A hand torque chart is a reference for a specified thread size, strength grade and assembly condition, not a substitute for the joint design.
The chart data covers SAE Grades 2, 5 and 8, metric Classes 8.8, 10.9 and 12.9, selected stainless steel and nonferrous fasteners, and the friction assumptions behind them.
Why torque alone does not define bolt preload
A torque wrench measures applied torque, while the fastener carries tensile preload; thread friction and friction beneath the rotating head or nut consume part of the wrench input. Oil, coating, washer condition, surface texture and operator error can therefore change bolt tension at the same displayed torque [S1][S2].
For the worked M10 × 1.5 Class 8.8 example, proof load is 580 N/mm² multiplied by a 58.0 mm² tensile stress area, giving 33,640 N. Applying a 75% proof-load target gives 25,230 N, and T = K × F × d produces 50.46 N·m with K = 0.20 and d = 0.010 m [S2].
That calculation estimates one preload condition; it does not verify the capacity of the bolt, housing, gasket or tapped hole. Portland Bolt states that determining the correct torque requires experimentation under the actual joint and assembly conditions because lubrication and surface texture materially affect the torque-tension relationship [S1].
Metric selection by property class and thread
For M10 × 1.5 Class 8.8, the 75% proof-load calculation gives 50.5 N·m, equivalent to about 37 lbf·ft. Imperial’s separate coating-based table lists 51.0 N·m for zinc-plated fasteners and 46.0 N·m for unplated fasteners, confirming that surface condition belongs in the selection record [S2][S5].
At the same diameter and property class, a fine thread generally produces a higher calculated torque because its tensile stress area is larger. Imperial’s Class 8.8 examples show M8 × 1.25 at 25.0 N·m for zinc-plated and 23.0 N·m for unplated fasteners, while M8 × 1.00 is listed at 27.0 and 24.5 N·m respectively [S5].
Class 10.9 values also rise with diameter: Imperial lists M6 × 1.0 at 15.5 N·m, M10 × 1.5 at 75.0 N·m, M12 × 1.75 at 160.0 N·m and M16 × 2.0 at 310.0 N·m for zinc-plated fasteners [S5]. The calculation basis uses proof stresses of 830 MPa for Class 10.9 and 970 MPa for Class 12.9 in the metric reference tables [S2].
SAE Grade 2, 5 and 8 comparison

For a 1/2-13 SAE Grade 5 bolt, a 75% proof-load target and nut factor of 0.20 yield 75.4 lbf·ft, or about 102 N·m. A chart using another friction basis can publish a different setting for the same nominal bolt, so the chart basis must be checked before the number is copied into a work instruction [S2].
Bolt Depot’s US Recommended Bolt Torque table lists 1/2-inch coarse-thread bolts at 37 lbf·ft for Grade 2, 57 lbf·ft for Grade 5, and 80 lbf·ft for Grade 8. For 3/8-16, the corresponding values are 15, 23 and 33 lbf·ft, while 5/8-11 is listed at 73, 112 and 159 lbf·ft [S4].
Portland Bolt’s ASTM A307 table lists 1/2-13 fasteners at 29 lbf·ft for plain finishes and 37 lbf·ft for galvanized-and-waxed finishes. Its 3/8-16 values are 20 lbf·ft plain and 25 lbf·ft galvanized-and-waxed, showing why coating and lubrication must be identified rather than averaged into a generic Grade 2 value [S1].
Fine threads and stainless steel fasteners
Fine-thread values exceed coarse-thread values when diameter, grade, preload target and nut factor are otherwise equivalent. Bolt Depot lists a 1/2-20 Grade 5 value of 64 lbf·ft against 57 lbf·ft for 1/2-13, and a 5/8-18 Grade 8 value of 180 lbf·ft against 159 lbf·ft for 5/8-11 [S4].
Stainless steel requires its own chart entry rather than a scaled steel value. Imperial lists 316 and 18-8 stainless at 1/2-13 as 542 and 517 lbf·in, respectively, compared with 565 and 541 lbf·in for 1/2-20. The listed 3/8-16 values are 247 lbf·in for 316 and 236 lbf·in for 18-8 [S5].
Bolt Depot gives 18-8 stainless values of 43 lbf·ft for 1/2-13 and 45 lbf·ft for 1/2-20, plus 93 and 104 lbf·ft for 5/8-11 and 5/8-18. These charts use different fastener categories and calculation bases, so the values should not be merged into one universal stainless table [S4][S5].
Maximum metric values are not assembly targets

The metric maximum chart for lightly oiled coarse threads calculates tension at 85% of proof load, which is a different basis from the 75% target used in the worked reference tables [S2][S3]. A maximum chart therefore answers a capacity-oriented question, while an assembly chart estimates a wrench setting for a selected preload.
The distinction changes the numerical setting even when the bolt grade and diameter are unchanged. The 75% target used for M10 × 1.5 Class 8.8 produces 50.5 N·m, whereas the 85% basis cannot be substituted into that equation without recalculation [S2][S3].
Portland Bolt labels its values as suggested starting estimates, and its ASTM A307 table lists a proof load of 4,700 lbf, a clamp load of 3,525 lbf, and tightening torques of 29 lbf·ft for plain and 37 lbf·ft for galvanized-and-waxed 1/2-13 fasteners.
Torque wrench limits for hand work
The wrench must cover the intended setting with meaningful resolution, because a small fastener may require graduation in lbf·in while a larger bolt is commonly tightened in lbf·ft. The calculated 1/4-20 Grade 5 value is approximately 101 lbf·in, so a wrench whose smallest increment is too coarse cannot apply that setting accurately [S2].
Imperial’s fastener chart applies the relationship T = R D P for Grade 5 and Grade 8 values, with T as torque, D as nominal diameter and P as clamp load. Its structural bolt table includes 1/2-13 Grade C at 12,800 lbf clamp load and 45–62.5 lbf·ft assembly torque, versus 9,050 lbf and 37–50 lbf·ft for Grade B [S5].
Socket-drive capacity is a separate limit from fastener torque. The comparison of 1/4 versus 3/8 versus 1/2 inch socket drive torque is useful when selecting the hand tool, but the drive rating must exceed the wrench output while the fastener, joint and technique remain the controlling factors [S5].
Sources, standards and the working record

The metric reference calculations use ISO 898-1:2013 tensile stress areas and proof-load stresses, while the SAE calculations use SAE J429 proof stresses of 85,000 psi for Grade 5 and 120,000 psi for Grade 8 over the listed sizes. Grade 5 uses 74,000 psi above 1 inch, and the table must not be extrapolated to larger diameters [S2].
These published tables are calculated references, not torque specifications issued by ISO. The proper assembly target depends on joint design and tightening procedure, while the chart calculation depends on proof stress, tensile stress area, nominal diameter, preload fraction and nut factor [S2].
For a traceable work instruction, record the bolt designation, diameter and pitch, grade or class, coating, lubrication, target preload and nut factor. Recheck the fastener marking, thread form, wrench range and joint condition before applying a listed value, because a diameter alone does not identify the assembly [S1][S2][S4].
A controlled torque record should also capture the wrench identification, calibration status and achieved setting. If preload must be verified rather than inferred, use an instrumented fastener or tension-indicating method because the same wrench setting can produce different bolt tension under different friction conditions [S1][S2].