Modes
Movement joints accommodate differential movement and prevent tile tenting.
Three practical failure modes deserve review. First, a joint that stops at the tile face does not extend through the setting material and substrate as required [S3]. Second, a joint aligned away from a substrate cold joint can place the tile joint over uncracked concrete while the underlying joint opens independently [S3]. Third, an undersized exterior joint can be inadequate where temperature variation exceeds 40°C [S3].
The movement joint is not a substitute for structural crack control. Substrate saw cuts, isolation joints, construction joints, and crack-isolation membranes address structural movement separately, while the tile joint must correspond to those features [S3][S5].
Specification Checklist for the Detail

A complete wall-to-floor detail should identify 6 mm as the minimum interior tile-joint width, 10 mm as the minimum exterior tile-joint width, and 13 mm where summer-to-winter temperature variation exceeds 40°C [S3]. It should also show the joint extending through the tile, setting material, and substrate [S3].
The schedule should state whether the joint uses sealant alone, a prefabricated profile, or a double metal or plastic strip with sealant. For interior work, the selected profile must be suitable for interior use; for exterior work, the profile or sealant must be suitable for exterior exposure [S3].
Field verification should confirm joint width, sealant depth, profile continuity, alignment with any substrate joint, and coordination with the industrial flooring or adjacent floor finish at doorsills and hard-material transitions [S1][S3]. Any deviation from the 4,878 mm to 6,098 mm interior spacing or the 2,439 mm to 3,659 mm wet or sunny-area spacing should be resolved in the design before installation [S3].