The seal joint has a joint efficiency of approximately 70–75% of the strap breaking load, while the punched or no-seal joint has a joint efficiency of approximately 85%.
The seal joint is suitable for strapping small surfaces, while S2 and S3 describe manual and automatic tools for steel and plastic strapping and seals sized for a selected tool and load.
Crimp seal and TIG weld mechanics
A crimp seal joint places a steel sleeve over two overlapping strap ends and mechanically deforms the seal and strap into a wavy interlock. Crimp-type sealers press the edges of the strap and seal into those waves without cutting them, so holding power comes primarily from friction generated by the deformed steel [S2][S3].
Crimping damages the steel strap on both sides, and mechanical wearing of the crimping unit decreases joint efficiency.
Strength, fatigue and impact performance
The crimp seal joint has an efficiency of approximately 70–75% of the strap breaking load, while the punched or no-seal joint has an efficiency of approximately 85%. The punched or no-seal joint therefore has approximately 10–15 percentage points more joint efficiency than the seal joint.
Crimp seals can still provide high static and dynamic holding power. Specifically shaped seals create friction against the strap, and crimp joints are used in carloading applications where the secured load experiences severe impact [S2]. The lower efficiency figure therefore does not mean that every crimp joint is unsuitable for impact service; it means the design margin must be established from the complete joint, not from strap tensile strength alone.
For package design, Signode directs users to ASTM D3953 minimum break strengths for package design and safety-factor purposes [S2]. This matters because a strap can meet its material specification while the assembled closure becomes the limiting component. The same principle applies when comparing tools: tension repeatability, joint geometry and tool wear all influence the effective system strength [S4].
Tooling, automation and operating constraints
Crimp tooling can be deployed as a manual tensioner plus separate sealer, a pneumatic combination tool, or an automatic machine that feeds and crimps a steel strap seal. A sealer must match the seal dimensions, while automatic installations must also match the machine brand, model and magazine-feed geometry [S3][S7].
The additional steel seal is a disadvantage of the seal joint, and the punched or no-seal joint requires no additional material.
For a manual operation, place the specified seal over the overlapping ends, tension to the required level, crimp with a matched sealer and cut the excess tail [S7]. Push-type seals are installed before tensioning, while snap-on or open seals go over the strap ends during or after tensioning [S2][S3].
Seal sizing and consumable control
Seal width must match strap width, while seal length and thickness should be selected according to the strap and load. The strapping band and strapping machine should therefore be specified as one interface, not as unrelated purchases [S3].
Published dimensional examples include 32 × 0.6 mm seals for 12.7, 15.9 and 19.1 mm strap, push-type seals from 22 mm long for 12.7 mm strap to 75 mm long for 31.8 mm strap, and a 55 × 0.9 mm open-flange seal for 25.4 and 31.8 mm strap. Magazine seals include 28 × 0.6 mm for 19.1 mm strap and sizes up to 75 × 1.2 mm for 50.8 mm strap [S3].
GB/T 39040-2020 expresses a steel seal as style code, thickness, width and length; the example P0.8×19×45 identifies a push-type seal, 0.8 mm thick, for 19 mm strap and 45 mm long [S3]. A longer, thicker seal can increase joint capacity, but it requires compatible sealer jaws, which makes replacement consumables and tooling inventory part of the operating cost [S3].
Crimped versus welded joint decision
The punched or no-seal joint has an efficiency of approximately 85%, compared with approximately 70–75% for the seal joint. For installation flexibility, the crimp seal wins where separate tensioners, sealers and several seal sizes support mixed manual work, while TIG welding is more dependent on a matched automated head [S2][S3].
For consumables, TIG welding avoids replacement steel seals, whereas a crimp system consumes one sleeve per closure and must maintain correct seal dimensions and compatible jaw geometry [S3].
Use a crimp seal when the load is suitable for the lower joint efficiency, the application requires the established manual or pneumatic sealer format, and consumable logistics are acceptable. Use TIG welding when the closure must approach full strap capacity, impact or fatigue exposure is significant, or a high-throughput fixed machine justifies dedicated welding equipment. Neither option should be selected from nominal strap strength alone; validate the assembled joint and the tool-machine combination before releasing production use [S1][S2].
Failure modes and quality control
Crimp joints are vulnerable to incorrect seal size, incomplete closure, skewed overlap, worn sealer jaws and degraded friction surfaces. Notch-type sealers cut into the seal and strap to form tabs, whereas crimp-type sealers deform the edges into waves without cutting them, so tools and seals must not be mixed by assumption [S2].
Weld joints require inspection for incomplete fusion, misalignment, oxidation, contamination or an undersized overlap. TIG shielding protects the molten steel, but the process still depends on clean metal, a functioning gas circuit and a sound electrode [S1]. Tool wear also affects mechanical joints: crimp units can reduce joint efficiency as the crimping unit wears, while punched heads lose efficiency as cutting units wear [S1].
Qualification should therefore include joint pull testing at the intended tension, inspection under ASTM D3953 design criteria where applicable, checks for complete closure and alignment, and periodic verification of tool wear. Track the seal dimensions, strap width and machine model as controlled process variables, because a nominal 19 mm seal does not create a repeatable joint if it is fitted to a different strap width or fed through incompatible jaws [S2][S3].
Before approving a joint design, record the strap grade and breaking load, seal or TIG-head configuration, applied tension, tool model, joint efficiency and the test method used. A change in any of those inputs, including seal supplier or seal thickness, requires requalification of the complete closure rather than a change to the packaging instruction alone.