UL 746 relative thermal index is the temperature at which specified properties retain 50% of their initial value after 100,000 hours of thermal exposure [S4][S5].
The 100,000-hour reference exceeds 11 years of uninterrupted operation, making RTI a long-duration material-aging index rather than a short-term heat-deflection value [S5].
What RTI Measures for Continuous Service
Relative thermal index describes a plastic's ability to retain a designated physical or electrical property during prolonged exposure to heat [S1][S2]. Under the cited UL definition, the temperature is expressed in °C and is tied to a 50% property loss after 100,000 hours [S4].
Engineering plastics include ABS, polyamides, polycarbonate, PBT, LCP, PAI, and fluoropolymers, each with a property-specific RTI under UL 746 [S1][S4]. A material-grade RTI is therefore not a universal statement that the component will work unchanged under every thermal and mechanical condition.
The engineering plastic family can vary widely by polymer, grade, colorants, flame retardants, reinforcement, and processing history. The grade designation and the property being qualified must travel with the purchase specification.
UL 746 Testing Basis and Property Limits
The Relative Thermal Index is the temperature at which a material's properties decrease to 50% of their initial value after long-term exposure for 100,000 hours [S5].
Electrical insulation, mechanical impact, and mechanical strength can produce different RTI values for the same polymer because each property decays at a different rate [S5]. The result must always specify the property, color, grade, and relevant material thickness or construction.
Selecting RTI by Polymer Family

These values belong to the stated grades and must not be transferred automatically to unreported variants.
A defensible comparison uses four criteria: the qualified property, continuous-use temperature, service load, and exact grade. Polymer family alone is too coarse, and changing thickness, reinforcement, color, or additive package can invalidate a direct comparison [S4][S5].
Who Should and Should Not Use RTI
RTI is suitable for early material screening, thermal endurance comparison, and procurement control when the part has sustained exposure near the selected temperature [S2][S4]. It is especially relevant to electrical insulation, molded housings, gears, bushings, and other components needing predictable retention of a defined property [S1].
RTI is not a replacement for creep, fatigue, impact, chemical compatibility, or product-level validation. Creep is permanent deformation under prolonged stress below the elastic limit, and the cited RTI presentation explicitly states that RTI does not address creep [S1].
RTI also does not cover short thermal spikes, which must be evaluated against separate short-term properties and the actual duty cycle [S5]. For molded components exposed to solvents or cleaners, chemical resistance remains a separate selection problem rather than an RTI assumption.
Service Life, Stress, and Environmental Constraints

An RTI is derived from thermal aging, not from a guarantee that every design property remains unchanged at the index temperature [S1]. The tracked electrical or mechanical property reaches a defined endpoint during the 100,000-hour evaluation, and other properties may retain more or less capability [S5].
Continuous-use temperature is also affected by polymer structure, elapsed time, and loading level, while additives and reinforcements can alter the result [S5]. A component held under bending, compression, or tension therefore needs an appropriate mechanical assessment in addition to its RTI.
Thermal exposure history matters because long-term degradation can accumulate through chemical reactions [S1]. Frequent excursions, local hot spots, sterilisation cycles, radiation, moisture, and chemical exposure need separate qualification, and each condition can shift the effective aging rate.
Specifying and Verifying the Correct RTI
A procurement specification should name the polymer, manufacturer, grade, RTI property category, color, thickness, and applicable certification or laboratory report [S4]. It should also state whether the requirement is electrical insulation, mechanical impact, or mechanical strength, because those values can differ for one material [S5].
Requesting the RTI by generic resin name leaves avoidable ambiguity. These entries show why grade-level data belong in the datasheet and purchasing system.
For design verification, compare the service temperature with the qualified RTI, inspect load and creep separately, and validate the finished assembly. Where solvent exposure is part of the duty, use the separate framework in Engineering Plastic Solvent Resistance: Selection Criteria.
Temperature Limits That Common Confusion

Heat-deflection temperature describes short-term resistance to deformation under a specified load and test method, whereas RTI addresses property retention over extended thermal aging [S1][S4]. A glass-filled PBT blend is listed at 193°C RTI in one published table, but that value does not make its short-term heat-deflection temperature equal to 193°C [S4].
Glass transition temperature, melting point, Vicat softening temperature, and continuous-use temperature answer different engineering questions. The valid continuous-operation threshold is the RTI assigned to the correct property and grade, interpreted together with the actual load and environment [S1][S2][S5].
Track three procurement signals before release: the supplier's RTI property category, the exact grade and color, and whether any thickness, reinforcement, or processing change occurred since qualification. These controls prevent a generic material-family temperature from being treated as a finished-part limit.