FKM is the stronger choice for fuel and oil service, with typical continuous capability near 200°C and compound-specific limits up to about 230–250°C [S1][S5][S9].
Silicone covers a wider low-temperature envelope, reaching about −60°C in common compounds, but it should not be specified for prolonged contact with gasoline, petroleum oils, or hydrocarbon solvents [S1][S2].
Temperature ranges by material and compound
Marcor lists 70 Shore A silicone compounds with low-temperature limits of −60°C or −55°C and high-temperature limits of 205°C or 320°C.
These numbers are not interchangeable material specifications. The selected compound, section geometry, media, compression, and exposure duration determine usable performance. FKM offers continuous temperature performance up to approximately 230°C.
Silicone is normally the better low-temperature material, while FKM is normally preferred for hot fuel and oil.
Fuel, oil, and hydrocarbon exposure
FKM combines heat resistance with strong performance around oils and many chemicals and is suited to fuel systems and other demanding service environments.
Silicone should not be used where prolonged contact with fuel is expected.
Temperature alone cannot determine compatibility. A seal operating at 180°C in clean hot air may suit silicone, while the same temperature in diesel can require FKM. For real fuel-system qualification, also assess FKM seal swelling in biodiesel and conventional diesel.
Decision matrix for seals and O-rings

For fuel compatibility, FKM is the clear choice: it resists gasoline, oils, lubricants, and aromatic hydrocarbons, whereas silicone is limited in prolonged hydrocarbon service [S1][S5]. For cold service, silicone wins, with listed compounds reaching −60°C to −75°C, compared with −30°C for common FKM grades [S2].
FKM and silicone generally have typical high-temperature capabilities around 200°C, while FKM offers continuous temperature performance up to approximately 230°C and Marcor lists a silicone compound with a high-temperature limit of 320°C. These are compound ceilings, not blanket service ratings.
FKM is harder and more durable than silicone, while silicone is more flexible and elastic. For outdoor weathering, both resist UV and ozone, but silicone is widely available in medical, food-contact, and biocompatible grades [S1][S3].
Application selection by service envelope
Use FKM for fuel-system O-rings, hot hydraulic or pneumatic seals, chemical processing, and static or dynamic sealing where hydrocarbon exposure is significant. FKM compounds around 200°C combine heat resistance with resistance to mineral oils, synthetic lubricants, fuels, and aromatic hydrocarbons [S5].
Use silicone for static seals in hot air, medical equipment, food and pharmaceutical applications, electrical insulation, and outdoor equipment exposed to weather. FDA 21 CFR 177.2600-compliant silicone grades are available, as are USP Class VI platinum-cured grades [S1][S2].
Do not use either material as a universal answer. EPDM is particularly useful around hot water and steam, FKM combines heat resistance with strong performance around oils and many chemicals, and silicone maintains flexibility across a broad temperature range. For steam or glycol service, compare FKM against EPDM rubber rather than defaulting to heat resistance alone.
Compression set, movement, and service life

FKM normally retains sealing geometry better under sustained heat and pressure because its compression set is excellent; silicone is generally acceptable for static, low-stress applications but is less suitable for repeated dynamic motion [S1].
For fuel-system integrity, this distinction matters because fuel exposure and compression can occur together. A compound with adequate bulk temperature resistance may still fail if it swells excessively or loses recovery under sustained closure pressure. The material comparison for fluororubber should therefore include recovery, media compatibility, and gland conditions.
Sealing function also affects the choice between static and moving interfaces. FKM is suitable for both static and dynamic sealing and is often selected for rotating or reciprocating service. Silicone is normally specified for static seals because its low tear strength and abrasion resistance limit long-term dynamic life [S1][S5].
Sourcing, standards, and qualification checks
Silicone compounds should likewise be identified by designation, durometer, low-temperature limit, high-temperature limit, and compliance requirement. Examples include 70 Shore A silicone rated from −60°C to 205°C and 70 Shore A silicone rated from −55°C to 320°C.
Validate the final seal in the actual fuel, oil, or cleaning medium at operating temperature and pressure. For adjacent material decisions, silicone rubber offers the appropriate low-temperature and weathering context, while nitrile rubber remains a separate oil-and-fuel comparison outside the FKM-versus-silicone decision.
The next specification checkpoint is the compound data sheet: require the continuous and intermittent temperature ratings, fuel exposure time, swelling data, compression set, hardness, and regulatory status before approving either material.