A spiral concentrator is a gravity separation machine with no moving parts: an open helical trough, wound in a few turns around a central column, down which a thin stream of pulp flows under nothing more than its own weight. As the stream descends, dense grains sink to the bottom of the flowing film and are carried toward the inner edge of the trough, light grains stay higher in the film and are swept toward the outer edge, and at the bottom the band of heavy minerals, the middlings between the bands, and the band of gangue are cut apart by splitters. Mineral Technologies product literature describes the trough and its splitter arrangements; the buying object here is a whole bank, its columns, starts, distributor, and splitters.
The engineer tasked with a spiral circuit at a mineral sands plant, a chromite or iron ore concentrator, a coal preparation plant, a tin or tantalum gravity circuit, or a placer gold operation is the reader this page has in mind. The chapters run from definition to upkeep: what the machine is and the two numbers it is bought to deliver, the physics of the flowing film, the types and their limits, the specification parameters, the selection factors with RFQ wording, and the installation, safety, failure modes, and maintenance of a working bank. The measure of a good bank does not change from one chapter to the next: as much of the heavy mineral as the ore allows, in as clean a concentrate as the ore allows, from starts that are fed evenly and worn little.
The purchase goes right or wrong in five places: the feed, its size range, its slimes content, and the density difference between the valuable and the waste minerals; the trough, its diameter, pitch, profile, and number of turns, which set how far the bands have separated by the bottom; the pulp density and the feed rate per start, which set the thickness of the film and the sharpness of the cut; the splitters, which trade concentrate grade against recovery; and the circuit, rougher, cleaner, and middlings return, which reaches what one pass cannot. Feed and circuit decide more than any trough option.
Chapter 1 / 06
What a Spiral Concentrator Is and What Is Being Decided
A spiral is a column, two to six meters tall, with one or more helical troughs wrapped around it and a frame that carries the whole assembly above the floor. Pulp enters each trough at the top through a small feed box, flows down three to eight turns in a film a few millimeters deep, and reaches a set of splitter blades at the bottom, where it leaves as two to four products. Nothing rotates and nothing opens or closes in normal operation. The only adjustments are the rate and dilution of the pulp entering each start, the name for one helix, and the positions of the splitters at its end, and the only consumables are the linings of the trough, which wear slowly under sand.
A spiral concentrator is bought against a grade and a recovery, both measured on the real ore. The order is for a stated share of the valuable heavy minerals recovered into a concentrate of stated grade, from a feed whose heavy mineral content and size distribution are known, and for a tailings loss low enough for the reserve to pay. Grade is what the downstream separation plant has to work with; recovery is what the mine actually sells. Diameter, pitch, turns, starts per column, and splitters are means to those ends, and a vendor that declines to run a sample of the ore through its own troughs, at the proposed rate and density, has not yet earned the order.
The spiral concentrator belongs to gravity concentration, the oldest branch of mineral processing, and it is worth separating it from two machines that share its name or its place in a flowsheet. It is neither a spiral classifier nor a hydrocyclone: those machines sort by size, and chapter three draws the boundaries. The three are often found in the same plant, one feeding or protecting another, but only the spiral concentrates a heavy mineral from grains of similar size.
The mineral decides how the trough is set. A mineral sands producer recovers ilmenite, rutile, zircon, and monazite from quartz sand and runs rougher and cleaner spirals in long banks. A coal preparation plant runs the opposite case: coal is the light mineral, and the spiral washes shale and pyrite toward the inner edge so that the coal reports to the outer product. An iron ore concentrator upgrades fine hematite or goethite; a chromite producer does the same. Tin, tantalum, and tungsten ores and placer gold reach spirals after crushing, grinding, and desliming, wherever the dense mineral has been liberated.
Running a spiral is cheap; feeding it properly is not, and that contrast shapes every circuit. A spiral uses no chemical reagent, consumes no power of its own, needs only the pumping head that lifts pulp to the top of the column, and has no wearing parts beyond the trough lining and the splitter edges. Against that stand the steps ahead of it: crushing and grinding to liberate the heavy mineral at a fine size, screening to remove oversize and trash, and desliming to remove clay, and these steps commonly outweigh the spirals in cost. A single pass upgrades by a limited ratio and loses some heavy mineral to tailings, so plants accept two or three stages and a middlings return.
Tracing one bank from the pump sump to the tailings launder shows how the parts connect. A slurry pump lifts pulp from a sump to a constant-head box above the top of the columns; a distributor splits the flow into a dozen or more launders, one for each column; each launder feeds one, two, or three starts; the troughs discharge over splitters into launders for concentrate, middlings, and tailings; rougher concentrate is pumped to cleaner spirals on the next row, middlings return to the rougher feed, and tailings flow to a gravity thickener for water recovery. Every start on the bank must receive the same flow, and the whole bank performs only as well as its worst fed column.
Chapter 2 / 06
How Flowing Film, Cross Flow, and Splitters Do the Work
The principle is stratification in a thin, fast stream. Pulp enters the top of the trough as a uniform mixture and spreads into a film a few millimeters deep that accelerates down the first turn and then settles to a steady speed. In that film, dense grains experience a stronger settling force than light grains of the same size and sink toward the trough floor, a process accelerated because the crowded flow lets small dense grains trickle down through gaps in the bed, a mechanism called consolidation trickling. Within one or two turns the film has become layered: heavy minerals along the floor, light gangue above them, and the finest and lightest grains nearest the free surface.
A cross flow sorts the layers sideways. Water in the trough turns as well as slides: near the free surface it moves toward the outer wall, and along the floor it returns toward the inner wall, so each part of the stream travels on a helix of its own across the width of the trough. Heavy grains resting on the floor meet the inward current and are pushed toward the inner edge; light grains held higher meet the outward current and are carried toward the outer edge, where the water runs deepest and fastest. Flat and flaky grains behave as light grains whatever their density, because their large faces catch the surface current.
Trough geometry sets how long and how gently the separation proceeds. Mineral Technologies names diameter, pitch and variable pitch, trough profile, and number of turns among the variables that define a spiral. A larger diameter gives each start more capacity and spreads the bands farther apart before they reach the splitters, which makes the cut easier, but it raises the height of each turn. A longer pitch, the height lost per turn, steepens the trough and speeds the pulp, which raises capacity while shortening the time the film has. A shorter pitch slows the film and sharpens the separation at lower capacity, and the floor profile, a composite curve with a flatter portion near the inner edge, gives the heavy band a quiet place to collect.
Splitters are where the machine becomes a purchase decision. At the end of the lowest turn the flow passes a set of blades whose edges can be swung across the trough, dividing it into two, three, or four products: concentrate from the inner band, tailings from the outer band, and one or two middlings cuts between. A cutter set outward, into the middlings, raises recovery and lowers concentrate grade; a cutter set inward does the reverse. Some designs add diverters partway down the trough, which lift and remove a band early, and repulpers, which add water to keep the heavy band moving; Mineral Technologies lists both, with auxiliary splitters, among its design variables. Others add wash water along the inner edge to rinse fine light grains out of the concentrate.
Pulp density and feed rate control the film that the geometry has to work with. Pulp that is too dense is crowded: hindered settling keeps light grains in the bed and holds heavy grains off the floor, so heavy minerals wander into the middlings and tailings. Pulp that is too dilute carries more water for the same solids load, so the stream runs deeper and faster and sweeps heavy grains into the middlings and tailings before they find their band. Most spiral duties run best at roughly twenty-five to thirty-five percent solids by mass, and the feed rate per start, in tonnes of dry solids each hour, is held within a band set by the vendor's test, since more feed shortens the time each grain has to find its band.
Capacity comes from numbers of starts, and numbers of starts create the distributor problem. A single-start column carries one helix; a double- or triple-start column carries two or three helices wound on the same column, each with its own feed box, and triples the throughput of a floor position. A bank may hold a hundred starts or more, and each must receive an equal share of a pulp that settles if it stands still. The pulp is lifted to a constant-head box, dropped through a stilling section, and split by launders, orifices, or a radial distributor into equal streams; a start that is starved or flooded by a poor split performs below its neighbors on either side.
Chapter 3 / 06
Spiral Types and Machine Boundaries
Duty names the first type. A rougher spiral receives the whole deslimed feed and is set to recover as much heavy mineral as it can, sending a concentrate of moderate grade forward and a tailing that should carry little value. A cleaner spiral receives the rougher concentrate, a much smaller flow, and is set for grade, producing the final concentrate and a tailing that returns to the rougher feed. A scavenger retreats rougher tailings where the ore justifies it. The middlings cut of each stage is neither product and is recycled, to the rougher feed or to a middlings bank of its own where the ore justifies it, and because a spiral bank reaches its steady state only when the recycled load has built up, the circuit, not the single trough, is what the design has to balance.
The Humphreys spiral, the gravity spiral of the mineral sands trade, and the spiral chute sold for iron ore and sand are this one machine under other names. Starts and construction name the second type. Assemblies with one, two, or three starts share a column and a footprint, with the two- and three-start forms favored where floor area is short, as in a plant built on a bench. The earliest spirals were cast iron; most modern troughs are molded fiberglass, an FRP composite shell laid up around a former and finished with a smooth gelcoat, or they carry a polyurethane elastomer lining over the whole surface or over the zones that wear fastest; Mineral Technologies describes its spirals as built from strong, wear-resistant composite materials. Wash-water designs add a small controlled flow along the inner edge for high-grade cleaner duty; wash-waterless designs, common in coal, have no plumbing to maintain.
The first boundary is drawn against machines that sort by size. A spiral concentrator is not a spiral classifier or any other mechanical classifier: those machines hold a pool of water in which coarse grains sink and fine grains overflow, with a rake or a rotating screw lifting the sand out, and they sort by size, while a spiral concentrator sorts by density in a film thin enough for every grain to reach the floor. It is no more a cyclone separator, whose hydrocyclone form presses pulp through a vortex and splits it by size in seconds. Plants use both ahead of spirals, a hydrocyclone to deslime and a screen to remove oversize, because a spiral needs a feed with a set top size and its slimes removed.
The second boundary is drawn against machines that separate by other physics. A flotation cell separates by surface chemistry: collector reagents render one mineral water-repellent so it attaches to bubbles, and a slime-sized or oxidized feed that a spiral cannot stratify may float well. A magnetic separator pulls ferromagnetic and paramagnetic minerals, such as magnetite and ilmenite, by their susceptibility, which is how many mineral sands plants split a spiral concentrate into its minerals. A spiral separates by density alone and works on mixtures where the valuable mineral is at least about one SG unit denser than the gangue, a margin that coal against shale clears and that two heavy minerals rarely do. It ignores magnetism, it uses no reagent, and it cannot separate two heavy minerals from each other.
A bank is only one stage in a plant, and the stages around it decide what it can do. Hard-rock ores, chromite, tin, tantalum, and tungsten, arrive from the pit by mining dump truck, are crushed, typically in a jaw crusher or cone crusher, and travel by belt conveyor to a ball mill or SAG mill, where they are milled until the heavy mineral is liberated but not ground finer than the spiral can treat; mineral sands are free-digging and reach the spirals after scrubbing and screening, with no crusher or mill. A trommel screen or rotary drum screen takes oversize off the scrubber discharge, a vibrating screen with spray wash takes out trash ahead of the spirals, and hydrocyclones remove clay and slimes. A fine concentrate, iron ore or tin, is dewatered in a gravity thickener and then a filter press; in mineral sands the concentrate is dewatered in cyclones and drained, then dried in a rotary dryer before magnetic and electrostatic separation. Tailings are thickened, and the water returns to the mill.
Instrumentation and utilities are few because the machine is passive. An electromagnetic flowmeter on the feed line and a nuclear density gauge, or a Coriolis flowmeter on a smaller stream, give the two numbers that govern a bank, the flow rate and the pulp density of the feed; an open channel flowmeter in the tailings launder shows what the bank passes on. A level transmitter in the pump sump drives the slurry pump, which is usually run through a VFD so that a change in sump level changes speed rather than slamming a valve. An agitator in the pump sump keeps the sand from settling out during a pump changeover. The only utility is water, for dilution and for wash water where the design uses it.
Chapter 4 / 06
Key Specification Parameters
Spiral data sheets are short. They describe the trough, the feed the trough will take, and the load each start will carry, and every figure on them constrains the next one. The values gathered below come from common gravity concentration practice, because the Mineral Technologies pages name the design variables without publishing numbers. A start is one helix, and the ranges are written per start. For a real project the governing numbers are produced by a test on the real ore at the intended rate, and that test, not the table, is where the recovery and grade are fixed; the table shows the neighborhood, not the address.
Parameter
Typical range
What it decides
Trough diameter
roughly 600 to 1,000 mm (23.6 to 39.4 in.)
Capacity per start; distance between bands
Pitch, height lost per turn
roughly 300 to 450 mm (11.8 to 17.7 in.)
Pulp velocity; capacity per start
Trough slope
about 6 to 14 degrees, set by pitch over diameter
Residence time; sharpness of the cut
Number of turns
3 to 8, longer on special designs
Time for the film to stratify
Starts per column
1 to 3
Capacity per floor position
Feed size
roughly 0.05 to 2 mm
Whether grains reach the trough floor
Slimes limit
deslimed below about 10 to 20 micron
Pulp viscosity; clarity of the bands
Feed pulp density
typically 25 to 35 percent solids by mass
Film thickness; crowding of the bed
Feed rate
roughly 1 to 5 t/h dry solids per start
Recovery; grade; number of starts
Wash water
none, or a small metered flow
Cleanliness of the heavy band
Splitters
2 to 4 products, adjustable blades
Grade and recovery of each product
Materials
fiberglass with polyurethane wear lining; cast iron on early units
Wear life; mass of the assembly
Deck arrangement
single or double deck
Floor area per start; access height
Three entries in that table are routinely quoted without the evidence that makes them mean something. A recovery figure needs the heavy mineral content and size distribution of the ore it was measured on, because a spiral recovers liberated grains only, and an ore that is locked or slimed defeats it. Capacity per start needs the pulp density and concentrate grade it assumes, since throughput is bought with recovery. A minimum feed size needs the desliming it assumes, or it flatters a trough that will in fact receive clay. An RFQ should require the test conditions behind every recovery and grade figure and a run on a sample the buyer provides; vendors who tested will answer, and the others will qualify.
Trough materials follow the wear and the chemistry of the pulp. Cast iron belongs to the earliest spirals, which were heavy and are met today only in old plants. Fiberglass shells are light, resist most pulps, and can be molded to the exact profile the designer wants, with a polyurethane elastomer lining on the floor of the trough and around the splitters where sand runs deepest. Frame and fastener steel is galvanized or painted for a wet, humid plant, and a bank needs no heavy structure beyond a braced frame. Wash-water plumbing, where fitted, is a few polymer pipes with small valves at each start.
Chapter 5 / 06
Selection Decision Factors and RFQ Language
The ore comes first and the catalog last. A sample of the run-of-mine material, taken across the ore body, gives the heavy mineral content, the mineral suite with the density of each mineral, the liberation size, and the amount of clay and slimes. The liberation size decides how fine the ore must be ground, and therefore whether a spiral can treat it at all, since grains below about fifty microns stratify poorly. The mineral suite decides how many stages the circuit needs: a heavy mineral sand with one valuable mineral may need two stages, while an ore with several heavy minerals of similar density needs further magnetic or electrostatic separation after the spirals.
Feed preparation decides what the spiral receives. Grinding must liberate the heavy mineral without producing slimes, so many plants grind in a ball mill, return the coarse discharge to it after a cyclone separator classifies it, and deslime before the spiral bank; the fresh feed is commonly weighed on a weigh feeder. Oversize and trash, wood, plastic, and steel, must be screened out, because a single large flake can bridge a feed box and starve a start. The density and flow of the pulp entering the bank should be steady: a pump that surges sends alternating slugs of dense and dilute pulp down every start, and the splitters, set for the average, are then wrong for each.
Circuit and capacity are the same decision. The feed rate per start that passes the test, in tonnes of dry solids each hour, divides into the plant throughput to give the number of rougher starts; the rougher concentrate volume gives the number of cleaner starts, usually a fraction of the rougher count. Single-, double-, or triple-start columns then convert starts into columns and floor area, and a second deck is used where the footprint is tight. A plant that expects its ore to become finer or lower in grade over its life buys spare positions in the distributor and space in the frame for more columns, because a spiral bank is cheap to extend and hard to rebuild.
Cost and lead time concentrate in the mold and in the numbers. A spiral trough is a molded product, so its price per start falls with the size of an order, and a large bank of a standard design ships on schedule, while a new profile or a special liner lengthens the order. The distributor, the frame, the walkways, and the launders can rival the troughs in cost. Fiberglass shells with molded liners are the usual choice for abrasive mineral sands and for coal alike. Spare splitters, feed boxes, and a few spare turns shorten the first interruption, and a test program on the actual ore adds weeks to the order and years of predictability.
What the plant downstream can accept decides where the splitters finally sit. A mineral sands separation plant takes a heavy mineral concentrate within a narrow range of composition, so cleaner splitters are set for grade even at some loss back to the rougher feed. A coal plant sells a product with a limit on ash and sulfur, so its splitters are set to keep shale and pyrite at the inner edge and to accept a little coal in the refuse. An iron ore concentrator has a concentrate grade to meet for the pellet plant. The RFQ should state the product limit for each stage, the recovery expected, and how both are measured.
Nine decisions recur in every gravity circuit, and each one of them needs an answer before an RFQ is sent. A question left open here comes back as a bank that misses its grade or sends its heavy mineral to tailings storage.
Decision
What the buyer states
Cost of leaving it open
Mineral suite
Valuable and gangue minerals, with their densities
Wrong number of stages; an ore that should have floated
Particle size range
Top and bottom size of the feed; liberation size
Grains that never reach the trough floor
Slimes and clay
Minus ten micron content; desliming method
Blurred bands; thick pulp; dirty concentrate
Feed pulp density
Percent solids by mass at the distributor
Film too thick or too thin; off-test recovery
Capacity
Tonnes per hour of dry solids, average and peak
Wrong number of starts; starved or flooded starts
Duty
Rougher versus cleaner; middlings return
Splitters set for the wrong product
Splitters and wash water
Number of products; whether wash water is fitted
A grade that cannot be held at the bench
Layout
Floor area, deck height, access, launder routes
A bank that cannot be extended or walked
Test basis
Sample of the ore; witnessed test; assayed products
Recovery and grade quoted without evidence
A spiral concentrator RFQ should describe the ore, the pulp, and the duty and let each vendor propose its own trough. A complete specification lists: the mineral suite, valuable and gangue minerals with their densities, and the particle-size range of the feed, top and bottom size, with the liberation size; the feed pulp density in percent solids by mass and its tolerance at the distributor; capacity in tonnes per hour of dry solids, average and peak, for the whole plant and per start; rougher versus cleaner duty for each bank, with the middlings return drawn; the number of starts per column and the space available; splitter and wash-water requirements; trough materials and liner for the pulp chemistry; the distributor, frame, walkways, and launders in scope; the power and water available at the site; spare troughs, splitters, and feed boxes; and how acceptance will be judged, which is a test on ore the buyer supplies, with every product assayed for recovery and grade.
Chapter 6 / 06
Installation, Standards, Failure Modes, and Maintenance
Erecting a spiral bank is assembly and leveling work. The frame is bolted to a slab and leveled, the columns are plumbed, and the turns are stacked on each column in order, with each joint aligned so that the trough floor runs without a step or a lip; a misaligned joint throws the film toward the outer wall and spoils the turns below it. The distributor is set level and at the head the vendor specifies, with launders of equal length so that each start receives its share. Walkways need to run along both ends of every bank, because the operator's work is at the top, the feed boxes, and at the bottom, the splitters. Splash guards and floor drainage keep the pulp contained and the walking surfaces dry.
Fill the constant-head box with water and check that every start receives an equal flow, clearing any blocked orifice.
Introduce pulp at the design rate and density, and let the bank run until the middlings return has reached steady state.
At each start, swing the splitters clear and catch the whole flow in buckets placed across the trough width to see where the bands land.
Set the inner splitter between the heavy band and the middlings and the outer splitter between the middlings and the gangue, then lock the blades.
Cut samples of every product with a sample cutter, assay them, and move one splitter at a time until grade and recovery both meet the design.
Standards for spiral concentrators are the standards of the plant around them, because no product standard governs the trough. Access platforms, ladders, walkways, and guardrails follow ISO 14122 for permanent means of access to machinery, and the guards around pump drives follow ISO 14120. Sampling and assay follow the mineral testing standards the plant already uses, named in the RFQ so that vendor and owner report recovery by the same method. Structural steel follows the local building code, and electrical installations follow the local wiring rules. What the RFQ must add is the acceptance test, since nothing else defines whether a spiral performs as sold.
Most trouble on a spiral bank comes from the feed or from wear. Uneven distribution starves some starts and floods others; the flooded ones lose heavy mineral to the tailings while the starved ones make a clean but tiny concentrate, and the sign is a concentrate launder running cloudy on some columns. Wear thins the trough floor near the inner edge and rounds the splitter blades, so the heavy band drifts outward and the cut moves; the sign is a grade that falls slowly over months. Tramp steel and wood bridge feed boxes. A slime buildup from a failed desliming stage thickens the film across the whole bank at once, and a blocked launder overflows pulp onto the floor.
What is inspected and when follows from what the feed does to the trough. The cadences below reflect common practice; an abrasive ore and the vendor's manual shift them, and a bank on coarse mineral sands sits at the short end of each range.
Item
Typical action
Typical cadence
Feed distribution
Check that each start receives equal flow; clear blocked orifices and feed boxes
Each shift
Pulp density and flow
Read the feed density gauge and the feed flow reading; compare with the setpoints
Each shift
Splitter positions
Inspect blades for wear; confirm settings against the commissioning marks
Weekly
Product assays
Cut samples of concentrate, middlings, and tailings; assay for the heavy mineral
Daily to weekly
Trough liner
Inspect the floor near the inner edge for wear through; patch or replace a turn
Monthly to quarterly
Wash water
Confirm flow at each start; clear blocked nipples
Weekly
Frame and walkways
Check bolts, plumb of columns, guardrails, and slab drainage
Quarterly
Pump and sump
Inspect the slurry pump impeller; verify the level transmitter and drive response
Monthly
Full bank survey
Re-run the bucket test on every start; reset all splitters to one standard
Yearly
A bank that tested well at commissioning does not stay that way on its own. Ore changes as a pit deepens: the heavy mineral content, the clay, and the liberation size all drift, and splitters set for last year's ore are wrong for this year's, which a monthly sample and assay of every product stream will show. A regrind or a new desliming stage upstream changes the feed size and calls for the bucket test to be repeated on the whole bank rather than on a few starts. Spare turns, splitters, and feed boxes in stock keep a broken turn from idling a column for a week, and the plants that get the most from spirals are those whose operators walk the bank every day.
FAQ
How does a spiral concentrator work?
Pulp of water, sand, and ore minerals enters a helical trough at the top and flows down three to eight turns in a film a few millimeters deep. Dense grains sink to the floor of the film, by hindered settling and by trickling through gaps in the bed, while light grains stay higher. A cross flow in the trough carries the grains on the floor toward the inner edge and the grains near the surface toward the outer edge, so heavy minerals form a band along the inner wall and gangue a band along the outer. At the bottom, adjustable splitters cut the bands into concentrate, middlings, and tailings. Nothing in the machine moves except the pulp.
What are the main types of spiral concentrator?
Types are named by duty, by starts, and by construction. Rougher spirals treat the whole feed for recovery, cleaner spirals take the rougher concentrate and raise its grade, and scavengers retreat tailings where worthwhile. A column carries one, two, or three helices: a single-start column has one, a double-start column two, and a triple-start column three. Troughs are molded fiberglass, often with a polyurethane elastomer lining, and come with and without wash water, with different pitches, profiles, and numbers of turns for mineral sands, coal, and gold; cast iron survives only on the earliest machines. None of these is a spiral classifier, which sorts by size in a settling pool, or a hydrocyclone, which sorts by size in a vortex; a spiral sorts by density.
What specifications matter most on a spiral concentrator?
Trough geometry, feed condition, and load per start. Diameter, pitch, profile, and number of turns set how far the bands separate before the splitters. Feed size commonly runs from about two millimeters down to roughly fifty microns, after desliming below about ten to twenty microns. Feed pulp density is commonly 25 to 35 percent solids by mass, and feed rate is roughly one to five tonnes of dry solids each hour per start. Beyond these, the number of starts per column, the number and adjustment of splitters, wash water, and the liner material decide what the catalog numbers deliver on the plant floor.
How do you choose a spiral concentrator for a plant?
Start with a sample of the ore and a test on a spiral at the intended feed rate and pulp density. The test gives the recovery and grade the machine can reach and the feed rate per start; no catalog number replaces it. Then fix the feed: grind to liberate the heavy mineral, screen out oversize and trash, and deslime. Size the circuit from the test: plant throughput divided by the feed rate per start gives the number of rougher starts, and the cleaner count follows from the rougher concentrate. State the grade the product must meet and how it is measured, and buy space in the distributor and frame for more columns as the ore changes.
How is a spiral concentrator inspected and maintained?
The work is at the top and the bottom of each column. At the top, operators check that every start receives an equal share of pulp and clear feed boxes blocked by wood, steel, or oversize. At the bottom, they inspect the splitter blades for wear, confirm their positions against the commissioning marks, cut samples of each product, and have them assayed for the heavy mineral. The trough floor near the inner edge, where the heavy band runs, is inspected for wear through, and a worn turn is patched or replaced. Once a year the bucket test is repeated on every start so that the whole bank is set to one standard.
What drives the cost and lead time of a spiral concentrator?
A spiral trough is a molded product, so cost per start falls with the size of an order, and a large bank of a standard design ships sooner than a new profile with a special liner. The distributor, frame, walkways, and launders can rival the troughs in cost. Fiberglass shells with molded liners suit abrasive mineral sands and coal alike, and a bank of triple-start columns saves floor area but not troughs. Lead time lengthens when the buyer asks for a test program on its own ore, which is also the step that decides whether the bank performs as promised. Spare turns, splitters, and feed boxes ordered with the bank shorten the first interruption.
What safety and standards issues come with a spiral concentrator?
A spiral is a passive machine with no drive and no reagent, so its hazards are the plant around it: working at height on walkways beside open launders, wet and slippery floors, manual handling of trough turns, and the rotating equipment of the feed pump. Access platforms, ladders, and guardrails follow ISO 14122, and guards around pump drives follow ISO 14120. No product standard governs the trough itself, and no standard defines its performance, so the RFQ has to name the sampling and assay methods and the acceptance test on which recovery and grade will be judged. Pulp is usually benign, though a plant treating sulfide ores should state the pulp chemistry in the liner specification.