A gyratory crusher is the primary compressive crushing machine for the highest tonnage mines: a tall steel shell whose top carries a spider, a bridge with a central bearing, from which the main shaft hangs, and an eccentric near the bottom that gyrates the shaft so the mantle, the conical breaking head, sweeps the inside of the concave lining without ever rotating on its own axis. Run of mine rock dumped into the top is nipped, crushed, and falls through the narrowing gap on every gyration, and the product leaves the bottom onto conveyors at a size the secondary stage, usually a cone crusher, is built to take. Metso's Superior MKIII series is a representative industrial catalog, and this page treats the complete machine, spider, shaft, shells, liners, drive, and hydraulic system, as the purchasing object.
This page is written for the engineer specifying a primary gyratory crusher for a mine, a major quarry, or an in-pit or underground crushing station. It works through what the machine does and what is being bought, how the gyration and the liner geometry make the size reduction, which crusher designs fit which installations, the parameters that appear on vendor data sheets, and the selection factors and RFQ language that decide whether the crusher meets its throughput for a liner and mainshaft budget that stays predictable.
The decision concentrates in five places: the run of mine feed size distribution and the product size the downstream stage demands, the tonnage the machine must pass at availability the mine plans around, the machine size and power whose capacity curve covers that duty, the liner profile family and the closed side setting the product is made at, and the installation, surface dump station, in-pit, or underground, that fixes the machine's layout and access. Get those right and the drive, the hydraulics, and the maintenance plan follow with little freedom.
Chapter 1 / 06
What a Gyratory Crusher Is and What Is Being Decided
The machine this page describes is built around a vertical mainshaft suspended from a spider bridge at the top of a two or three part shell. An eccentric bushing in the bottom shell gives the shaft its gyration, a few degrees off vertical, sweeping the mantle against the concaves that line the top shell's internal cone; the drive is an electric motor through gears or belts onto the eccentric, and the machine runs continuously, fed by trucks dumping into a stationary or movable feed hopper above, or by an apron feeder from a surge bin in underground and in-pit duty. Nothing in the crushing zone rotates, everything gyrates, and that single distinction explains the machine's capacity, its constant crush in every revolution, and the height that dominates its building.
What is being decided when a gyratory crusher is purchased is a throughput and product size guarantee backed by a power and liner statement. The buyer is purchasing a stated tonnes per hour from a stated run of mine feed size to a stated product size, typically expressed as a percent passing curve at a stated closed side setting, at a power draw the drive and the mine's electrical system can carry, with liner wear rates in tonnes crushed per set that hold the operating budget. Everything on the vendor data sheet, mantle diameter, feed opening, eccentric throw, installed power, exists to support those guarantees, and the honest vendor sizes from crushing testwork on the actual ore, its strength and abrasiveness, rather than from an analogy to someone else's rock.
The gyratory crusher sits at the head of the comminution family with defined neighbors. It is not a jaw crusher, the compressive machine whose swinging jaw breaks rock in a V, a rugged and cheaper primary that this encyclopedia's own page describes, and the two compete directly for the primary duty: below a few thousand tonnes per day the jaw usually wins on capital and layout, above it the gyratory wins on capacity per installed kilowatt and on its ability to take direct truck dumps. It is not a cone crusher, the secondary and tertiary machine that shares the gyratory's geometry in miniature and whose own page notes that it is not a gyratory; the cone takes the gyratory's product and makes the mill feed. The ball mill downstream grinds what the crushers have reduced.
Different buyers buy the same machine for different materials. A porphyry copper mine buys the largest primary gyratories, taking direct dumps from a mining dump truck of two hundred tonnes and more, feeding SAG and ball mill circuits through conveyors and stockpiles. An iron ore operation buys heavy duty machines for hard abrasive ore, the product continuing to a magnetic separator and flotation cell circuit after milling. A cement plant buys a gyratory or a large jaw for limestone, feeding the raw mill and the rotary kiln line. An underground mine buys a compact underground duty gyratory, fed from a grizzly and a surge bin below the haulage level, delivering onto a conveyor to surface. The specification language differs, but the nip and compressive physics is shared.
The economics deserve their own paragraph because the primary crusher is the mine's front door and its bottleneck when it is down. Capacity per unit of installed power is the gyratory's advantage, it crushes on every gyration of every revolution, and its availability, the percentage of scheduled hours it receives trucks, is the number the mine plan is built on; a primary down costs the fleet, and a primary that must wait for a liner change in single large pieces costs the fleet every change. Liner consumption is the operating cost that matters, tens of tonnes of manganese per set in the largest machines, and the shell and mainshaft are the capital items whose decades-long life the purchase is really about. A buyer who compares offers on machine price alone has ignored the liner column and the availability clause, which is where the money actually lives.
A short tour of named installations makes the machine concrete. At a copper concentrator, 240 tonne trucks dump into a stationary gyratory over a 1.5 meter feed opening, product at 175 millimeters CSS feeds apron and belt conveyors to a stockpile, and the secondary cone crusher section follows. At an in-pit station, a semi-mobile gyratory on a sled or gantry follows the bench down, cutting the haul distance a mining dump truck must climb. Underground, a compact duty gyratory under a grizzly and surge bin crushes to conveyor size for the haulage belt to surface. At a quarry, dumped rock meets the primary gyratory's concaves, and a belt scale or weigh feeder on the product conveyor closes the tonnage record. Each installation names the same knobs, feed, setting, throw, and liners, with sizes that scale while the nip physics barely changes.
Chapter 2 / 06
How the Gyration and the Liners Do the Work
The breakage is compression in a narrowing annulus. Each gyration brings the mantle toward a concave region, rock in the chamber is nipped where the closing gap and friction can grip it, and it fractures under compressive loads far below its intact strength because the loading geometry concentrates stress at contacts. The particle then falls or is squeezed downward as the gap opens on the far side of the sweep, and the sequence repeats down the chamber, each zone reducing size a modest ratio until the product passes the closed side setting at the bottom. Chamber design, the paired profiles of mantle and concaves, is the machine's engineering heart, because the profile sets how many crushing zones the chamber holds and how each passes rock to the next.
The closed side setting is the product dial. CSS, the narrowest gap between mantle and concave at the bottom of the chamber on the closing stroke, bounds the product size, coarser settings raise tonnage and reduce fines and liner stress per tonne, finer settings do the reverse, and the setting is measured and adjusted by the machine's hydraulic system, which raises or lowers the mainshaft to move the mantle vertically against its concaves. The open side setting, the widest gap, bounds the maximum feed the chamber will accept. Between them the throw, the radial travel the eccentric gives the shaft, sets the sweep and the volume the chamber can pass per gyration, and throw, speed, and profile together make the capacity curve the vendor publishes at each setting.
Liners are the consumable engine. Mantles and concaves are cast manganese steel, work hardening under impact so the surface toughens in service, in profiles matched to the duty, coarse for primary reduction, fine for the tightest product, and in the largest machines a concave set weighs tonnes and a mantle nearly as much. Liner wear widens the chamber and coarsens the product, and the operating discipline is to change liners at the wear limit, tracked in tonnes crushed or by chamber measurement, rather than at failure. Modern designs divide concave rings into segments for safer handling and add wear sensors or measured cavity wear maps to make the change predictable; shell rotation, rotating the top shell a planned fraction over the liner life, evens circumferential wear where feed distribution biases it.
The spider and mainshaft carry the machine. The spider bridge bears the vertical load through its hub and bushing, the shaft hangs from the spider with a nut and head, and the eccentric, in spider bushings and a main frame step or plain bearing, gives the gyration; hydraulic systems position the shaft and, in most modern machines, provide overload release, dropping the setting to pass an uncrushable and restoring it after. Mainshaft fractures were the historical catastrophe of the class, and modern shaft metallurgy, generous fillets, and conservative stresses have made them rare, but a shaft remains the machine's most consequential single component and its supply terms deserve explicit contract language.
Feed presentation decides whether the engineering is expressed. The chamber wants a distributed feed across its whole circumference, rock centered and spread, not a stream dumped onto one side, and feed arrangements, truck dumps through deadbed protected hoppers, grizzlies and rock breakers scalping oversize, and apron feeders metering from bins, exist to deliver it. Oversize, rock larger than the open side setting, must be broken at the face or on the grizzly by a hydraulic breaker, because the gyratory crushes what fits and merely absorbs what does not. Fines in the feed waste chamber capacity, and scalping screens ahead of the crusher, where the flowsheet allows, raise the machine's effective tonnage at the same setting.
Dust and debris are the environmental work. Primary gyratories generate dust at the dump and the discharge, and the station carries dust collection, a bag filter or equivalent capture at the dump pocket and under the crusher, with water sprays or dry collection by climate and permit; spillage conveyors and launder design carry the flush of crusher bowl drains. In cold climates the station is enclosed and heated; in wet climates the dump pocket must shed water without carrying it into the chamber. None of this is the crusher vendor's scope by default, which is exactly why the RFQ must name the interfaces, or the buyer owns a crusher that works and a station that does not.
Chapter 3 / 06
Crusher Types, Installations, and Machine Boundaries
Stationary primary gyratories are the baseline class: a fixed machine in a concrete station, fed by direct truck dump through a hopper, product onto conveyors to the secondary stage or a stockpile. The class spans feed openings from around half a meter to well over one and a half, installed power from hundreds to over a megawatt, and machines whose shells divide into top and bottom, or three, parts for maintenance access. Layout is vertical, the machine and its dump pocket stand tall, and the civil work is a large fraction of the station price.
Semi-mobile and fully mobile installations move the machine toward the rock. Semi-mobile gyratories sit on a movable steel sled or gantry, relocated by crawlers in pieces as the pit deepens, cutting the truck haul a mining dump truck must climb and with it the fleet's fuel and time; fully mobile machines, fed directly by a shovel or a surface miner, eliminate the trucks but bind the crusher to the face schedule. Both trade relocation flexibility for structure and feed system complexity, and both are engineered as a station, crusher, feeder or dump hopper, conveyors, and dust plant, rather than as a machine alone.
Underground duty gyratories are compact members of the same class, reduced height and layout for excavation economics, fed by grizzly, rock breaker, and an apron feeder from a surge bin under the ore pass, discharging onto the haulage conveyor. Shaft stations and ore pass configurations constrain every dimension, and the machine is specified as much by what fits the excavation as by tonnage. Segmented shells and liner handling designed for limited headroom, and mainshaft handling tools engineered for the station, are the underground buyer's specific scope questions, and the vendor's underground reference list is the honest answer to them.
Direct dump, gyratory versus jaw, is the primary decision this page's machine exists for. The gyratory takes truck dumps continuously with high capacity per kilowatt, needs taller civil work, and carries a higher machine capital; the jaw crusher is lower, cheaper at moderate tonnage, easier to maintain in confined plants, and its product and capacity curves stop where the large gyratories begin. Below roughly two to three thousand tonnes per day, and at smaller feed sizes, the jaw usually wins; above, and with direct dumping of large run of mine rock, the gyratory is the standard. The secondary and tertiary stages belong to the cone crusher, the vertical shaft and horizontal impact machines serving recycle and softer rock duties, all of them their own topics in this encyclopedia's pages.
Adjacent machines complete the station. The dump pocket and grizzly, the rock breaker that clears it, and the apron feeder that meters underground and semi-mobile machines are station equipment bought with the crusher's duty in mind. The product side carries the conveyors, a belt conveyor to the secondary or stockpile with a belt scale closing the tonnage, and the screens, a vibrating screen scalping or sizing ahead of the cone stage. Downstream of the crushing and grinding line the concentrator's hardware follows, cyclone separators on mill classification, the magnetic separator and flotation cell already named, and the tailings train, a gravity thickener then a filter press or a vacuum belt filter, with a screw press in some water recovery schemes, closing the plant's water. The gyratory's RFQ names its own machine; the station's RFQ names all of this.
Chapter 4 / 06
Key Specification Parameters
The vendor data sheet for a gyratory crusher centers on feed opening, setting range, capacity, and power, and each number carries a sizing consequence. The table below lists the parameters that recur across manufacturers' catalogs, with typical ranges for the primary class; values for a specific project come from testwork on the actual ore, and the ranges here are orientation, not a substitute for a crushing study.
Parameter
Typical catalog range
What it decides
Feed opening
700 to 1,600 mm
Maximum run of mine lump the chamber accepts
Mantle diameter
1.1 to 3.4 m by class
Capacity class; machine scale and civil height
CSS range
100 to 300 mm primary duty
Product size; tonnage at each setting
Eccentric throw
20 to 45 mm by machine
Sweep volume; capacity; nip character
Installed power
250 to 1,200 kW
Throughput ceiling; electrical supply class
Capacity
1,500 to 9,000 t/h by size and ore
Station sizing; fleet and conveyor match
Concave life
2 to 20 Mt per set by abrasion
Liner budget; change outage plan
Eccentric speed
250 to 450 rpm small, slower large
Crushes per minute; energy per tonne
Three of these numbers deserve the buyer's suspicion when they arrive without a basis. Capacity quoted at an open side setting or on a light, nonabrasive ore is the classic flattery, and the honest curve is quoted at the CSS the buyer will run with the buyer's ore work index. Concave life quoted in hours rather than tonnes hides the utilization assumption, and two vendors' hour figures at different tonnages are not comparable. Product curves quoted without the test basis, a crusher model run on what data, flatter the chamber design beyond recognition. An RFQ that attaches the ore's strength and abrasion test results separates engineered offers from assembled ones.
Materials and construction follow the ore. Mantles and concaves are manganese steel castings in grades and profiles matched to duty and abrasion, with martensitic alloys and composite options in the harshest service; shafts are forged alloy steel, spider and mainframe castings of generous section; bearings are bronze bushings or rolling element by class, with lubrication and cooling systems the machine's life support. Hydraulic adjustment and overload systems, liner handling tools, and shell rotation provisions are scope items the RFQ must price, because they decide whether the station can actually change liners in the outage window it has.
Chapter 5 / 06
Selection Decision Factors and RFQ Language
Selection starts with the ore and the mine plan, not the catalog. The run of mine size distribution, from the blast design and the fleet's bucket, the ore's compressive strength and abrasiveness, from testwork, and the product size the secondary stage or the mill expects, fix the machine class and setting. The tonnage and the availability the mine plans around fix the size within the class, with surge capacity, the dump pocket and any bin, covering the crusher's maintenance windows. The installation, stationary, semi-mobile, or underground, fixes the layout family, and the electrical supply fixes the drive options. A buyer who skips the mine plan buys a crusher that fits a different mine.
The trade against the jaw crusher belongs in the study, not in habit. At moderate tonnages a large jaw, or jaw plus apron feeder station, is cheaper to build and easier to maintain, and the gyratory's capacity and dump advantages must pay for its height and capital; at high tonnages the gyratory is standard without serious argument. Within the gyratory class, the buyer balances machine size and speed, a larger slower machine against a smaller faster one for the same tonnage, liner profiles, coarse versus fine, and the degree of automation, hydraulic setting control, and wear monitoring, that the operating team will actually use.
The table below organizes the decision into the factors that recur across projects, with the questions the buyer should be able to answer before the RFQ goes out. Each row is a place where an incomplete answer turns into an underspecified machine and a bottleneck argument later.
Decision factor
What the buyer must state
Consequence if left open
Ore characterization
ROM size distribution, strength, abrasiveness, test data
Capacity and liner life guessed; guarantee void
Tonnage and availability
Design and peak t/h, scheduled hours, surge strategy
Machine undersized or overcapital
Product requirement
Target product curve and CSS the stage must run
Chamber profile mismatched to duty
Installation class
Stationary, semi-mobile, or underground; layout limits
Civil and handling scope wrong
Feed method
Direct truck dump, grizzly and breaker, apron feeder
RFQ language for a gyratory crusher should name the ore and the basis of guarantee. A workable specification states: run of mine feed size distribution and ore test data, strength and abrasion; design and peak throughput at the stated CSS with the product curve required; installation class and layout constraints; feed arrangement, dump, grizzly, breaker, and feeder; installed power and electrical supply conditions; hydraulic adjustment and overload release scope; liner profiles and expected life in tonnes for the stated ore, with handling tools and shell rotation provisions; lubrication and cooling scope; dust control interfaces; and the acceptance basis, water or no-load run, followed by a performance window at design tonnage against the guaranteed capacity and product curve. Naming the station neighbors, the apron feeder and conveyors, the belt scale, the secondary cone crusher, and the dust collection bag filter, lets the vendors bid the interfaces as well as the machine.
Chapter 6 / 06
Installation, Standards, Failure Modes, and Maintenance
Installation is a heavy civil and heavy mechanical campaign. The station is excavated and poured around the machine's layout, the bottom shell, spider, and shaft are set in lifts measured in tens to hundreds of tonnes, the eccentric and drive follow, and the high pressure lubrication and hydraulic systems are flushed and commissioned before the mantle and concaves are finally set to the starting CSS. Feed pocket, grizzly, breaker, and dust plant complete the station. Dry commissioning proves drive, lubrication, hydraulics, and interlocks; first ore is introduced at reduced rate to work-harden liners and tune the setting, and the performance test, tonnage and product curve at design CSS, closes the guarantee. The vendor's field engineers typically stay through the performance window, and an RFQ should price that presence explicitly.
Standards for these machines are mechanical and structural. The machine and its fasteners follow the manufacturer's engineering and the jurisdiction's machinery practice, the station follows structural and concrete codes, guarding follows machinery safety rules for rotating and crushing hazards, and the electrical, drive, and control scope follows the plant's ordinary standards. There is no single international gyratory crusher standard that governs the machine end to end, so the RFQ must name the applicable codes and the vendor's own standards for shaft and shell manufacture, test certificates, and nondestructive examination of the mainshaft. Any edition reference in project documents should be checked against the current issue at purchase rather than copied from an old specification.
The recurring failure modes are liners, liners' neighbors, and the rare catastrophe. Liner wear is the designed consumable, tracked and changed on plan. Spider and eccentric bushing wear raise clearance and vibration gradually, and spectral trending catches them seasons ahead. Mainshaft and spider failures are the class's rare catastrophic events, guarded against by conservative design and by the monitoring of shaft load and lubrication; when they occur they are rebuild campaigns measured in months, which is why mainshaft supply terms and inspection access belong in the contract. Un-crushables, tramp iron and tooth fragments, are handled by the hydraulic release; repeated passage coarsens product and distresses the shaft, and a tramp metal magnet upstream, where the flowsheet allows, is cheap insurance for the machine.
Maintenance planning is outage driven around the liner set. The table below lists the actions with the typical cadence a mine will schedule, assembled from common vendor practice; actual intervals follow the ore's abrasion and the mine's utilization and should be set from the first sets' measured wear.
Long term care is a chamber and shaft campaign. Ore hardness drifts as the mine deepens, and the chamber profile and setting that met the product curve at year one may leave tonnage on the table at year ten; periodic capacity surveys and profile reviews keep the machine matched to the rock. Liner metallurgy upgrades pay in abrasive service, and shaft inspection programs, ultrasonic and magnetic particle at major outages, convert the catastrophic failure mode into a planned repair. The mine that treats its primary as the fleet's gatekeeper, measured, surveyed, and stocked with liners, is the mine whose mill never waits for its rock.
FAQ
When is a gyratory crusher chosen over a jaw crusher for primary duty?
The gyratory wins when tonnage is high and feed is large: it crushes on every gyration, so its capacity per installed kilowatt exceeds a jaw's, it accepts direct truck dumps of large run of mine rock, and it runs continuously through the dump cycle. Below roughly two to three thousand tonnes per day, a jaw crusher station is usually cheaper to build, easier to house, and simpler to maintain, and it wins. The two machines' capacity curves overlap in the middle, and the choice there is a capital and layout study rather than a rule.
What is the closed side setting on a gyratory crusher?
The closed side setting, CSS, is the narrowest gap between mantle and concave at the bottom of the chamber on the closing stroke, and it is the main control of product size: tighter settings make a finer product at lower tonnage and higher chamber loading, coarser settings do the opposite. Modern machines adjust CSS hydraulically by raising or lowering the mainshaft, sometimes while running, and the same hydraulic system releases the setting to pass uncrushable tramp and restores it after. CSS is quoted with the product curve it produces on the specified ore.
How long do gyratory crusher liners last?
Concaves and mantles are manganese steel castings that work-harden in service, and life is quoted in tonnes crushed per set because hours depend on utilization. In hard abrasive metal ore, a concave set might carry a few million tonnes; in softer, less abrasive rock, many times more. Wear widens the chamber and coarsens product, so sets are changed at a measured wear limit, not at failure, and shell rotation, turning the top shell periodically, evens circumferential wear where the feed biases one side.
What does the spider do in a gyratory crusher?
The spider is the bridge across the top of the crushing shell, and its central hub carries the mainshaft: the shaft hangs from the spider, and the eccentric near the bottom of the machine gyrates it, sweeping the mantle against the concaves. The spider takes the vertical crushing loads into the shell structure, and its bushing is one of the machine's principal wear clearances. The spider and shaft arrangement is what distinguishes the true gyratory from the cone crusher, which supports its head from below.
Can a gyratory crusher be installed underground?
Yes, underground duty gyratories are compact members of the same class, engineered for reduced height and limited access. They are fed from ore passes through grizzlies, rock breakers, and surge bins onto apron feeders, and they discharge directly onto the haulage conveyor. The purchase is dominated by excavation economics: segmented shells, liner handling tools designed for low headroom, and mainshaft handling provisions are specified with the station, because a machine that cannot be maintained in the excavation is a bottleneck, not a crusher.
How is gyratory crusher capacity specified?
Capacity is quoted as tonnes per hour at a stated closed side setting on a stated ore, with the product size curve attached, because tonnage, setting, and ore are inseparable. The vendor's curve derives from chamber modeling calibrated by testwork on the buyer's rock, strength and abrasion data, and it should be checked against the mine's peak truck dumping pattern and the station's surge capacity. Guarantees should state the measurement basis, belt scale tonnage over a defined window at design CSS.
What should a gyratory crusher RFQ include?
State the run of mine size distribution and ore test data, design and peak throughput with the required product curve at the stated CSS, the installation class and layout constraints, the feed arrangement from truck dump or feeder, installed power and electrical supply, hydraulic adjustment and release scope, liner profiles with expected life in tonnes and the handling tools, lubrication and cooling scope, dust interfaces, and the acceptance basis including a performance window at design tonnage. Naming the station equipment, apron feeder, conveyors, belt scale, secondary cone crusher, and dust collection, lets vendors bid the interfaces correctly.