NdPr oxide was assessed at $103.76/kg on 10 March 2026, while the September benchmark reached RMB729,500/t, or $108,696/t [S5][S7].
The 2026 price structure separates magnet-grade NdPr from heavy rare earths Dy and Tb, while Sm and Y occupy a lower-priced segment of the oxide market [S3][S4][S5].
2026 rare earth oxide benchmark prices
On 10 March 2026, the China domestic benchmark was $103.76/kg for NdPr oxide, $113.05/kg for neodymium oxide and $113.69/kg for praseodymium oxide [S5]. The same table placed dysprosium oxide at $189.58/kg and terbium oxide at $803.81/kg, versus $653/t for lanthanum oxide and $1,761/t for cerium oxide [S5].
By September, the Benchmark Minerals review recorded an average NdPr oxide assessment of RMB729,500/t, equivalent to $108,696/t, after a 1% increase from the prior level [S7]. The Shanghai Metals Market snapshot dated 24 September 2026 showed NdPr oxide at RMB738,000/t [S6]. These two September observations use different assessment bases, so they should not be treated as a single continuous series.
Historical and forward reference points
USGS recorded 2025 average prices of $69/kg for 99% minimum NdPr oxide, $74/kg for 99.99% minimum praseodymium oxide, $73/kg for 99.5% minimum neodymium oxide and $2.82/kg for 99.5% minimum samarium oxide [S1]. The US NdPr oxide annual average price was US$69/kg in 2025, US$55/kg in 2024 and US$124/kg in 2022 [S8].
The March 2026 China domestic price of $103.76/kg was about double the approximately $49/kg December 2024 level and 7% below the $111.50/kg multi-year high reached on 25 February 2026 [S5].
A defensible October or November 2026 value for every oxide in the requested basket cannot be stated from the supplied evidence. The table should therefore separate dated market assessments from annual averages and historical reference points, rather than present all values as a single synchronized 20 November 2026 quotation.
NdPr versus Dy, Tb, Sm and Y

The March 2026 comparison was decisive: terbium oxide at $803.81/kg was about 7.7 times the $103.76/kg NdPr benchmark, while dysprosium oxide at $189.58/kg was about 1.8 times higher [S5]. Samarium oxide averaged $2.82/kg across 2025, approximately 4.1% of the 2025 NdPr annual average of $69/kg [S1].
NdPr and DyTb should not be treated as interchangeable price lines. NdPr is the principal rare earth input in NdFeB magnets, while Dy and Tb serve different heavy rare earth supply chains that S&P Global identified as related but distinct [S3]. The DyTb versus NdPr volatility comparison provides additional context on how the premium and swing range widened.
Geographic basis and specification requirements
NdPr oxide prices on China's domestic market stood at $103.76/kg on 10 March 2026, according to Shanghai Metals Market (SMM) [S5]. The difference between domestic and FOB figures shows why geography must be stated in any procurement table.
This spread reflects the assessed delivery condition and supply location, but it should not be applied mechanically to every oxide or contract because transaction terms, inventory and trade conditions differ [S3].
Each quotation also needs an assay, chemical specification, unit, delivery basis and effective date. Historical comparisons show that neodymium oxide at 99.5% minimum averaged $55.27–$56.27/kg FOB in May 2024, while yttrium oxide at 99.999% averaged $6.10–$6.50/kg FOB over the same period [S4]. These figures are dated historical references, not quotations for 20 November 2026.
Where the 2026 price pressure comes from

The largest cost driver is the feedstock value of each separated oxide, but geographic availability and security of supply can add a substantial premium.
Processing adds separation, conversion, assay, packaging and freight costs. Volume tier also affects the delivered price because large contracts can secure feedstock and production scheduling, while small lots carry additional handling and minimum-lot costs. Lead time becomes more valuable where supply is constrained, particularly for separated heavy rare earths [S3].
For buyers, the relevant cost is not the oxide label alone. Total ownership cost includes the purchase price, incoming assay testing, storage and handling, conversion yield, production loss, inventory financing and the effect of supply interruptions on magnet output. The NdPr oxide price trend through November 2026 is useful for following the benchmark movement behind procurement decisions.
Procurement approach for five oxide categories
NdPr suits buyers exposed to NdFeB magnet consumption, Dy and Tb require a separate heavy rare earth qualification and supply plan, and Sm and Y need application-specific comparisons because their volumes and prices differ materially [S3][S4]. Sm is associated with Sm-Co magnets, while Y is used in ceramics and other applications; Argus priced 99.999% yttrium oxide at $6.10–$6.50/kg FOB in May 2024 [S4].
The United States produced an estimated 51,000 t of rare earth oxides in mineral concentrates in 2025, valued at $240 million, while apparent consumption of compounds and metals reached 27,000 t [S1]. Imports of rare earth compounds and metals increased 169% in 2025, but their estimated value fell from $168 million in 2024 to $165 million as the mix shifted toward lower-value products [S1].
For a five-line purchasing schedule, record each oxide as 99% minimum NdPr, 99.5% minimum Sm, 99.999% Y where that grade is required, and the contracted assay for Dy and Tb, alongside the delivery term. USGS reported $2.82/kg for 99.5% minimum samarium oxide and $69/kg for 99% minimum NdPr oxide in 2025, while the 2026 market evidence supplies dated March and September benchmarks for NdPr, Dy and Tb [S1][S5][S7].
Track the next SMM NdPr assessment, the next Benchmark Minerals monthly review and any revision to the US annual price series. Those three signals provide a practical way to update the table without mixing annual averages, historical FOB ranges and 2026 spot assessments.