A published EVA film for V-process vacuum casting exceeds 20 MPa tensile strength and 600% elongation [S3].
The comparison covers shape adaptation, thermoformability, drawdown, material use, casting integrity, and process control for foundry vacuum forming and investment casting.
Decision Criteria for V-Process Film
Film selection should be based on four measurable criteria: elongation, thermoformability around complex geometry, thickness consistency, and ease of removal after casting. A published EVA film for V-process vacuum casting exceeds 20 MPa tensile strength and 600% elongation [S3].
The decision rule is direct: specify EVA for deep draws, sharp features, large mold surfaces, and complex castings; qualify LDPE only when its simpler forming behavior and material economics compensate for the loss of stretch and shape conformity.
Why EVA Fits Complex Molds
EVA is less crystalline than LDPE, producing broader diffraction peaks and, in some cases, a halo pattern associated with amorphous structure [S1].
Commercial V-process grades are formulated for thermoformability, high elongation, deformability, impact strength, puncture resistance, flex-crack resistance, and easy peeling [S2].
EVA film is suitable for shaped or pointy molds and is described as ideal for complex, contoured, or sharp-edged molds [S2][S3]. It is also the practical choice where film removal must avoid damage to delicate cast surfaces.
EVA and LDPE Compared

On extension, EVA has the documented advantage: dedicated V-process film exceeds 600% elongation and 20 MPa tensile strength [S2][S3]. LDPE remains a flexible, semi-transparent film produced by both blown-film and casting processes, but the cited LDPE sources do not provide equivalent V-process-specific limits [S8].
On mold conformity, EVA offers superior adaptability to complex shapes, while LDPE is easier to specify from general-purpose film grades. On thickness control, one EVA producer reports average deviation of ±3% using an auto-gauge-controlled blown-film line [S2]. On formulation freedom, LDPE can be used as a base in polyethylene film constructions or blended with HDPE and EVA, whereas EVA’s vinyl acetate content is integral to its elastic and stress-cracking behavior [S7][S5].
On casting economics, EVA’s downgauging capability can reduce resin use per casting, but LDPE may win when its lower material cost offsets scrap and rework. No sourced unit price supports a universal cost claim, so the valid comparison is qualified trial data on the same casting family, including film weight, rejected castings, labor, and rework.
Application Fit by Casting Geometry
LDPE is more defensible for relatively flat or gently contoured patterns, short draw paths, and trials where the plant already controls LDPE forming and peel-out successfully.
The V-process line must hold the film at a stable temperature and stretch it without local wrinkling. A molding line that cannot control drawdown, vacuum distribution, or film removal should not be compensated for simply by selecting a thicker film.
Limits, Failure Modes, and Trial Qualification

Thicker film can improve draw strength but does not cure poor sealing, uneven vacuum, sharp mold radii, or excessive draw ratio.
Use the same casting trials to compare film mass per part, elongation at failure, seal failures, vacuum losses, film rupture locations, casting surface defects, peel force, dimensional variation, and rejected part count.
LDPE/EVA blended films also exist, and PE processing guidance permits LDPE as part of a film construction or blend with HDPE and EVA [S7]. Such blends complicate material naming: specify the complete formulation, vinyl acetate content where relevant, gauge tolerance, width, and lot performance rather than accepting “EVA film” as an adequate purchasing description.
Specification and Purchasing Requirements
Purchase V-process film as an engineered consumable, not a generic packaging film. Require the supplier to state grade, gauge, tensile strength in MPa, elongation in percent, thermal shrinkage in percent, width, roll length, and thickness-deviation method. The available supplier specification identifies four gauge bands, more than 20 MPa tensile strength, more than 600% elongation, and no more than 4.5% thermal shrinkage [S2].
Film width is a production constraint: one V-process EVA supplier lists roll width up to 4,400 mm and a minimum order of 1,000 kg [S3]. Confirm the machine’s maximum sheet width before evaluating a supplier, and require production samples from the proposed width rather than relying only on resin-grade data [S2][S3].
Final approval should follow a documented trial: one LDPE baseline and one EVA grade on the same mold, using controlled film thickness, forming temperature, vacuum level, draw rate, and cooling conditions. Select EVA when it reduces forming failures or rejected castings enough to offset material and changeover costs; retain LDPE only when it meets surface, dimensional, and integrity requirements with better measured yield.