Engineering-plastic compatibility must be checked chemical by chemical because concentration, temperature, exposure time, and applied load can change a rating from resistant to unsuitable [S3][S4].
The practical choice spans fluoropolymers, PEEK, PPSU, PPS, PEI, POM, PA, PET, PC, polyethylene, polypropylene, and PVC, with PTFE, PFA, and FEP providing the broadest solvent tolerance in common comparisons [S1][S5].
What a Chemical Resistance Chart Actually Measures
A resistance chart rates a defined polymer and chemical combination under specified conditions, not an unconditional approval for every process configuration. MCAM's chemical resistance guide provides information on which chemicals and fluids are known to attack or be compatible with engineering plastics [S1].
The rating systems differ, so codes must not be transferred mechanically between suppliers. The supplied chemical resistance chart legend defines A as no attack or possible slight absorption with negligible effect on mechanical properties, and B as slight attack by absorption [S2].
Temperature and concentration notation also needs interpretation.
Solvent Selection by Polymer Family
For strong organic-solvent service, fluoropolymers such as PTFE, PFA, and FEP rank excellent against the solvent categories covered in common laboratory comparisons, while PVC, polycarbonate, and polystyrene are attacked by most solvents [S5].
Polyethylene and polypropylene are more selective. HDPE and LDPE are rated limited for ketones such as acetone and methyl ethyl ketone, whereas polypropylene is rated good for that group; both are less dependable for chlorinated solvents than fluoropolymers [S5].
High-performance thermoplastics can provide a different balance of mechanical strength and resistance.
Four Variables That Change the Selection

Concentration, temperature, contact time, and mechanical load are explicit selection variables in the Curbell plastics chart [S3].
Chemical mixtures create another boundary. Harrington states that concentration, chemical combinations, temperature, internal pressure, weather exposure, external mechanical stress, and product quality can alter chemical resistance in plastic piping systems [S4]. A rating for a neat solvent cannot be assumed to cover a blended solvent, a catalyzed mixture, or a contaminated process stream.
Permeation also matters in closed containers. The wall thickness, closure design, headspace, and storage duration therefore belong in the specification, not only the resin name.
Where Engineering Plastics Fit, and Where They Do Not
Engineering plastics fit pumps, valve components, bearings, seals, tubing, tanks, and liners where the chemical, concentration, temperature, duration, and mechanical duty are all documented. MCAM's database covers conditions where chemicals are known to attack or remain compatible with engineering plastics [S1].
They are not a universal substitute for metal, glass, or fluorinated elastomer components. The 2026 guide separates laboratory containers and tubing from wetted materials used in pumps, valve trim, and gaskets, and it does not cover glove selection or chemical-storage segregation rules [S5].
For common industrial degreasing, solvent choice also affects the disposal and handling process rather than only the wetted part. The comparison of D-limonene and petroleum solvents for industrial degreasing provides a separate decision frame for solvent performance and handling.
Common Failure Modes and Test-Planning Triggers

Three rating levels distinguish practical outcomes.
Harrington's piping guide uses a different decision scale: A is acceptable, C means caution and testing are necessary, X means unsuitable, and a dash means insufficient data requiring testing under actual use conditions [S4]. Its metal-rating criteria quantify penetration as less than 2 mils per year for A, less than 20 mils per year for B, and less than 50 mils per year for C [S4].
Testing is warranted whenever the chart entry is limited, the concentration exceeds the listed case, or process temperature exceeds the rating condition. Curbell's chemical resistance chart states that resistance also depends on concentration, time, and temperature [S3].
How to Use a Chart Without Over-Specifying
A defensible workflow starts with the exact chemical name, concentration, process temperature, exposure duration, and load. Select the polymer with a suitable rating, then verify maximum service temperature, grade, reinforcement, filler, and manufacturer-specific limitations [S1][S3][S4].
These examples show why chemical identity and temperature must be read together rather than reduced to a family-level label.
The industrial solvent compatibility overview is useful for narrowing the solvent side of the screen, while engineering plastic selection guidance covers the material-design context. A chemical reagent guide is also relevant when concentration, purity, or formulation data must be tied to the service condition.
Use the chart to eliminate unsuitable candidates, not to sign off a critical component. For continuous solvent service, unspecified blends, elevated pressure, or mechanical loading, verify the exact resin grade with the manufacturer and conduct coupon or component testing under the actual exposure profile before release.