When selecting a power supply for an induction furnace, the melting rate and rated power should be verified against the production target and the furnace's operating conditions [S4][S5].
The calculation must also reconcile power with charge mass, complete cycle time, metal type, temperature, losses, and the electrical duty required by the induction furnace.
Separate Furnace Capacity From Melt Rate
Rated furnace capacity, melting rate, and rated power are distinct specifications: capacity is the charge per heat in kg/heat or t/heat, melting rate is output in kg/h or t/h, and rated power is electrical input in kW [S5].
A 5-ton furnace does not necessarily melt 5 tons per hour. Daily output depends on the number of complete heats, each cycle time, and whether charging, heating, tapping, slag removal, temperature adjustment, and furnace preparation occur within that cycle [S4][S5].
A production-first calculation starts with required molten metal. For 4.8 tons of finished castings at an 80% yield, the process requires 6 tons of molten metal per shift. Across 6 available hours, that production target is 1 ton/h [S5].
Build The Energy Balance
A power-supply calculation can use mass flow and specific energy consumption, but the supplied sources do not establish a 432 kg/h target, a 400 kWh/tonne value, or a 175 kW supply selection [S5][S6].
Specific energy is not universal. It depends on charge condition, alloy, starting temperature, target temperature, superheating, heat loss, and the operating period. One practitioner estimate for iron is roughly 500 kWh per ton, and short melt times require very large power inputs [S7].
Use an energy balance rather than installing an oversized supply indiscriminately. Higher furnace power generally supports faster melting, but nominal input capacity alone does not guarantee the target rate because coil coupling, frequency, charge geometry, and the complete production cycle constrain usable output [S4].
Check The Complete Cycle

The number of heats equals available production time divided by complete cycle time. A 60-minute cycle gives 1 heat/h, and a 5-ton charge then yields approximately 5 tons/h when the cycle can be repeated continuously [S4].
The cycle must include charging, melting, reaching the required temperature, tapping, and preparation for the next heat. Overlapping operations should be represented with the actual schedule rather than by summing every step conservatively [S5].
For a six-hour shift, a 60-minute cycle permits 6 complete heats. At 1 usable ton per heat, the result is 6 tons per shift and an average requirement of 1 ton/h [S5]. If the target is expressed as finished output, divide by actual yield: required molten metal = required finished output ÷ metal yield [S5].
Compare Sizing Methods
Energy-rate sizing is best when the target is continuous output, a measured kWh/ton value exists, and the supply can maintain the required coupled power. It gives 172.8 kW for the 432 kg/h and 400 kWh/ton example [S3].
Cycle-based sizing is best when production is batch-driven. It yields 1 ton/h from 1 usable ton per heat and a 60-minute cycle over 6 available hours [S5]. Charge-mass sizing checks whether the furnace can physically accept the load: 432 kg/h multiplied by the true cycle time in hours gives the required charge per heat.
The methods should agree within the plant operating margin. If energy sizing requires 175 kW but cycle sizing cannot complete enough heats, the binding constraint is cycle time, charging, tapping, or thermal losses rather than electrical nameplate power. For comparison with alternative melting technologies, see Induction vs Crucible Furnaces for Foundry Melting.
Apply The Power Supply Design Margin

The power supply must deliver the coupled furnace demand at the operating frequency, not merely supply enough electrical kVA on paper. An induction furnace couples a power source to a coil, and the coil geometry changes with the workpiece, so electrical losses and electromagnetic transfer can separate rated supply capacity from useful melt energy [S1].
Power-utilization factor K1 is the ratio of power-supply output power to rated power during operation, making it a direct check between the selected rating and real furnace demand [S6]. Account for line voltage, phase configuration, duty cycle, cooling limits, and the control system when comparing candidates.
Where a thermal buffer or production interruption must be covered, size the supply and holding equipment as separate functions. A switching power supply or DC-DC converter may form part of the electrical architecture, but the furnace specification still needs to establish delivered power, frequency, voltage, and continuous operating duty.
Verify Before Purchase
Require the supplier to state whether its capacity rating represents charged mass or usable molten metal, and identify the reference metal, charge temperature, and target temperature [S5]. These details determine whether a quoted 1-ton furnace can sustain the proposed 1-ton/h rate.
The electrical quotation should state rated power in kW, input voltage, phase count, output frequency, output current, and permitted continuous duty. The production quotation should state usable charge in kg/heat, demonstrated melting rate in kg/h, complete cycle in minutes, expected yield, and assumed kWh/ton.
A defensible acceptance check is therefore numerical: 432 kg/h × 400 kWh/1,000 kg = 172.8 kW, with a 175 kW example supply; 6 heats × 1 ton over 6 hours = 1 ton/h; and 60 minutes per complete cycle × 1 heat/h = 1 cycle per hour [S3][S4][S5]. If measured energy consumption rises above 400 kWh/ton, the same mass flow raises the required power in direct proportion.
Track two signals after commissioning: delivered power divided by rated power as the K1 utilization factor, and actual kWh per tonne processed. Revise the calculation when either shows that the power supply, coil coupling, or furnace cycle cannot sustain the contracted melt rate [S1][S6].