A loss-in-weight feeder meters material by weighing a hopper and its discharge mechanism while the contents are being fed. The feeder estimates mass flow from how quickly its measured weight falls and adjusts a screw, vibratory tray or other dosing device to hold a target. When material is added to the hopper, the weighing signal contains both addition and discharge. The controller uses an alternate estimate of discharge until ordinary gravimetric control can resume.
The equipment is specified as a weighing and dosing system. Its actual range and delivery error depend on the material, installed mechanical interfaces, the feed mechanism and the refill sequence. A useful offer answers how the machine will hold the recipe under the plant's real conditions, including the moment the hopper fills.
Historical batching deck with suspended weigh hoppers. Context photo: U.S. National Archives (NARA), Hoover Dam construction record, Public domain via Wikimedia Commons.
Budget the feeder around a working material sample, the smallest and largest required mass rates, and the independent test used to verify both routine dosing and refill. Geometry and control must work together on the most difficult ingredient, which may be the lightest, slowest or stickiest one in the line.
Chapter 1 / 06
What a Loss-in-Weight Feeder Measures
The weighed assembly normally includes the hopper, the feeding body and selected equipment rigidly attached to them. Its total load is the dead weight of the assembly plus the changing inventory. While the inlet is closed, a decrease in measured mass over elapsed time gives an estimate of the discharge. If an independent mass sample is needed, collect the output at the receiver and weigh it separately. Agreement between the feeder's indicators and the recorded settings is useful for diagnostics. Acceptance of dosing itself depends on comparison with a separate measurement.
The mechanical and measurement boundary is a prominent buying distinction. A load cell is a force transducer that can support a weighed vessel, with a strain gauge used in a common sensor construction. A hopper scale weighs material in a vessel, which can also be useful in a gain-in-weight process. A bench scale may help check a catch sample. Each of those devices can form part of a plant measurement strategy. The loss-in-weight feeder includes the driven metering element and a controller that repeatedly compares estimated delivery to its assigned rate.
A continuous weigh feeder on a belt uses belt loading and movement to determine flow during passage. A separate belt scale can provide rate or accumulated tonnage on a belt without necessarily controlling it. A belt feeder meters material out of a bin and can work with a volumetric arrangement. The applications overlap at a system level, especially when a designer can choose several ways to meter an ingredient. Batch recipe precision, very low throughput, material behavior and plant space can favor the weighed hopper. Large bulk streams often point the other way. Ask for quoted products to be tested against the same mass delivery duty.
In continuous proportioning a master rate may be supplied by the downstream line controller. Each loss-in-weight feeder then delivers its ingredient at the rate derived from the recipe and its own testable operating envelope. A batch duty can stop at a target mass loss or use a coarse and fine delivery sequence. Batch error can involve material still falling past the discharge at the stop command or a delayed shutoff. Specify whether mass is accepted at the feeder outlet, in the receiving vessel or in the finished batch. Each point captures different loss, in-flight material and holding volume.
Bulk density is mass per occupied volume for the loose material in a named condition. It can change after transport, storage, agitation, drying or refill. One volume per screw revolution can therefore represent a different mass on different days. Gravimetric feedback compensates within the mechanical capacity and stability of the feeder. A blocked throat, variable degree of screw fill or inadequate torque sets physical limits. The controller cannot deliver powder it cannot get into its discharge device. Test with representative material and reject the assumption that a single bulk-density value fully specifies the way it will flow.
Device or arrangement
Directly observed quantity
What the plant should verify
Loss-in-weight feeder
Change in weight of the dosing assembly during normal discharge
Delivered mass and rate, including refill periods
Volumetric screw feeder
Discharge setting such as screw speed
Delivered mass for each relevant material condition
Material test along the weighed span and delivered total
Batch receiving scale
Weight gained by the receiving vessel
Batch target, cutoff and material held between feeder and receiver
Chapter 2 / 06
Weighing, Filtering and Refill Control
The charge of material can change within the feeder even when the sum of its weight is known. A fine powder dropped into a low-inventory hopper may hold air and flow more freely for a short period. A dense, angular material can pack against the walls and load the tool differently after a refill. The same speed command used before the event can then deliver a different mass. Support the tuning decision with a sample of the actual refill material and its feeding method. A supplier can distinguish disturbances from impact and pressure from changes in bulk state by running trials with agreed positioning and reference collections that span the transition.
The weight signal contains effects from machine vibration, blower or vacuum pulses, mechanical contact and incoming material as well as the desired loss of mass. The controller estimates the slope over a finite period using a filtering or estimation method. A very short estimate may follow vibration or the cyclic discharge of a screw. Heavy filtering can make the rate slow to respond when the actual flow changes. Ask how the quoted accuracy depends on the averaging window and whether the same window is representative for the process. A feeder supplying ingredients into a short-residence mixer can need evidence on a shorter window than a feeder filling a surge hopper.
The moving weight range for a low-rate ingredient can be small even when the plant is using a scale with adequate total capacity. Define the dead weight, operating inventory and smallest mass change the system needs to resolve over the selected measurement window. If an inlet bellows rubs on the suspension or the outlet is held in a rigid chute, force bypasses the intended weighing path. The controls can compensate for only some predictable effects. Verify that utilities, guards, ducting and cables leave the weighing structure free over the whole range of operating movement and temperature.
During refill the incoming flow raises the hopper weight and breaks the ordinary loss calculation. Many feeders hold a volumetric discharge command based on the recent stable conditions, or apply a controller model to account for expected fill behavior. When the refill gate closes, added material settles and the weighing signal returns to a usable state. The controller then transitions back to gravimetric operation. The term refill compensation describes a strategy and its performance depends on the implementation. Ask for a trend showing inlet command, weight, estimated delivery, control state and actual catch data before, during and after the refill event.
A refill cycle starts before the usable inventory falls below the level at which the feeder can sustain uniform delivery. The upper limit leaves suitable free space for the incoming surge and provides an operating inventory for the next interval. A very small refill can make the unit spend much of its running time in the alternate control mode. A large refill can compress or aerate the powder, increase mechanical forces on the weighed hopper and lengthen settling time. The most useful specifications give a refill mass, duration and frequency window for each case and name who supplies the inlet equipment and its signals.
A rotary airlock may form part of a refill arrangement where a pressure boundary has to be maintained. A screw conveyor can deliver a controlled stream from a buffer bin, and a station using a bulk bag may operate intermittently. The refill storage needs enough usable mass for repeatable operation under the expected delivery constraints. Ask which of these items is on the scale and which one is structurally independent. If an upstream device dribbles after the refill completion signal, the controller may resume normal estimation before the inlet actually stops adding material.
Operating phase
What the weight trace shows
Dosing evidence to capture
Stable gravimetric feed
Falling mass with material-related variation and measurement noise
Commanded rate, estimated rate and time-matched independent collection
Low inventory and refill request
Mass approaching the selected operating low point
Refill trigger, response delay and remaining working inventory
Filling
Net gain while the dosing mechanism can still be running
Refill duration, feed command, independent mass delivered during the window
Settling and transfer
Transient fluctuations as forces and bulk state settle
Time to stable estimation and combined output over refill and recovery
Fault or stopped feed
Trace may show an impossible slope, empty hopper or stale value
Alarm, host message, safe response and documented restart condition
When the hopper or discharge is connected to a vent system, a pressure difference can exert an apparent force on the weighed assembly. Loose connection boots and pressure compensation features may help if the package is engineered for the actual environment. Also identify static forces from hose routing, compression of flexible joints and any change in upstream fill pressure. The plant controls philosophy should say how instrument failure and invalid weight data are reported. During site testing include the normal ventilation states and neighboring machines most likely to introduce disturbances. A quiet bench result can hide failures that appear only when the entire line is running.
Chapter 3 / 06
Screw, Vibratory and Other Feed Mechanisms
Tooling selection also determines what happens at zero demand. Some powders can leak through an idle tool, while pellets may retain a short column of material that falls after an outlet device opens. A feeder serving a batch operation may need a positive shutoff or a provision that keeps product out of a receiving line waiting for another recipe. Establish whether such a component is inside the weighed boundary and how its moving parts, flexible connections and hold-up affect the result. Define the release and restart sequence in the controls design so any retained material goes to the intended batch and can be inspected when carryover is investigated.
A single screw can suit pellets and certain powders that enter and move through the flights consistently. Screw pitch, diameter, core and outlet opening determine what volume can be carried at a given speed. Some duties need a hopper agitator or other approved flow aid to keep the throat filled. In other duties unnecessary agitation generates fines, compacts the product or disturbs the weight signal. A single screw may be easier to clean or replace where frequent changeover matters. Coperion describes the stainless steel Coni-Steel hopper and internal agitator and access from the nonprocess side for its MechaTron design, available in volumetric or gravimetric use [4]. Confirm the offered layout matches the station's access constraints.
Twin screws offer different feeding tools for cohesive powders, fibers and flakes or for applications that need better flow consistency from a difficult hopper. They have geometry and clearance that must suit the product, and tooling changes can meaningfully change capacity. The K2-ML-D5-T35 example lists several screw forms and fine or coarse pitches [3]. A screw set proven on one material can have poor fill or unacceptable compaction on another. Ask the supplier to identify tool materials, acceptable wear, removal method and any need to change gearing across the process rate range. The drive must sustain the worst representative material condition as well as the high speed implied by the nominal capacity.
A vibratory tray can suit free-flowing or fragile ingredients where handling through screw flights would be undesirable. Its movement needs to feed the product at the usable lowest rate without intermittent starts that undermine recipe uniformity. At a high rate the material bed on the tray and the inlet supply must remain controlled. Since vibration is inherent in the feeder, the weighing arrangement and measurement filter are part of the design. The best way to compare a tray proposal with a screw proposal is to specify expected product condition as well as the test for short- and long-window mass delivery.
Standard choices extend to specialized bulk-solids devices and liquids. K-Tron lists single and twin screw and liquid loss-in-weight feeders among its different families and explains the importance of matching equipment to material properties [1]. A liquid version can use metering equipment on a weighed supply vessel. Effects such as pump pulsation, pipe forces and leakage still matter even though the material is pumpable. For dry powders, measure moisture with an appropriate moisture analyzer when moisture affects flow. Material samples should span the actual feed condition, including dried material coming from a fluid-bed dryer or a fine powder made by a spray dryer.
Handling choice
Representative use
Ask the supplier to measure
Single screw
Flowing pellets and powders whose screw fill is reproducible
Rate variation, gear range, screw fill at low inventory and cleaning time
Twin screw
Cohesive powder, fibers or flakes with verified suitable tooling
Torque, buildup, refill stability and screw change scope
Vibratory tray
Free-flowing or fragile particles with a stable discharge bed
Short-window delivery at the low rate and product condition at high rate
Agitation or conditioning
Hopper-throat flow assistance for a characterized handling issue
Mass delivery before and after refill, buildup and segregation
Liquid metering head
Pumpable ingredient with suitable pressure and material compatibility
Pulsation, usable mass resolution and outlet pressure effects
Poorly flowing ingredients may bridge above the throat, form a stable channel surrounded by stagnant material, adhere to walls or suddenly flush after aeration. Those behaviors need distinct remedies. Tighter screw pacing cannot correct a persistent overhead bridge, and an agitator can worsen segregation of some mixtures. A plant receiving product from a paddle dryer or rotary dryer may see different temperature, moisture or size from the material used to pick a standard feeder. Define storage interval, head of material and handling history for performance samples so the trial includes the condition that challenges the throat.
Chapter 4 / 06
Key Specifications and Rating Evidence
For a very low-rate application, obtain the catch mass anticipated during the shortest required interval before selecting a reference instrument. If that amount is too close to the resolution of the reference scale, longer collection can establish the cumulative result and a more sensitive method may be needed for local variation. Agree whether delivery variation refers to successive nonoverlapping samples or a rolling window. Report rejected catches and the reason they were excluded. Document material left on the transfer chute, dust retained by extraction and residue in the collection arrangement. The acceptance method needs enough resolution to discriminate a process error from measurement and recovery error.
A proposed operating range should include the smallest, usual and largest mass rates for the actual ingredient. State bulk density as measured on the supplied sample and characterize its variation. The theoretical volume moved per revolution is useful for checking a geometry choice, but the vendor must assess changing fill and torque. As a model-specific example, Coperion's K2-ML-D5-T35 sheet gives volume ranges of 2.9 to 1,417 cubic decimeters per hour for coarse-pitch twin concave screws and 2.1 to 920 cubic decimeters per hour for fine-pitch twin concave screws [3]. These sample values use free-flowing semolina with the documented servo and controller arrangement. The sheet says actual rates depend on material characteristics. The example gives no guarantee for an unrelated powder.
Nominal feed accuracy may represent average deviation from setpoint, scatter between catches or a statistical band on repeated measurements. Those are different metrics. Require a definition of averaging time, reference scale accuracy and number of repeats. Specify both mass deviation on a steady run and behavior across a refill with the outlet operating. If the ingredient is used in a critical recipe, establish the smallest weight of a finished quantity or shortest residence in which a variation matters. Set acceptance limits on that time or batch basis as well as on the longer cumulative total. A monitor built into the feeder can log what it estimated, but it does not independently verify what entered the process.
Specification
State the basis
Reason for requiring it
Rate range
Actual mass per time at minimum, normal and maximum for each material
Confirms that the selected throat and tool have useful range
Turndown
Largest divided by smallest guaranteed continuous rate with named tooling
Avoids quoting a maximum and minimum that require different hardware
Mass error
Setpoint deviation and repeatability over specified windows
Links feeder data to finished product uniformity and process residence
Refill duty
Usable inventory limits, refill mass, settle time, frequency and supply device
Establishes how much of each run depends on alternate control
Weighing envelope
Dead load, live load, signal resolution and mechanical overload provisions
Protects low-rate measurement after the equipment is installed
Materials and finish
Product-contact parts, seals, access, surface and cleaning method
Controls corrosion, contamination, wear and maintenance needs
Environment and utility
Vibration, dust, ambient, washdown, drive load and connection design
Captures plant conditions that can affect dosing performance
Control interface
Setpoint source, units, alarms, state, event log and factory testing plan
Avoids a functioning feeder that cannot be operated as part of the recipe
An AC motor and variable frequency drive may be appropriate at some rates and loads. Alternative drive options can give finer speed control or useful torque characteristics at slow rates. Ask for motor and gear checks at the actual operating extremes, restart with the credible loaded condition, and the longest drive run at slow speed. Record the method used to estimate discharge when the weight slope is unavailable. The plant programmable controller should read an unambiguous status for that mode so the run historian can distinguish normal feedback from modeled delivery.
A useful quote identifies measurement traceability. Scale calibration with reference weights checks some of the measurement chain. Independent flowing material tests demonstrate dosing under realistic conditions. New material, a replacement screw or an extended connection boot can make previous calibration data insufficient. Establish the owner's reference weighing method, sample transfer and retention rules. Provide a way to measure low-rate material without losing dust on a larger collection container or disturbing the flow with an unsuitable collection technique. Keep raw time and mass data so reported accuracy can be recomputed after a test without interpreting a screen capture.
Chapter 5 / 06
Selection, Integration and RFQ
For several feeders serving one process, simultaneous refill can be a practical limit. A common receiver or vacuum system may refill only one feeder at a time, or more than one feeder may need to avoid estimating delivery simultaneously during a sensitive recipe. Give the line integrator the usable inventory at every rate and the realistic upper bound on refill delay. Include what happens when the upstream supply is unavailable for part of a run. This turns a collection of individual machine capacities into a schedule that can be tested. If a common refill queue is used, inspect priority and low-inventory alarms under a controlled combined test.
Match the line recipe to actual dwell and discharge dynamics. A ribbon blender can accumulate ingredients for a batch. A downstream high-shear mixer may see concentration changes if an ingredient surges, with consequences depending on its mixing dynamics. A liquid leg can feed a static mixer where the concentration depends on the simultaneous delivery of the inlet streams. In a compounding plant, each feeder can assign a polymer, filler or additive to a different feed point. Coperion's K 2025 publication describes feeder equipment in its broader compounding and bulk-handling offering [2]. Its component examples do not establish performance for another recipe.
When the delivered material may contain agglomerates or tramp matter, assign upstream protection that preserves the size fraction and flow character needed to dose the ingredient. A vibrating screen can remove lump material where appropriate. A magnetic separator can handle specified ferromagnetic contamination. A pneumatic refill or dust extraction system may have a cyclone separator and bag filter as components. Put the vent arrangement and expected pressure differential in the inquiry. Keep connections off the weighing path unless they are included in the design and tested with the assembled feeder.
Daily operating changes define the choice of mechanical access. If two formulations must be kept separate, request the surfaces that will contact both and how residues are removed and verified. Assess whether wet cleaning is allowed and what drying or inspection follows. Wet-rated electrical equipment alone does not establish a complete sanitary or washdown design. For hazardous areas, document the process material and area classification with the responsible site engineer, including inside and outside the hopper as applicable. The datasheet's optional approvals and a generic motor designation are insufficient to approve equipment in the installed configuration. Request project-specific declarations, drawings and responsibility boundaries.
RFQ schedule item
Give the vendor
Ask for the verified reply
Ingredient properties
Samples, density, shape, moisture, particle sizes, temperature and flow history
Chosen tooling and proof on the named production material
Recipe and downstream equipment
All rates, batch sizes, recipe sequencing and available hold-up
Stable time window and acceptable transitions at low and high demand
Refill and source
Silo, bag or batch supply, available height and volume, mode of conveying
Feed and outlet connections, useful inventory and compensation method
Cleaning and environment
Product contact criteria, area class, washdown and minimum accessibility
Materials, removals, hazardous-area configuration and cleaning procedures
Acceptance
Independent mass collection method, timing and error limits
Test conditions, raw evidence, tolerances and applicable retest rules
The RFQ should specify whether the line needs continuous proportional delivery or batch cutoff, identify minimum and maximum rates for each material, define acceptable steady and refill error, and disclose the live equipment above and below. Provide the wet cleaning and area classification requirements for the application and whether a belt option is under consideration for the highest mass rate. Request a sample trial that includes proposed geometry, a production-like refill, cleaning access and low-rate operation with a realistic material level. Vendors should quote setup and product changeover separately from active feeding. The buying team can then compare capacity, loss, intervention time and spare parts on a matched process basis.
Keep a downstream check separate from feeder feedback. A checkweigher can inspect the total mass of packaged units where appropriate. A correct package mass can still conceal a wrong ingredient proportion if different feeders offset each other's errors. A downstream blend sample or suitable product test may be useful when ingredient distribution is a quality characteristic. Choose these quality checks according to what happens to a missed or short dose. When a process can divert suspect batches, agree how the feeder logs deviation and which process or batch identifier travels with the reported event.
Chapter 6 / 06
Installation, Testing and Troubleshooting
Test a product change at the same station that will serve routine production. Establish the normal material left in the screw, throat and discharge after emptying. Give the operator a way to record the recipe, equipment identifiers and the time the first accepted material is released, especially when several formulations share a line. A feeder that can be emptied quickly can still incur a long restart if another formulation requires a different tool or if refill and weighing settings have to be established again. Include total changeover time, material discarded and the independent product clearance check in the trial if this duty was part of the buying decision.
Check that the weighing frame is supported, free from contact and protected from major vibrating loads before running material. Set connection alignment using the detailed supplier drawing. Verify flexures or supports, boot clearance and utility connection lengths over the full intended movement. Ask the site team to inspect whether guards, stairs or extraction ducts have introduced a fixed load path. Build an approved handling plan for tooling and hoppers that are removed during changeover. Where gravity discharge feeds a pressurized receiving vessel, verify the intended pressure interface with the actual process equipment installed and operating.
A factory trial can use representative samples with known handling history and a separate reference scale to establish whether the proposed geometry is credible. Run at the smallest and largest recipe setpoints and an intermediate case. Include repeat runs and at least several production-like refills across the relevant conditions under an agreed procedure. At the site, repeat the most important cases with the production inlet, dust extraction and downstream receiver in service. Use a reference receiver or independently weighed production flow where possible, and report any fallback method if the running line cannot accept a catch. Confirm that the correct event and timestamp are logged when material runs low or the refill does not complete.
In troubleshooting, collect the weight slope, rate setpoint, drive signal, actual speed, refill timing and downstream status together. A drive command climbing while indicated delivery falls can be consistent with bridging or starved screws. A repeating discrepancy synchronized with periodic agitation or nearby extraction can suggest an interfering force. Apparent delivery continuing after the drive has stopped may be caused by lingering discharge, a weight disturbance or the controller's smoothing period. Obtain material observations, rather than making adjustments from an isolated trend. An independent collected mass helps distinguish a problem in measurement from an actual flow failure.
Preventive maintenance should cover screw and sleeve condition, throat deposits, scale restraint and fasteners, inlet valve seals, outlet interfaces and any agitator or vibration aid. Keep replacement tools identified with their feed trial data. A change in material-contact geometry or venting can affect carryover, feed factor and cleaning even when the assembly fits. Repeat appropriate calibration and feed tests after relevant maintenance. Retain reference weights and the instruction for applying them safely with the equipment stopped and isolated. Obtain current control backups and approved settings transfer procedures so maintenance can restore a known recipe without guessing from handwritten notes.
Close the acceptance file with the approved operating bounds, source of reference mass measurements, curves and event records from the actual installed unit. Include spare tools or seals by material and duty, safe isolation and cleaning instructions, electrical and pneumatic diagrams, and the specific conformity evidence required for the project jurisdiction. Define the response to an out-of-range demand, loss of scale signal or an empty hopper. These are process and contract decisions for the responsible team. An accepted feeder should have a traceable effect on the product, with enough retained data for operators to relate observed quality deviations to the ingredient and time they occurred.
FAQ
Why is it called loss-in-weight feeding?
The controller estimates discharge from the decrease in the weight of the feeding assembly over time. During ordinary delivery the inlet is closed, so falling weight points to material leaving through the discharge. The output rate is adjusted to track the recipe. A separate collection on a reference scale checks actual delivery.
What happens while the hopper is refilling?
The input mass obscures normal discharge measurement. The feeder typically uses a held volumetric setting or a model-based control estimate while it is filling and settling. Normal feedback returns once the weighing signal is usable again. Catch and weigh the output through the entire event to test whether the recipe stays within tolerance.
When is a twin screw a candidate?
A twin screw can be considered for powders that bridge or flow poorly and for some fibers or irregular solids. Tooling, hopper flow, torque and loss through refill still need a test with representative material. The product name alone does not select a screw set. Ask the trial technician to document the pitch and tool profile.
Is feed range the same for powders and pellets?
The discharge device moves volume, and the mass carried depends on bulk density, filling, cohesion and equipment speed. The mass range demonstrated on one sample should only be applied to another ingredient after the vendor evaluates the different material. Record bulk density and moisture on the sample used for each trial, along with the tooling.
How should I ask for dosing accuracy?
Name the time window or batch mass, setpoint and test conditions. Require both collection repeatability and deviation against independently weighed material. Include refill and the recovery period as well as a settled run. Specify the smallest collection needed and check that the calibrated reference scale can resolve it with enough confidence for acceptance.
Can weight readings be disturbed by the surrounding plant?
Yes. Rigid piping, flexible connections under load, pressure differences, cables or local vibration can affect the scale. Check the installed equipment and compare the weight trace with independent catch samples and relevant plant events. A trial with the actual extraction system running helps reveal an offset that would be absent on a quiet test bench.
What is the practical difference from a belt weigh feeder?
A loss-in-weight feeder weighs the assembly as it empties. A belt-based weigh feeder senses the burden on a moving belt and tracks belt speed. Compare them using the same material, rates, acceptable delivery variation and site layout. State any small recipe amounts or handling constraints that matter to the lowest required feed rate.