SAG Mill

A SAG mill, short for semi-autogenous grinding mill, is the large-diameter, slow-rotating tumbling mill that performs primary grinding in most modern hard-rock concentrators. Ore is fed directly from crushing or even straight from the mine, and the mill grinds it by cascade and cataract action in which the ore itself does most of the crushing work, assisted by a small charge of steel balls that typically fills six to fifteen percent of mill volume. Autogenous, or AG, mills run the same machine concept with no ball charge at all where the ore is competent enough to grind itself, so AG and SAG are two settings of one machine family rather than two products, and this page treats the complete mill, drive, liner, and discharge system as the purchasing object.

This page is written for the engineer specifying a SAG mill for a new concentrator, an expansion, or a reline and drive upgrade. It works through what the machine does and what is actually being bought, how the charge motion and grate discharge do the work, which design choices such as diameter to length ratio, drive type, and pebble removal separate one offering from another, the parameters that recur on vendor data sheets, and the selection factors and RFQ language that decide whether the circuit reaches design throughput on the actual ore body for a power and liner budget that holds.

Bulk material conveying hardware of the class that feeds SAG mill grinding circuits from the mine and crusher station, shown as an installed belt conveyor

Photo: RICHI Manufacture, CC BY 4.0, via Wikimedia Commons

The decision concentrates in five places: the ore's hardness and competency from testwork, because that single input decides whether AG, SAG, or a conventional crushing and ball mill circuit is right; the diameter and effective grinding length that set throughput and residence; the installed power and drive architecture, gearless, twin pinion, or single pinion, with its speed range; the discharge system, grate, pulp lifter, and trommel screen, with or without pebble ports and a pebble crusher; and the liner and ball charge strategy that sets the operating cost per tonne. Get those right and the cyclone circuit and downstream flotation follow with little freedom.

Chapter 1 / 06

What a SAG Mill Is and What Is Being Decided

The machine this page describes is a horizontal cylindrical steel shell, lined with wear-resistant liners, supported on hydrostatic trunnion or slipper pad bearings at one or both ends, rotated by an electric drive through a gear ring or a direct gearless motor at a speed typically between seventy and eighty percent of critical, the speed at which centrifugal force would pin the charge to the shell. Feed enters through a trunnion or feed chute at one end, water is added to form a slurry, and the tumbling charge of ore and balls breaks the rock until it is fine enough to pass through the grate and pulp lifters at the discharge end into a trommel screen that separates oversize pebbles from the pulp. Installed powers run from a few hundred kilowatts in small units to more than twenty megawatts for the largest gearless machines, and diameters run from under six meters to over twelve meters in the current production fleet.

What is being decided when a SAG mill is purchased is a throughput guarantee against a defined ore, backed by a specific energy statement and a liner wear schedule. The buyer is purchasing the ability to grind a stated tonnage per hour of a stated ore, characterized by hardness indices such as the Bond ball mill work index, the SAG power index, or a drop-weight test profile, to a product size the downstream circuit accepts, at a specific energy consumption in kilowatt hours per tonne and with liner and ball consumption rates that hold the operating budget. Everything on the vendor data sheet, diameter, effective grinding length, installed power, speed range, grate open area, exists to support that guarantee, and honest vendors size the machine from testwork on the actual ore rather than by scaling someone else's mill.

The SAG mill sits in the comminution family with well-defined neighbors that this encyclopedia treats separately. Where the ore comes from a mine, a gyratory crusher or a jaw crusher has already broken it at the face, often feeding the mill through a coarse ore stockpile reclaimed by an apron feeder, and some circuits add a cone crusher in pebble-crushing duty rather than primary duty. Downstream, the SAG discharge usually enters a closed circuit with a cyclone separator whose overflow goes to flotation and whose underflow returns to a ball mill for secondary grinding, the SAB arrangement, or returns through a pebble crusher to the SAG mill itself, the SABC arrangement, and this page leaves the steel-media secondary mill to the ball mill page because that machine has its own duty, media, and sizing logic. Screens and conveyors surround the mill on both sides, a vibrating screen or trommel guards the discharge, and slurry pumps move pulp between stages.

Different buyers buy the same machine for different ore bodies. Copper and gold concentrators in the Americas and Australia made the SAG circuit the industry default because hard, competent ores grind themselves well and single-line capacities of fifty thousand tonnes per day became achievable with one mill. Iron ore and magnetite plants use AG and SAG mills ahead of magnetic separation, where the ore's abrasion dominates the liner budget. Nickel and platinum circuits in hard ultramafic rock run high ball charges to handle tough ore. Diamond operations use autogenous mills deliberately, because smashing ore against ore, called scrubbing duty in its lighter form, liberates diamonds without steel contact that could break stones. The specification language differs, but the machine physics is shared.

The economics deserve their own paragraph because the SAG mill is usually the single most expensive machine in a concentrator and the throughput bottleneck of the whole plant. A mill that is five percent undersized caps the entire mine's revenue at its own limit, and expansions after the fact are costly, so buyers routinely pay for design margin in diameter and power. Installed power cost, the electrical infrastructure for a twenty-megawatt gearless drive is a substation project by itself, liner consumption at the wear rates of abrasive ore, and grinding media consumption together dominate operating cost, and every one of those numbers is set at selection time; remote sites that run the whole train from a gas engine or diesel generator power plant feel the same numbers twice, once as operating cost and once as installed generating capacity. A buyer who compares offers on mill price alone has again compared the smallest number in the least important column.

A short tour of named duties makes the machine concrete. In a typical copper concentrator, trucks dump ore into a gyratory crusher, coarse ore is reclaimed and fed by conveyor to a forty-foot diameter SAG mill driven by a gearless motor at around twenty megawatts, discharge passes a trommel screen, pebbles go to a cone crusher and return, and screen underflow pumps to a cyclone separator battery that splits feed between flotation and a ball mill in closed circuit. In a small gold plant, a six-meter SAG mill in single-stage duty grinds to flotation size directly, with no ball mill at all, trading energy for simplicity. In an iron ore plant, an AG mill with no balls grinds magnetite ahead of separators fed by belt conveyors and weighed by a belt scale.

Chapter 2 / 06

How Charge Motion and Discharge Do the Work

The mechanism is impact and attrition from a tumbling charge. At rotational speeds below critical, the charge rises with the rotating shell on lifters until gravity overcomes friction, then cataracts, falling in a parabola whose toe impacts ore and breaks it by fracture, and cascades, rolling down the charge surface, which abrades and shears particles. The fraction of critical speed, the lifter face angle, and the charge filling together set the balance between high-energy impacts that crack large rocks and the gentler cascading that produces fines, and the operator moves that balance with speed on variable-speed mills and with ball charge and liner profile everywhere.

Autogenous means the ore grinds itself. In an AG mill the largest rocks in the feed become the grinding media that break the smaller ones, which is why ore competency, the strength of the coarse fraction, is the make-or-break ore property for autogenous duty, and why a feed size distribution starved of large lumps starves the mill of media. Semi-autogenous adds a steel ball charge, typically six to fifteen percent of mill volume in SAG duty, which supplies a fixed grinding inventory independent of the ore's lumpiness and stabilizes throughput across ore hardness swings, at the cost of steel consumption measured in grams per tonne and a higher power draw. The practical dial between zero and fifteen percent balls is one of the first results a testwork program produces.

The grate and pulp lifter system at the discharge end converts a tumbling drum into a pump. Slurry fine enough to pass radial slots in the grate enters pulp lifter chambers behind it, which lift the pulp to the discharge trunnion as the mill rotates, and the grate's open area and slot width set both the maximum particle size escaping the mill and the holdup of slurry inside it. Pebble ports are simply larger grate slots that let critical-size chunks, rock too big to grind but small enough to escape, exit the mill deliberately so a pebble crusher can break them outside and return them, preventing the critical-size accumulation that otherwise throttles autogenous throughput. A trommel screen bolted to the discharge end, a rotating cylindrical screen which this encyclopedia treats on its own page, washes and scalps the discharge, returning oversize to conveyors and passing pulp to the sump.

Throughput responds to a small set of handles. Mill weight, measured by load cells or bearing pressure, indicates charge inventory and is controlled by feed rate; water addition to the mill and discharge sump sets pulp density and transport through the grate; speed trims power draw and impact energy on drives that allow it; and ball charge is restored continuously or in scheduled additions to hold its volume fraction. Modern control suites add expert systems or model-predictive layers that push throughput against constraints such as power, bearing pressure, and noise or vibration signatures of impact. The mill vendor supplies the actuators and the mechanical limits; the control philosophy belongs to the plant, and an RFQ that does not state it buys an instrumented machine nobody can tune.

Energy efficiency is the honest tension in the design. Tumbling mills convert only a small fraction of the electrical energy into new surface area, most becomes heat and noise, and the industry's response has been larger single machines, because specific energy improves slowly with scale, plus circuit moves such as pebble crushing and pre-crushing with a high pressure grinding roll, which this encyclopedia covers on its own page, that take hard ore fragments out of the inefficient impact regime and break them under compression. A buyer specifying a SAG mill today is really specifying a grinding circuit architecture, and the mill is its largest single component rather than its whole story.

Wear is the second physics running constantly under the first. Shell liners and lifters in abrasive ore lose profile in months, and a worn lifter face angle changes the charge motion and drops throughput long before the liner is worn through, so liner profiles are replaced on a schedule set by wear measurement, and composite designs, steel bodies with removable wear segments, chrome-moly alloys, and rubber or composite liners in less abrasive duties, trade cost against life. Grinding balls are consumed at grams to kilograms per tonne depending on ore abrasiveness, and the vendor's liner design practice, number of rows, lifter height and angle, pulp lifter radial design, is as much a part of the purchased machine as the shell itself.

Chapter 3 / 06

Mill Types, Circuit Arrangements, and Machine Boundaries

AG and SAG are settings of one machine. A fully autogenous mill runs no steel media and suits competent ores that supply their own coarse grinding inventory; a semi-autogenous mill adds the ball charge for ore bodies whose coarse fraction cannot carry the duty alone, and the same shell, drive, and discharge hardware serves both regimes, which is why plants switch between them as the ore body changes. The vendor conversation is not AG or SAG as separate catalogs but one machine sized and lined for a ball charge range, with testwork deciding where in that range the plant will actually run.

Geometry separates primary mills from secondary ones. SAG mills are large diameter and relatively short, with length to diameter ratios commonly around one to two for the grinding chamber, because primary grinding wants impact energy from a deep charge and high throughput of coarse feed, while the secondary ball mill is long relative to its diameter because fine grinding wants residence time and attrition. Pebble mills, which use screened ore pebbles as media instead of steel balls, occupy a niche where iron contamination matters. Within the SAG family, effective grinding length, the length between end liners, is the number the vendor quotes because it, not shell length, drives the grinding volume.

Drive architecture is a primary fork in the specification. Gearless mill drives wrap the motor rotor around the mill shell, eliminate the gear ring, deliver the highest powers and a wide continuous speed range, and dominate the large end of the market at the highest electrical sophistication. Twin-pinion drives, two motors through girth gears, cover the middle range with proven robustness and partial speed control through variable frequency drives, and single-pinion drives with wound rotor or squirrel cage motors serve the small end where simplicity wins. The drive choice decides the electrical scope, the maintenance skill set, and the speed flexibility the control system will live with for decades, so it belongs in the RFQ, not in a vendor's default.

Circuit arrangements name the mill's context. In a SAB circuit the SAG mill runs in open circuit with a discharge screen, and screen undersize pumps to a cyclone separator battery whose underflow feeds a ball mill in closed circuit with the cyclones. In an SABC circuit the cyclone underflow returns to the ball mill while SAG discharge pebbles pass through a pebble crusher, a short-head cone crusher in most plants, and return to the SAG feed, protecting the mill from critical size. Single-stage SAG circuits close the SAG mill itself with cyclones and skip the ball mill entirely where the ore grinds fine enough in one pass, common in smaller gold plants. Pre-crushing circuits add a high pressure grinding roll or a cone crusher ahead of the SAG mill to cut specific energy.

Adjacent machines mark the boundary. The SAG mill is not the ball mill, whose steel-media secondary duty has its own page, and it is not the rod mill of older circuits, which this site leaves to general comminution history. Upstream it takes feed from a gyratory crusher or jaw crusher, often via stockpile and apron feeder, and its discharge trommel is a trommel screen, covered separately, while a vibrating screen may replace it in some plants. Downstream it hands pulp to a slurry pump sump, cyclones, and usually a ball mill, then flotation or magnetic separation, with a gravity thickener and a filter press or screw press handling tailings and a decanter centrifuge on some concentrate streams. Ore arrives on conveyors weighed by a belt scale and may be metered by a weigh feeder, and mill water recirculates through a cooling tower circuit in some plants; none of those neighbors is part of the mill purchase, but every one of them appears in the interface list of a complete RFQ.

Chapter 4 / 06

Key Specification Parameters

The vendor data sheet for a SAG mill centers on geometry, power, speed, and discharge, and each number carries a sizing consequence. The table below lists the parameters that recur across manufacturers' catalogs for the primary grinding fleet, with typical ranges a buyer will see across the market from small single-pinion machines to the largest gearless units. Values for a specific project come from ore testwork and throughput targets, and the ranges here are orientation, not a substitute for that engineering.

ParameterTypical catalog rangeWhat it decides
Mill diameter (inside liners)5 to 12.8 mImpact energy scale; maximum feed size; single-line capacity
Effective grinding length2 to 9 mGrinding volume; residence time at design tonnage
Installed power1 to 28 MWThroughput ceiling; specific energy margin
Fraction of critical speed70 to 80 percentCharge motion regime; impact versus cascade balance
Ball charge, SAG duty6 to 15 percent of volumeGrinding media inventory; power draw; steel consumption
Total charge filling25 to 35 percent of volumeHoldup; throughput; bearing load
Feed size, F8080 to 150 mm typicalPrimary impact duty; crusher circuit upstream
Product size, T801.5 to 4 mm to cyclone feedBall mill or downstream circuit feed quality
Grate open area and slotVendor-specific per diameterDischarge capacity; pebble escape; pulp holdup
Liner set life, abrasive ore4 to 9 months shellAvailability; relines per year; operating cost

Three of these numbers deserve the buyer's suspicion when they arrive without a basis. Installed power quoted without the corresponding speed range and drive type hides whether the mill can actually use the power at the charge the ore will carry. Effective grinding length quoted as shell length pads the volume the charge never sees. Liner life quoted without naming the ore and the ball charge is a number from a different mine. An RFQ that asks for the basis of each figure, test data, reference plants on similar ore, or vendor standard practice, separates engineered offers from assembled ones.

Materials and construction follow the ore. Shell and head steel are specified by the mill builder to code stress requirements; liners are chrome-moly steel in most hard-rock duty, rubber where ore is less abrasive and mills smaller, and composites where impact and abrasion trade; grates and pulp lifters are steel or metal-backed rubber; and the trommel screen panels are polyurethane or wire. Trunnion bearings are hydrostatic with high-pressure jacking for startup. Feed chutes wear hard and are lined with wear plate or ceramic. Each wear interface has a stated replacement interval in operating hours or tonnes, and those intervals, times the relines per year, set the maintenance labor plan and the spare liner inventory the buyer must budget.

Chapter 5 / 06

Selection Decision Factors and RFQ Language

Selection starts with the ore body, not the catalog. Comminution testwork, Bond indices, drop-weight and abrasion tests, SAG power index or equivalent pilot and semi-industrial programs, produces the hardness and competency profile that decides AG versus SAG, the ball charge range, and the specific energy the circuit needs. A geometallurgical model that maps hardness across the ore body protects the design from sizing to an average that half the mine fails to meet. Buyers who skip this work buy a mill sized for an ore they do not have, and the throughput shortfall appears every day of the mine's life; it cannot be fixed by control tuning.

The circuit decision frames the machine decision. Single-line capacity, the tonnage one mill must carry, sets the diameter class and the drive power, and the SAB versus SABC choice, with or without pebble crushing, changes both the grate design and the downstream equipment list. Pre-crushing with a high pressure grinding roll or cone crusher ahead of the SAG mill can cut specific energy or raise throughput on an existing mill and belongs in the trade study even when the final answer is to omit it. The mill vendor supplies the mill; the circuit belongs to the buyer's metallurgist, and the RFQ should present the circuit, not ask the vendor to invent one.

The table below organizes the decision into the factors that recur across projects, with the questions the buyer should be able to answer before the RFQ goes out. Each row is a place where an incomplete answer becomes an underspecified mill and a throughput argument later.

Decision factorWhat the buyer must stateConsequence if left open
Ore and testworkHardness indices, competency, abrasion, geometallurgical spreadMill sized to a guess; guarantee is void on the real ore
Throughput and stagesDesign and peak tonnes per hour, single-line intent, SAB or SABCDiameter and power wrong; bottleneck lands in the wrong place
Feed and product sizeF80 from crusher or stockpile, T80 target to downstreamGrate, trommel, and media choices mismatched
Drive architectureGearless, twin pinion, or single pinion intent; speed range neededElectrical scope and control flexibility fixed by vendor default
Pebble strategyPebble ports yes or no, pebble crusher destination, recycle routingCritical size accumulates; throughput decays
Wear environmentOre abrasion, target liner life, media consumption allowanceLiner budget and reline schedule undefined
Interfaces and layoutFeed chute, discharge trommel or screen, sump and pump, crane accessReline access and interface steel contested late

RFQ language for a SAG mill should name the ore and the basis of guarantee. A workable specification states: ore source and comminution test basis with the hardness and competency data attached; design and maximum dry tonnes per hour with the ore's bulk density and moisture; feed size distribution including F80 and top size, and the product T80 the downstream circuit accepts; whether AG, SAG, or a ball-charge range is intended with the expected charge window; required effective grinding volume and the vendor free to propose diameter and effective grinding length; installed power with the drive architecture named and the speed range stated; grate design with pebble port intent and the trommel screen scope; liner materials and target liner life for the stated abrasion with media consumption allowance; bearing and lubrication scope; and the acceptance basis, witnessed mechanical run, load test, and a performance window defined as throughput at product size against the testwork prediction. Naming the interface equipment, the apron feeder or belt conveyor on feed, the cyclone separator battery and slurry pump on discharge, and the pebble crusher if the circuit includes one, lets vendors bid the connections correctly.

Chapter 6 / 06

Installation, Standards, Failure Modes, and Maintenance

Installation is a heavy-lift and precision project measured in months. Foundations carry a mill that can exceed two thousand tonnes with charge; ring motor or pinion alignment tolerances are fractions of a millimeter; and the shell is shipped in segments, field-welded or flanged, then lined before the charge goes in. Commissioning runs the drive first on barring gear, then unloaded, then with charge in steps, watching bearing temperatures, vibration, and power draw against the vendor's curves. Feed systems, the apron feeder or conveyor and chute, and discharge systems, trommel screen, sump, and slurry pump, commission with the mill because nothing else can move the first ore. Vendor field supervision through first ore is standard and should be priced in the RFQ rather than assumed.

Standards for grinding mills are practical and mostly structural rather than a single machine code. Mill structures follow the plant's design code framework for steel and foundations; rotating machine safety follows jurisdictional guarding practice; motors, drives, and transformers follow the applicable electrical apparatus standards; and large gearless drives follow the rotating machine and converter standards of their class. There is no single international SAG mill standard that governs the machine end to end, so the RFQ must name the applicable structural, mechanical, and electrical codes and the vendor's own manufacturing standards for shell stress, girth gear quality, and balance. Any edition reference in project documents should be verified against the current issue at purchase time rather than copied from an old specification, because drive and electrical standards in particular are revised on short cycles.

The recurring failure modes are honest and mostly scheduled. Liner wear is the dominant event, throughput decays as lifter profiles round, and relines, which stop the mill, are planned from wear surveys at every shutdown; a missed survey turns a planned reline into an emergency one. Bearing distress, from oil contamination, cooling failure, or dirt in the high-pressure jacking system, is rare but stops the plant, so lubrication skids are instrumented and alarmed. Girth gear and pinion wear in geared drives is monitored by tooth contact checks and vibration; gearless drives shift the risk to power electronics and cooling, which are maintained on their own schedules. Slurry washouts through worn grates and pulp lifter erosion appear as tramp oversize in the trommel and are caught by screen surveillance.

Maintenance planning is interval driven and shutdown shaped. The table below lists the recurring items with the typical cadence a plant will schedule, assembled from common vendor practice; actual intervals follow the ore's abrasion, the mill's utilization, and the wear survey data from the first year of operation.

ItemTypical actionTypical cadence
Shell and end linersWear survey, partial or full reline at limit4 to 9 months
Grate and pulp liftersInspect slots and chambers, replace on erosion limit3 to 6 months
Trommel screen panelsInspect panels and sprays, replace worn sections1 to 3 months
Ball chargeReplenish to target volume percentDaily to weekly additions
Bearings and lubricationOil analysis, filter change, high-pressure system checkMonthly checks, service per hours
Drive trainVibration survey, gear contact check or motor diagnosticsQuarterly
Feed chute and dischargeWear plate renewal, trommel seal inspectionEach reline window

Long-term care keeps the circuit honest against the ore body's drift. As mining moves, hardness and competency shift, and the ball charge, speed, and grate design that were right at commissioning slowly become wrong; periodic mill surveys, charge audits, and energy-per-tonne reviews recover the throughput tenths that compound into serious money across a mine life. Liner profile evolution, new alloys, and optimized lifter geometries are offered for existing mills and often pay in availability or energy. The plant that treats the SAG mill as a living machine, measured every shutdown and adjusted, is the plant whose single most expensive asset is still earning its design throughput in year fifteen.

FAQ

What is the difference between a SAG mill and an AG mill?

Both are the same large-diameter tumbling machine. An AG, autogenous, mill runs with no steel grinding media and relies entirely on the ore's own coarse lumps as the grinding charge, which suits competent ore that supplies its own media. A SAG, semi-autogenous, mill adds a ball charge, typically six to fifteen percent of mill volume, that stabilizes grinding when the ore's coarse fraction cannot carry the duty alone. Most plants run semi-autogenous because ore hardness varies across a body, and the same shell can shift between the regimes as the mine changes.

What does SABC mean in a grinding circuit?

SABC names the equipment chain: SAG mill, ball mill, and pebble crusher. The SAG mill grinds primary feed, discharge passes a trommel screen, undersize pumps to cyclone separators, and cyclone underflow feeds the ball mill. Oversize pebbles from the trommel, rock too large to grind further but small enough to escape the grate, pass through the pebble crusher, usually a cone crusher, and return to the SAG feed. The crusher removes critical-size accumulation, the classic throughput killer in autogenous duty, which is why SABC is the default arrangement for hard-ore concentrators.

How is SAG mill size and power determined?

From ore testwork and throughput targets. Comminution tests, Bond work index, drop-weight profiles, and a SAG power index or equivalent, give the specific energy in kilowatt hours per tonne the ore needs; multiplying by design tonnes per hour gives installed power with a design margin. Geometry follows power class and residence needs, with diameter dominating for impact energy and effective grinding length supplying volume. Vendors then confirm the selection against their reference mills, and buyers should insist the guarantee references the testwork, not an analogy to another mine.

Why do gearless drives dominate large SAG mills?

A gearless mill drive wraps the motor rotor directly around the mill shell and eliminates the girth gear and pinions. That makes the highest powers practical, twenty megawatts and above, gives a wide continuous speed range the control system can exploit to follow ore hardness, and removes gear maintenance as a constraint. The trade is electrical complexity, a converter and cooling plant of its own, and specialist maintenance skills. Below roughly twelve megawatts, twin-pinion drives with variable frequency remain competitive and simpler to support, which is why both architectures persist.

What are pebble ports and why do they matter?

Pebble ports are enlarged openings in the SAG mill grate that let critical-size chunks leave the mill before they accumulate. Critical size is the fraction of ore, typically a few tens of millimeters, that is too small to break efficiently as grinding media but too large for the grate slots to pass; if it stays inside, it cushions the charge and throttles throughput. With pebble ports the material exits to the trommel screen, reports to a pebble crusher, and returns broken, keeping the internal charge clean. Mills on hard ore without a pebble path lose capacity steadily between grinds.

What wear parts drive SAG mill operating cost?

Liners and grinding balls dominate. Shell and end liners in abrasive hard rock wear out in four to nine months, and relines, mill stops with crews working inside the shell, set the maintenance calendar; grate and pulp lifter sets live shorter lives. Ball consumption runs from grams to more than a kilogram per tonne depending on ore abrasiveness and ball charge. Bearing and lubrication costs are small but availability-critical. Vendors should state expected liner life and media consumption for the named ore, and buyers should budget on those wear bases rather than on the liner purchase price alone.

What should a SAG mill RFQ include?

State the ore and its comminution test basis with data attached; design and peak dry tonnes per hour; feed size distribution and F80; product T80 to downstream; AG versus SAG intent with the expected ball charge window; required effective grinding volume with vendor free to propose diameter and length; installed power with drive architecture and speed range; grate design with pebble port intent and trommel screen scope; liner materials and target life for the stated abrasion with media allowance; bearing and lubrication scope; interface equipment such as apron feeder or belt conveyor on feed and cyclone separator plus slurry pump on discharge; and the acceptance basis against the testwork prediction, including vendor field supervision through first ore.

Sources

  1. Metso Select SAG Mills datasheet (PDF)
  2. Metso Select mills brochure (PDF)
  3. Metso Grinding solutions brochure (PDF)
Ask SpecForge AI