A locking assembly can connect a plastic or nylon hub to a shaft when the selected design limits radial pressure, axial force, and bending load to the hub’s allowable limits [S2][S3].
The connection is friction-based and backlash-free [S3].
When Plastic and Nylon Hubs Are Suitable
Locking assemblies are engineered to create frictional shaft-hub connections by generating radial force against both the shaft and the hub bore [S3].
The basic selection requirement is a polymer hub that can accept circumferential compression without cracking, permanent deformation, bore distortion, or pull-out failure. The locking assembly must also satisfy the required torque, axial-force, and bending-moment classes; available designs cover low-torque, medium-torque, and very-high-torque applications, with bending capacity identified separately for each series [S3].
A locking assembly is not a universal answer for every plastic hub. A thin-walled molding, a glass-filled polymer with limited radial compliance, or a hub that must remain fully removable may require a lower-pressure design, a different connection method, or a reinforced hub. The locking assembly should be selected from the calculated load case, not simply because it fits the shaft diameter.
Pressure and Hub Geometry Drive the Decision
The resulting radial force bears against the shaft and the hub bore, making torque capacity dependent on both friction behavior and the compressive strength of the hub material.
This distinction is decisive for polymer applications because a higher-torque assembly is not automatically acceptable merely because it provides more margin against slip. Excess pressure can reduce the useful torque if it damages the hub before the assembly reaches its rated capacity.
Hub geometry must also permit the selected construction. The 7013.0 design sits entirely inside the hub and permits axial movement as the screws are tightened, whereas 7013.1 bears against the hub face and avoids that axial movement when positioning is critical [S2]. For a short polymer boss, the axial space, screw accessibility, and edge distance can determine whether an internally mounted or face-mounted arrangement is practical.
Compare Locking Assembly Types by Load and Fit

Locking assemblies differ in installation length, torque class, bending capacity, axial movement, and contact pressure, so the correct comparison is between the complete product series rather than between shaft diameters alone [S2][S3].
Bridge clearance also affects feasibility. Locking assemblies can fasten different hub types and bridge relatively large fit clearances, making them useful where machining precision is limited [S2]. That tolerance must remain within the selected assembly’s stated range, however, because excessive clearance reduces the reliable contact area and can raise local hub stress.
Design for Polymer Limits, Not Steel Limits
The critical failure modes in a plastic or nylon hub are radial splitting, permanent ovality, bearing-surface creep, screw-slot damage, and loss of preload during service. A metal hub commonly has greater resistance to these loads, but a polymer hub can still work when the design deliberately limits contact pressure and provides adequate wall thickness [S2][S3].
Assembly position and access matter as well. Ringfeder 7013.0 is completely inserted into the hub, creating a compact arrangement because the screws and flange do not project beyond it [S2]. This may suit a molded recess, provided the recess has enough diameter, depth, and edge support for the assembly. A face-mounted 7013.1 requires a flat, load-bearing hub face rather than a thin molded rim that could distort under the flange [S2].
Plastic hubs also require a controlled installation procedure.
Where This Connection Fits Best

A keyed connection may require machining and creates a localized stress concentration, while a shrink fit depends on heating or cooling and a permanent interference relationship; a locking assembly provides a reversible friction fit using standard tools [S5].
The connection is also attractive where contamination must not enter a keyway and where shaft alignment requirements are moderate. Locking assemblies make 360-degree contact with the shaft and mating component, distribute forces around the circumference, and eliminate the failure-prone keyway [S2]. For polymer hubs, that distributed load can be preferable to a concentrated key seat, but only if the hub has sufficient radial and circumferential strength.
The connection is less suitable when the hub is very thin, brittle, highly filled with low-viscosity material, dimensionally sensitive, or exposed to sustained heat that can relax the polymer. It is also a poor fit when axial position can shift, unless a face-mounted model is selected, or when the design requires the hub to be structurally integral with another polymer component that cannot tolerate the assembly’s load path.
The material comparison with acetal and nylon gears is also relevant because hub strength cannot be separated from the surrounding molded geometry. Acetal, Nylon, or Steel Gears for Light Loads provides a useful starting point for evaluating whether a polymer hub has adequate local strength for the intended duty.
Procurement and Qualification Checklist
A polymer-hub locking assembly should be released with four documented checks: calculated torque, calculated axial force, calculated bending moment, and hub compressive stress at the actual bore. The shaft collar and related shaft-selection data can establish the shaft diameter, length, and shoulder arrangement, but the hub remains the component most likely to limit the design. [S2]
The procurement record should identify the locking assembly series and size, shaft diameter, hub bore, hub material, hub outside diameter, minimum wall thickness, axial position requirement, installation length, specified tightening torque, and service temperature. It should also state whether the assembly may be removed during maintenance, because a reusable locking arrangement and a permanently bonded polymer hub have different service expectations [S5].
Inspection should verify bore concentricity, hub roundness, cracking around the bore, screw access, axial travel, and uniform contact after tightening. This is especially important when comparing a standard lock nut approach with a full locking assembly, because the two products solve different shaft-hub problems.
The next engineering decision is measurable: identify the calculated torque, axial load, bending moment, hub material, bore diameter, and wall thickness, then compare them with the selected assembly’s published limits and a prototype test. If any comparison depends on assumed polymer strength, the design is not ready for purchase.