Individual ball spacers provide local separation and movement freedom, while a segmented cage mechanically couples the rolling-element set for tighter circumferential position control [S1][S4].
The decision depends on load, speed, deformation, lubrication, temperature and duty cycle, not on the cage label or polymer-versus-metal construction alone [S1].
How Ball Spacers and Segmented Cages Control the Ball Set
An individual spacer sits between two adjacent balls and primarily enforces local minimum separation. In simplified form, the arrangement is ball, spacer, ball, spacer, ball; there is no continuous bridge transferring displacement around the full circumference [S1].
A segmented cage consists of connected cage sections that guide and position the rolling elements as a system. Compared with separate spacers, it offers stronger circumferential position control and a smaller residual gap [S1][S4].
Both arrangements prevent adjacent balls from rubbing during rotation. That contact would generate heat, wear and debris in the raceway, impairing smooth operation and reducing bearing life [S4]. Material is a separate choice: typical separators can be plastic, plastic-coated steel or bronze, selected to reduce friction against steel rolling elements [S4].
Criterion-by-Criterion Selection Comparison
For position control, individual spacers provide mainly local constraint, a continuous cage provides stronger system-level positioning, and a segmented cage occupies an intermediate position [S1]. Cages keep balls or rollers in precisely defined positions relative to each other within the raceway, while spacers maintain the minimum distance to the next rolling element.
For cost, cages are generally more expensive than spacers, so a cage should not be specified unless the duty requires its added control [S4]. For heavy or intermittent slewing, individual spacers remain practical where local freedom can accommodate structural deformation and uneven loading [S1].
Continuous rotation often favors a cage, which keeps the rolling elements in precisely defined positions relative to each other within the raceway. For heavily deformed, oscillating or dynamically loaded large bearings, the segmented cage must be evaluated as a loaded structural component, including pocket contact, guidance loads and wear [S1].
Application Fit and Residual-Gap Risk

Individual spacers fit low-speed, intermittent slewing applications in which the ball set can shift locally without disrupting operation. They are also less costly than cage systems, but the resulting residual gap may concentrate load at one location [S1][S4].
Segmented cages fit continuous rotation, higher circumferential speed and duties requiring controlled rolling-element position, but they are not automatically the low-friction solution. Cage-to-ball friction, lubrication condition and structural loads can offset any benefit [S1]. RPM alone is therefore an incomplete selection criterion [S1].
Material and Construction Checks
Published slewing-ring material options illustrate why polymer versus metal is not the primary architecture decision. Integral or segmented cages can be made of 20-gauge steel or ZL102 cast aluminium alloy, while spacer block cages can be made of polyamide 1010 resin, ZL102 cast aluminium alloy, QA110-3-1.5 aluminium bronze or nylon GRPA66.25.
A separate product specification lists integral and segmented cages in 20-gauge steel or ZL102 cast aluminium alloy, isolated-block cages in polyamide 1010 resin, ZL102 or QA110-3-1.5 aluminium bronze, and GRPA66.25 nylon for segmented-cage designs [S5].
For the rolling elements, GCr15 or GCr15SiMn carbon-chromium bearing steel is a documented option. Ring steel options include 50Mn and 42CrMo, while seals include NBR, silicone and fluororubber for different temperature duties [S3][S5]. The separator material still requires checking against load contact, temperature, contamination, lubrication and dimensional tolerances for the specific bearing geometry [S1].
Lubrication, Temperature and Wear Constraints

Lubrication must be selected from load, temperature, vibration and environmental conditions.
A cage is not a substitute for lubrication. In a spacer arrangement, free movement can increase sliding at the spacer-to-ball interfaces; in a cage arrangement, the cage becomes a sliding guide that requires sufficient lubricant film and clearance [S1].
For any slewing ring bearing, record the grease quantity, relubrication interval and sealing condition as part of the separator decision. Undersized seals admit dust and moisture, while insufficient grease raises contact temperature and accelerates wear [S4][S5].
Failure Modes During Selection and Operation
Spacer-specific risks include residual-gap accumulation, unequal sharing between neighboring balls, increased local loads and possible spacer-to-ball wear [S4]. Individual spacers also depend on the local stack remaining controlled under ring deformation and oscillation [S1].
Cage-specific risks include pocket interference, cage fracture or distortion, guide wear and friction heating. A segmented construction can bridge local gaps, but its joints and ends remain structural discontinuities that require inspection [S1][S3].
Crossed-roller slewing bearings require separate treatment because roller skew and guidance add constraints beyond the simple ball-spacer relationship [S1]. For a roller slewing bearing, do not transfer a four-point-contact ball selection matrix without checking roller guidance, contact geometry and the specified cage architecture [S1][S2].
Engineering Selection and Supplier Verification

Specify the intended separation architecture explicitly: individual spacer, integral cage or segmented cage. Request the separator material, adjacent-ball spacing, circumferential residual gap, cage pocket clearance, guide geometry and fastening arrangement rather than accepting a generic cage or spacer note [S1][S3].
Use the operating load, rotation direction, oscillation range, peak speed, continuous or intermittent duty, ring deformation, ambient temperature and lubrication method as the comparison inputs [S1][S7]. Confirm that the arrangement remains compatible with the ring construction and rolling-element type specified for the slewing drive.
A practical default is individual spacers for slow, intermittent slewing where residual-gap effects are tolerable and cost matters. Select a segmented cage where continuous rotation, higher speed, tighter position control or reduced residual gap is required. Require validation before release of a heavily loaded or dynamically loaded large bearing, including torque measurement, pocket-contact inspection and a lubrication plan [S1].
The next verifiable checkpoint is a supplier package listing separator architecture, material, residual-gap tolerance, installed clearance and lubrication limits, followed by a no-load rotation and torque comparison against the specified operating profile [S1].