The manufacturer pairs pressure bars with tampers in its high-compaction systems [S6].
Pressure-bar compaction architecture
A high-compaction screed uses more than vibration alone to consolidate the asphalt behind the screed. VÖGELE specifies its high-compaction technology with tamper and pressure bars, while the AB 600 documentation separates the pressure-bar drive from the maximum compactor speed [S3][S10].
These figures identify adjustment points within the pressure-bar mechanism rather than a universal compaction specification for every material, layer thickness, or paving width.
Pressure-bar systems should be treated as a combined compaction arrangement. The wider VÖGELE product family covers vibrators and the high-compaction system with tamper and pressure bars, confirming that pressure bars form one part of a broader compaction package rather than a replacement for every vibratory function [S6][S10].
AB 600 versus AB 500 and AB 220
The AB 220 is available in two screed versions, with listed widths of 1 ft 8 in to 11 ft 6 in for V, TV and 3 ft 11 in for TV [S8].
The comparison matters because “pressure bar” is not a complete model specification: the AB 500 is described through the tamper-and-pressure-bar system, while the AB 220 TV uses tamper and vibrators and is positioned in the Mini Class [S6][S8].
Fixed-width and extending screed roles

VÖGELE separates compact-class extending screeds from high-capacity fixed-width machines: the SB 300 covers paving widths from 3 to 16 m and layer thicknesses up to 50 cm depending on the tractor unit, while the SB 350 covers widths from 3.5 to 18 m [S4][S7].
The SB 350 was designed for the SUPER 3000-3(i), and its stated role is large-width asphalt paving and thick base courses [S4][S5]. The SB 300 is described as a specialist in jointless paving, with the same stated width range of 3 to 16 m and a maximum layer thickness of 50 cm, subject to the tractor unit [S7][S10].
The AB 220 addresses a different operating scale. Its TV version, which combines tamper and vibrators, was designed for the SUPER 800-5 P and is positioned for high precompaction in the Mini Class [S8]. An extending screed such as the AB 600 therefore belongs in variable-width work planning, while fixed-width models such as the SB 300 and SB 350 suit defined paved widths and large stationary-production configurations [S3][S4][S7].
Material and production limits
The AB 220 lists basic extension width in feet and inches, while the SB 300 and SB 350 use metric paving ranges of 3 to 16 m and 3.5 to 18 m [S4][S7][S8]. Unit conversion is necessary during equipment comparison, but the published manufacturer values remain the controlling references for each model.
Layer thickness is another constraint. The SB 300 reaches up to 50 cm depending on the tractor unit, and the SB 350 is intended for thick base courses, while the AB 220 documentation gives no equivalent layer-thickness limit [S4][S7][S8].
That distinction is practical for asphalt paving because screed temperature control, material delivery, layer depth, and compaction settings must be evaluated together rather than treating pressure-bar output as an isolated performance figure [S3].
Procurement criteria for asphalt paving

Specify the pressure-bar arrangement against four measurable criteria: paving width, layer thickness, compaction system configuration, and machine compatibility.
The AB 220 is an extending screed available in two versions, with listed widths of 1 ft 8 in to 11 ft 6 in for V, TV and 3 ft 11 in for TV [S8].
For fixed-width projects, compare the SB 300 against the SB 350 using width and thickness. The SB 300 spans 3 to 16 m with layer thickness up to 50 cm depending on the tractor unit, while the SB 350 spans 3.5 to 18 m and is built for large widths and thick base courses [S4][S7].
Finally, verify the actual compaction package with the supplier, as the AB 500 documentation names tamper and pressure bars [S6].
Commissioning checks before asphalt production
For fixed-width fleets, record the paver-screed pairing and operating width. The SB 300 supports 3 to 16 m, while the SB 350 supports 3.5 to 18 m and was designed for the SUPER 3000-3(i) [S4][S7]. The tractor unit remains material because the SB 300 layer-thickness limit depends on it [S7].
Track achieved density and surface quality against the project specification after trials, using project-defined density criteria and test methods rather than relying on an unverified compaction threshold.