REQUEST FOR QUOTE → Request a quote
SpecForge Editorial Team

Samarium Oxide and SmCo Magnet Costs in 2026

Table of Contents
  1. Samarium Oxide Price: Purity, Basis and Trend
  2. SmCo Magnet Market Quotes and Regional Basis
  3. Why SmCo Magnets Cost More Than the Oxide
  4. Cost Drivers Behind 2026 Magnet Pricing
  5. SmCo Versus NdFeB for Specifiers
  6. Compliance, Qualification and Total Cost
  7. Monitoring the Price Signal
Samarium Oxide and SmCo Magnet Costs in 2026

Samarium oxide reached US$2.80/kg in China on September 21, 2026, while SmCo magnets were quoted from US$41,212.56 to US$41,404.28 per tonne in October 2026 [S2][S3].

The two prices describe different stages of the supply chain: oxide is a refined rare-earth feedstock, whereas a finished SmCo magnet combines samarium with cobalt, processing, qualification and regional delivery costs [S2][S7].

Samarium Oxide Price: Purity, Basis and Trend

Samarium oxide, Sm₂O₃, was quoted at about US$2.80/kg for 99.9% material on an EXW or FOB China basis on September 21, 2026, equivalent to US$2,800/t [S2]. The 2025 USGS average for 99.5% oxide was US$2.82/kg, compared with US$2.01/kg in 2024, a 40% annual increase [S2].

Monthly 99.9% oxide readings remained within US$2.22–2.28/kg from late March to mid-June 2026, advanced to US$2.31/kg in July and US$2.44/kg in August, and then rose 14.75% in one month to US$2.80/kg in September [S2]. The September reading was 26% above the late-March level [S2].

Buyers must preserve the quote conditions. The September value applies to 99.9% material, while the USGS annual series covers 99.5% oxide, and EXW, FOB and CIF values are not interchangeable [S2].

SmCo Magnet Market Quotes and Regional Basis

October 2026 SmCo magnet prices were US$41,212.56/t FOB China, US$41,338.26/t CIF India, US$41,404.28/t CIF USA, US$41,287.07/t CIF Germany and US$41,309.17/t CIF Australia [S3]. The full October cross-regional spread was US$191.72/t, or about 0.47% of the China FOB quote [S3].

China’s FOB price eased from US$41,643.97/t in September 2026 to US$41,212.56/t in October, a decline of US$431.41/t [S3]. The corresponding US CIF quote fell by US$410.87/t, from US$41,815.15/t to US$41,404.28/t [S3].

These are nominal magnet-market quotations, not universal transaction prices. Incoterm, grade, magnet geometry, coercivity, temperature rating, plating, certification and volume can move an actual order materially above or below a regional benchmark [S3].

Why SmCo Magnets Cost More Than the Oxide

samarium oxide price 2026 and SmCo magnet costs - Why SmCo Magnets Cost More Than the Oxide
samarium oxide price 2026 and SmCo magnet costs - Why SmCo Magnets Cost More Than the Oxide

The finished magnet price therefore cannot be explained by samarium oxide cost alone. Cobalt, samarium metal or alloy conversion, powder production, pressing, alignment, sintering, machining, plating, quality testing, export licensing and freight all add cost [S3][S4]. North American SmCo production also carries substantially higher costs than competing NdFeB production, particularly because SmCo requires different raw materials and processing [S7].

The comparison is direct: oxide was approximately US$2,800/t, while the finished SmCo benchmark was about US$41,000/t in October 2026 [S2][S3]. That 14.7-fold relationship is an analytical ratio between different products, not a manufacturing conversion ratio.

Cost Drivers Behind 2026 Magnet Pricing

Chinese export licensing was a major delivery-cost driver in 2026. In April 2025, China’s Ministry of Commerce introduced export license requirements for samarium, dysprosium, terbium, and related alloys, with reviews for rare-earth magnet applications later reported as slowed and sometimes delayed or denied [S4].

Chinese FOB SmCo quotations were US$41,643.97/t in September 2026 and US$41,212.56/t in October 2026 [S3].

Licensing compliance also affects inventory and lead time.

SmCo Versus NdFeB for Specifiers

samarium oxide price 2026 and SmCo magnet costs - SmCo Versus NdFeB for Specifiers
samarium oxide price 2026 and SmCo magnet costs - SmCo Versus NdFeB for Specifiers

SmCo and NdFeB magnets should be compared by operating requirement, temperature capability, cobalt exposure and procurement risk rather than by oxide price alone.

SmCo costs substantially more to produce than NdFeB, while NdFeB benefits from larger production scale and stronger demand-linked investment in neodymium and praseodymium [S7][S2].

For high-temperature or mission-critical duties, the relevant comparison is delivered magnet performance and qualified supply, not the per-kilogram feedstock spread. For volume applications where temperature requirements permit, NdFeB can provide a lower-cost route, but samarium oxide pricing remains a secondary cost factor in both cases [S2][S7].

Compliance, Qualification and Total Cost

In April 2025, China’s Ministry of Commerce introduced export license requirements for samarium, dysprosium, terbium, and related alloys, with later reports describing long reviews and increased scrutiny of end-use declarations [S4]. A magnet assembled outside China can still face contractual and traceability constraints when upstream feedstock originated in China [S4].

Defence procurement adds another sourcing layer. Buyers should verify the exact contract clause and chain of custody for the specific grade rather than assume finished assembly establishes compliance [S4].

Total cost of ownership extends beyond purchase price. Installation and machining losses, tooling, inspection, coating life, energy losses from a lower-efficiency magnet, expedited freight, safety stock and requalification after supply changes can outweigh the quoted material spread [S3][S4]. SmCo’s higher coercivity and temperature performance can reduce thermal derating or cooling requirements in demanding motors, while lower cobalt prices can improve the finished-magnet margin without lowering the customer’s delivered price immediately [S3].

Monitoring the Price Signal

samarium oxide price 2026 and SmCo magnet costs - Monitoring the Price Signal
samarium oxide price 2026 and SmCo magnet costs - Monitoring the Price Signal

Three indicators provide a practical way to track SmCo cost exposure: the monthly 99.9% oxide reading, cobalt-price direction, and the lead time associated with Chinese export approvals [S2][S3][S4]. A fall from the September oxide peak to US$2.80/kg would matter less than a sustained reduction in licensing delays or a material shift in magnet quotations [S2][S3].

For a 2026 budget, use the October 2026 SmCo benchmarks of US$41,212.56/t FOB China and US$41,404.28/t CIF USA as separate benchmarks, then add qualification, coating, tooling, freight and inventory costs to the applicable line item [S3].

Frequently asked questions

What was the September 2026 price of 99.9% samarium oxide, and what quote basis applied?

The quoted price was US$2.80/kg, equivalent to US$2,800/t, for 99.9% samarium oxide on September 21, 2026. It applied on an EXW or FOB China basis, which should be preserved when comparing it with other quotations.

What were the October 2026 FOB China and CIF USA prices for SmCo magnets?

SmCo magnets were quoted at US$41,212.56/t FOB China and US$41,404.28/t CIF USA in October 2026. The difference between these two regional benchmarks was US$191.72/t, or about 0.47% of the China FOB quote.

How much samarium oxide cost is represented in one kilogram of SmCo magnet?

At a samarium oxide price of US$2.80/kg, a SmCo magnet containing 25–35% samarium by weight represents about US$9 per kilogram of oxide-related material. This calculation uses 0.25–0.35 multiplied by US$2.80/kg and does not include cobalt, conversion, processing, qualification, plating, or delivery.

Which procurement risks should buyers consider when sourcing SmCo magnets from China?

Chinese export licensing can materially affect delivery time and inventory; approval reviews were documented at 45–60 days, with end-user documentation required for individual order lines.

9 sources
  1. Samarium Price Today: Metal Benchmark & Market Outlook (Jun 4, 2026)
  2. Samarium Oxide Price per kg: Chart and Drivers
  3. Samarium Cobalt (SmCo) Magnets Price Trend October 2026
  4. SmCo Magnet Supply & Cost Outlook – 2026 Update (Nov 3, 2025)
  5. Samarium Price Trend 2026, Forecast, Chart, News & Index (Oct 7, 2026)
  6. SEG Market Report
  7. North America Samarium Cobalt Magnets Market 2026-2034 (Feb 18, 2026)
  8. Samarium Cobalt Magnet Market - Strategic Insights and Forecasts ...
  9. Samarium Oxide Price Trends, Forecast, History, Chart And Index

Need to source matching manufacturers or get a quote?

SpecForge connects industrial buyers with verified manufacturers. Submit your requirement and we will route it to matched suppliers.

Submit RFQ now →
Ask SpecForge AI