REQUEST FOR QUOTE → Request a quote
SpecForge Editorial Team

Iridium Recovery from Spent PEM Electrolyzer Stacks

Table of Contents
  1. What Iridium Can Be Recovered from a Spent Stack
  2. Stack-Level Mass Versus Actual Iridium Content
  3. How Recovery Yield Changes the Supply Picture
  4. Comparison of Recycling Routes for Spent Stacks
  5. Closed-Loop Iridium and Ionomer Recovery
  6. What Spent-Stack Owners Should Contractually Require
  7. Limits on Reusing Recovered Iridium
Iridium Recovery from Spent PEM Electrolyzer Stacks

A 1 MW PEM electrolyzer stack contains approximately 300–500 g of iridium at stack level, making spent catalyst-coated membranes the main iridium-bearing fraction.

Recovering iridium from end-of-life stacks can supply a meaningful share of future demand, but collection, recycling delay, technical recovery, catalyst loading, and system design determine the result.

What Iridium Can Be Recovered from a Spent Stack

The practical answer is not a fixed percentage because PEM electrolyzer stacks do not have one uniform construction.

Each megawatt of PEM electrolyzer capacity currently requires approximately 0.3 to 0.5 grams of iridium per kilowatt at the stack level [S7]. That converts to approximately 300–500 g of iridium per 1 MW of installed stack capacity [S7]. The actual mass in a specific stack depends on its rated power, catalyst-coated membrane area, catalyst loading, and whether the estimate includes all stack-level hardware.

If the iridium-bearing catalyst layer is separated and processed with a technically effective recovery route, the recoverable quantity can approach the metal originally present. The material-flow study does not present one universal plant-scale recovery percentage, but it calculates secondary supply using technical recovery efficiency, collection efficiency, losses, and recycling delay [S1].

Stack-Level Mass Versus Actual Iridium Content

For commercial planning, use the 0.3–0.5 g/kW figure as a screening estimate, not as a weighbridge value for every stack [S7]. A 2 MW stack would therefore fall into a nominal range of 0.6–1.0 kg of iridium before processing losses, while a 5 MW stack would fall into a nominal range of 1.5–2.5 kg.

Heraeus recycles platinum, iridium, ruthenium, palladium, and ionomers from catalyst-coated membranes [S3]. Heraeus lists MEAs, CCMs, bipolar plates, PTLs, catalyst inks, pastes, coatings, and spent electrocatalysts among materials processed in hydrogen-system recycling [S3].

This matters because the practical recoverable value is tied to catalyst recovery, not to gross stack weight. A stack containing nominally 500 g of iridium will not deliver 500 g of saleable iridium unless the process achieves high recovery and the recovered material meets the buyer’s refining and quality requirements.

How Recovery Yield Changes the Supply Picture

how much iridium can be recycled from spent PEM electrolyzer stacks? - How Recovery Yield Changes the Supply Picture
how much iridium can be recycled from spent PEM electrolyzer stacks? - How Recovery Yield Changes the Supply Picture

Recovered iridium can reduce virgin-metal requirements, but it cannot eliminate primary iridium demand during rapid PEM electrolyzer scale-up. The 2026 material-flow analysis estimates that, under its central practical case, recovered iridium supplies 16.9% of global and 3.8% of U.S. PEM electrolyzer iridium demand in 2050 [S1].

That result is a system outcome, not a direct stack recovery rate. It combines annual PEM manufacturing capacity, new and replacement systems, catalyst loading, distributed stack lifetimes, collection performance, recycling delay, technical recovery efficiency, loss accounting, remaining primary requirements, and potential surplus [S1].

Collection is a practical bottleneck: a stack that is dismantled or sent to a refiner without recovering its catalyst-coated membrane has much less chance of returning its iridium to the supply chain. The study estimates secondary iridium and platinum supply using collection efficiency and technical recovery efficiency, among other factors [S1].

Comparison of Recycling Routes for Spent Stacks

Dismantling and mechanical processing are useful for separating the CCM and reducing mixed-metal handling. The PEMWE recycling-chain work emphasizes non-destructive disassembly, dry mechanical decoating of catalyst-coated membranes, membrane dissolution, and separation of anode and cathode particles before hydrometallurgical processing [S5].

The conceptual recycling chain for PEM water electrolyzers includes dismantling, mechanical processing, hydrometallurgical processes, and carbon reuse [S5]. The conceptual chain favors mechanical separation before hydrometallurgy because it reduces the amount of material entering energy-intensive chemical treatment and can separate anode and cathode fractions [S5].

Heraeus recycles and refines platinum, iridium, ruthenium, and palladium, as well as ionomers from catalyst-coated membranes [S3].

Closed-Loop Iridium and Ionomer Recovery

how much iridium can be recycled from spent PEM electrolyzer stacks? - Closed-Loop Iridium and Ionomer Recovery
how much iridium can be recycled from spent PEM electrolyzer stacks? - Closed-Loop Iridium and Ionomer Recovery

A complete recycling project must account for more than iridium. ERRIN’s Horizon Europe call, reference HORIZON-JU-CLEANH2-2025-05-01, targets simultaneous iridium and ionomer recovery after CCM separation from end-of-life stacks or production scrap [S4].

Iridium must still be recovered to make replacement CCMs when electrolyzers reach the end of their service life, while recovered ionomer can potentially return to the membrane-material loop [S3].

This creates a better procurement target than iridium alone. A project should require an assay of recovered metal, identify the catalyst fraction, document collection and process losses, and specify a route for the membrane ionomer. If only the iridium is counted, the stack may be recycled at a lower overall material value than a process designed for both streams.

What Spent-Stack Owners Should Contractually Require

Require a stack-by-stack mass balance rather than a generic “iridium recovery” claim. The contract should identify the installed capacity, stack model, CCM status, estimated iridium inventory, sampling method, recovery yield, refining route, assay basis, treatment of residues, and final allocation of saleable metal [S1][S3].

Do not confuse recovery with market availability. The iridium recycling market was estimated at USD 570.0 million in 2024 and projected at USD 880.0 million by 2030, with a 7.5% compound annual growth rate [S2]. Less than 25% of iridium demand was met through secondary sources in 2024 [S2]. These market figures show why recycling capacity is expanding, but they do not guarantee that every retired stack will be collected promptly.

For owners, the strongest commercial model is a return-and-refining agreement tied to measurable recovery of iridium, with optional credit for platinum and other materials. Heraeus states that recovered metal can be credited to a precious-metal account, used for new electrocatalyst or coating production, sold, or physically supplied to a customer destination [S3].

Limits on Reusing Recovered Iridium

how much iridium can be recycled from spent PEM electrolyzer stacks? - Limits on Reusing Recovered Iridium
how much iridium can be recycled from spent PEM electrolyzer stacks? - Limits on Reusing Recovered Iridium

Recycling reduces primary-metal requirements, but it does not restore all of the original catalyst performance automatically. The recycled product must meet the purity and performance requirements for new CCM manufacture, and the recovered ionomer must meet the stated electrochemical-application threshold of above 99.5% [S4].

Environmental benefit is also material-specific. Heraeus cites industry-average emission factors for secondary platinum-group metals that are 98.2% to 98.8% lower than those of primary platinum-group metals, based on an International Platinum Group Metals Association life-cycle assessment published in 2025 with reference year 2022 [S3].

The main failure modes are poor catalyst separation, uncontrolled dilution of iridium-bearing fractions, delays between stack retirement and processing, losses during sampling or dissolution, and failure to separate anode and cathode particles. These risks reduce both recovered mass and the usable fraction returned to new electrolyzer production [S1][S5].

The trackable procurement indicators are therefore simple: mass of CCM collected, grams of iridium assayed in the incoming fraction, measured recovery yield, saleable metal returned, and recycled ionomer purity against the greater-than-99.5% threshold. A spent stack with 300–500 g of nominal iridium per MW has meaningful recovery value, but collection and process yield determine how much becomes usable secondary supply.

Frequently asked questions

What iridium mass should be used for screening a 1 MW PEM electrolyzer stack?

Use an estimated stack-level loading of 0.3–0.5 g of iridium per kilowatt, equivalent to approximately 300–500 g for a 1 MW stack. Treat this as a planning estimate because actual iridium content depends on rated power, catalyst-coated membrane area, catalyst loading, and the included stack hardware.

How much iridium could technically be recovered from a spent PEM electrolyzer stack?

Recoverable iridium can approach the quantity originally present if the iridium-bearing catalyst layer is separated and processed through a technically effective recovery route. No universal plant-scale recovery percentage is established, and the saleable amount will be lower if collection, recovery, losses, or refining requirements are not accounted for.

Which spent-stack components should be targeted to maximize iridium recovery?

Retired PEM electrolyzer stacks may contain valuable iridium in their catalyst layers [S8].

Which recycling route is preferred for recovering iridium from catalyst-coated membranes?

The conceptual recycling chain favors mechanical separation before hydrometallurgy. Non-destructive disassembly, dry mechanical decoating, membrane dissolution, and separation of anode and cathode particles can reduce material entering energy-intensive chemical processing and preserve separation of iridium- and platinum-bearing fractions.

9 sources
  1. Recycling Iridium and Platinum from End-of-Life ...
  2. Iridium Recycling Market Report, Industry and ...
  3. Recycling Solutions for the Hydrogen Economy
  4. Simultaneous ionomer and iridium recycling
  5. Conceptual Recycling Chain for Proton Exchange ... (May 2, 2025)
  6. Closing the Loop for Iridium Recycling from Water ... (by D Brown · 2026)
  7. PEM Electrolyzer Iridium Catalyst Market
  8. Hydrogen Plants: Your Retired PEM Electrolyzer Stacks ... (5 days ago)
  9. Simultaneous ionomer and iridium recycling

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →