A jig concentrator is a wet gravity separator that repeatedly lifts and settles a bed of particles with a pulse of water. During many cycles, particles tend to stratify. Relatively dense grains travel toward the lower bed and lighter grains toward the upper bed. A discharge system draws off the separated layers as the feed moves through the machine. Wet jigs are used to clean coal, upgrade selected ores and recover metal from crushed slag or other recycling feeds.
The machine is a tank divided into one or more duties, with a perforated support for the bed, a controlled source of pulsation and a way to discharge the heavy fraction. The value of a purchase depends on how evenly the bed forms across the working width and how consistently the discharge follows the separation. Feed variability, water quality and the size distribution are design conditions.
A jig selection should connect particle liberation and density contrast to test results, an agreed deck loading, water and air demand, and product sampling. The test should show both the material recovered and the contamination left in that product.
Chapter 1 / 06
What a Wet Jig Separates
A jig's separation starts by delivering a reasonably uniform bed across the working width. Water movement then changes how strongly the grains touch and bear on each other. Through many cycles, particles change positions as the bed loosens and settles. Density matters, but particle size, shape and how the grains interlock matter as well. A coarse light particle may settle competitively with a fine heavy one. This is why feeds that seem to have an excellent pure-mineral density contrast can still make a poor separation once particle sizes and liberation are taken into account. A sample sent to the vendor should reproduce the size distribution and particle shapes the jig will actually see.
The upper stream is called lights or floats and the lower stream heavies or sinks. A coal operator may sell the lower-ash light product and discard the rock-rich heavies. An iron or manganese operation may want to recover the heavy product. In slag recovery the heavies may contain valuable alloy, with the light mineral stream used or disposed of separately if its qualities permit. Define the desired product and acceptable losses in the contract. Reporting a mass split alone cannot show that the commercial product makes grade, and a high assay can mask a low recovery if the jig sends good particles to waste.
Control the feed size ahead of the machine. A jaw crusher or gyratory crusher can carry primary duties where needed. A secondary cone crusher may prepare a narrower range below the primary stage. A vibrating screen or a trommel screen can split the feed into size classes before gravity separation. Each part of the upstream arrangement has its own efficiency and wear. Even a jig that runs well at its design feed can become unstable when worn screening media admit oversize or the fine fraction changes after a crusher adjustment.
Selection starts with the composite particles the plant receives. Mineral associations, particle shape and moisture can change within a quarry bench or recycled product stream. High clay content can foul the bed or raise the density and viscosity of recirculated water. A washing or cleaning step can help where material can be dispersed, while some breakage creates more fines for the downstream water system. A pilot program should record how much feed each preparation stage removes and how those streams are treated. Report the jig's own recovery and the cumulative recovery from raw feed. The two measures expose a circuit that loses a valuable fraction before the jig has a chance to separate it.
Feed duty
Usually valued stream
Results to document
Coal
Light fraction
Product ash, yield and combustible recovery at matched feed conditions
Iron or manganese ore
Heavy fraction
Grade, recovery, mass yield and selected impurity assays by size band
Alloy-bearing slag
Dense liberated metal
Metal recovery and concentrate purity, including losses in fine and coarse residues
Aggregates and recycling
Duty dependent
Named impurity, specific contamination limit and mass reporting to each product
A wet jig occupies a particular place in the preparation circuit. A spiral concentrator uses density and size effects in a continuous flowing film. A flotation cell relies on differences in surface behavior. A magnetic separator can clean or recover a magnetic fraction on the basis of magnetic response. With suitable dry feed an eddy current separator recovers conductive materials using a separate principle. These processes can serve other fractions in the same operation. Use feed tests and a flowsheet mass balance to find which one is appropriate at each position.
Chapter 2 / 06
How Pulsation, Stratification and Discharge Work
The working deck holds a bed of feed solids above a water chamber. A brief upward water movement opens spaces between grains and lets them move relative to one another. The changing flow and the subsequent return movement let the bed settle and consolidate. The sequence repeats while incoming feed displaces material along the deck. Different grains may separate by settling and by moving through openings among other particles, depending on the stage of the cycle and the duty. The interaction is repeated and cumulative. A single water stroke is not a scale reading of every grain and the discharge partition is a probabilistic result.
The pulse is described by frequency, amplitude and shape. Water displacement or velocity over time gives a useful picture of what the bed sees. A pair of settings with the same frequency can produce different bed behavior if the valves, air pressure or chamber water level change. More aggressive pulsation can open a tight heavy bed, but excess disturbance can remix layers or move small heavy grains with the upper flow. Insufficient pulsation can leave a packed region through which particles have poor access. Request observable process variables and a response to feed variation that a technician can verify independently of a displayed setpoint.
An under-bed air-pulsed jig admits and releases air from chambers arranged below the separating bed. The resulting movement of water through the deck pulses the solids. Side-pulsed layouts deliver the movement from a chamber at the side and need an effective arrangement for transmitting it across the machine. Plunger and diaphragm designs move water by mechanical displacement. Mechanical and air arrangements differ in valve hardware, moving seals, distribution and utility load. The APIC product brochure describes an under-bed air-pulsed machine with a controller that can display water and air pressure and an estimated pulse waveform by compartment [3]. Require the vendor to identify which sensors and displays are included in the offered package.
The working water carried with the feed and products is separate from the motion that lifts the bed. Air can provide the energy for pulsation while a separate water supply maintains the chamber and circuit balance. An air demand at the machine must account for transient supply at the pulse valves, any level control demand and the condition of the air assumed by the supplier. Water added to maintain bed behavior may leave as product moisture or a water treatment bleed. Define which demand is instantaneous and which is average. Compressors and service water pumps can be undersized when plant utilities are scheduled only against shift averages.
The heavy fraction settles below the light layer and must be withdrawn fast enough to maintain a useful bed. The control system can infer bed state from pressure, density indications or level sensing, depending on design. A gate, discharge device or compartment arrangement then meters heavy product. The measured height or resistance is a control signal. Validate its relation to product quality on representative feed before accepting it as a process report. A gate that opens too little can allow a heavy bed to build until it interferes with the lighter stream. Opening too far may lower the interface and rob the product stream of material that should stay above it.
Variable
What it changes
Evidence to ask for
Pulse frequency
Number of stratification cycles during residence on the deck
Recorded cycle timing at the relevant loaded conditions
Pulse displacement and shape
Degree and duration of loosening and resettling
Water movement trace, air pressure trace and effective adjustment range
Feed spread
Consistency of bed thickness across the working width
Feed distributor drawing and loaded observations at representative rates
Bed discharge
Heavy layer depth and routing of material around the interface
Sensor and gate trends, stability at variable background heavies loading
Input and outlet flow balance at each tested operating case
The light stream often travels with the upper forward flow over a weir. Some designs recover heavy material through the deck and others use an end or side outlet for a stratified layer. Certain fine-particle jigs use a prepared bed of coarser material to influence how certain particles pass to the lower collection section. Such internals change the meaning of a bed or aperture setting. Ask which particles the deck retains, which ones can pass, and what happens if the machine receives oversize or sticky material. A replacement deck panel should meet the same hydraulic and mechanical specification as the original tested deck.
Chapter 3 / 06
Pulse Drives, Compartments and Feed Duties
A single compartment can make a two-product separation where feed is reasonably consistent and the test shows that enough stratification occurs in one duty. Multiple compartments can allow a different pulse or discharge arrangement along the path. Some units recombine selected streams. Others take an intermediate grade as middlings for retreatment. Establish how each compartment adds value using assays and flow balances. Adding length or another chamber changes water distribution, access and field maintenance. A vendor arrangement that fits an existing pit may require tradeoffs in gate removability or product chute elevations, and those tradeoffs should be resolved against the complete drawing.
Working width and bed length influence throughput, but feed distribution across width and the time the solids spend in the bath influence quality. A wide machine with feed concentrated in a center channel cannot effectively use its outer deck. On start-up or when feed surges, a high local loading may stay unstable even if the overall feed meter reads within range. Test at the width load relevant to the quoted machine. On a wide bank ask how the inlet splitter, weirs or feed distributor are set up and how one part of the deck can be inspected. At low rates the control arrangement still needs enough bed for meaningful measurement and discharge.
Coal duties often focus on ash reduction subject to combustible loss and plant yield targets. A shifted size distribution or a different seam can move the operating compromise. Ore duties may need improved grade ahead of grinding as well as high valuable-mineral recovery. Liberation at the intended size remains the deciding factor. A high-pressure grinding roll can generate a different mix of particle sizes and shapes than conventional crushing. A hammer mill used on suitable brittle feed may open valuable material but also make excess fine solids. Check the actual preparation route and its production-size samples before choosing an equipment guarantee.
Slag and recycling duties introduce unusual shapes, tramp pieces and intermittent dense material. The useful test should include representative metal geometry and age or weathering of the slag. A jig that discharges a consistent fine ore bed may need a different heavy-product outlet for unusually coarse, dense particles. Metal grade alone is not a complete measure if the concentrate still needs a magnetic or screening stage. If additional liberation is needed after separation, downstream SAG mill or ball mill duties may depend on the mass and size routed to them. Budget the comminution and water demand for the selected circuit rather than assuming the jig replaces every downstream operation.
Wet coarse or fine duties with a controlled air chamber below the deck
How is pulse uniformity shown at the loaded full working width?
Side air chamber
Layout suited to the supplier's side transmission geometry
What distribution is demonstrated at the far side of the deck?
Mechanical plunger or diaphragm
Duties where mechanical water displacement suits the selected size and layout
What seals, moving assemblies and access are needed at expected duty hours?
Single deck compartment
A clean two-stream split proven over the feed envelope
Will the tested residence and discharge capacity carry all feed cases?
Staged compartments or bath train
Staged cleaning, retreatment or middlings handling with defined duties
What does each outlet produce and where do recycles report?
Wet gravity separation can be attractive when the density contrast is clear and water can be recycled. It becomes harder when valuable material is too fine for the chosen jig geometry, the feed has a broad size spread, or composites have densities close to the reject. A dense-medium circuit creates its partition in a deliberately weighted liquid suspension and often merits an evaluation on difficult feeds. Compare process routes at matched grade and recovery. Include any medium system, air demand, water recovery and maintenance hours. Electricity or fresh-water totals from a brochure are only comparable if both vendors use the same product specification and plant boundary.
Chapter 4 / 06
Key Specifications and Published Examples
Define a hydraulic guarantee alongside the solids guarantee. Feed water may arrive as surface moisture on crushed particles, slurry water from the upstream screening plant or separate dilution at the feed box. The procurement data sheet should give these streams different rows. Ask which flows the quote assumes are measured and which are estimated. A recycle pump may be selected for high circulation with little fresh-water consumption, provided the recovered-water quality is acceptable. Model the water retained in both products, losses to sludge treatment and interruptions in return flow. A running bleed may be necessary to maintain water quality even if the circuit has enough volume to operate without fresh makeup for short periods.
Published throughput gives a family envelope. allmineral lists 1 to 700 t/h per unit and a 0.1 to 150 mm particle size range for the alljig wet family [1]. TAKRAF lists APIC jig widths from 0.5 to 6 m, with 15 to 600 t/h for coal and light minerals, 15 to 300 t/h for heavy minerals, and 10 to 120 t/h for metal recovery per jig [2]. These are the manufacturers' stated envelopes for their product lines. They do not imply that every unit covers all rates or that the entire size range can be processed at the highest listed rate. Put any quoted values against the actual offered configuration and feed.
Specification
What to state
Why a buyer needs it
Capacity
Minimum, normal and maximum dry solids rates with conditions for each
Prevents wet feed or family throughput being mistaken for guaranteed sizing
Particle size distribution
Upper and lower design fractions plus oversize, fines and moisture
Defines the size-dependent separation and hydraulic loading
Working deck
Effective width and length, aperture geometry, compartment count and access
Shows usable separation area and allows maintenance planning
Feed density distribution
Washability or density fractions and assays by size
Shows the recoverable value and the sensitivity to feed variation
Product requirement
Recovery, grade, yield or specific impurity caps, with stream destinations
Fixes the acceptance point and exposes unsuitable tradeoffs
Water and air
Average and peak demand, pressure, carryover and reuse properties
Sizes pumps, air supply, receivers and treatment equipment
Pulse and bed control
Measured variables, actuators, logging and approved operating envelope
Lets operators trace unstable product to feed, utility or discharge changes
Availability and wear
Deck and gate material, replacement criteria and outage scope
Defines maintainability of the agreed machine and layout
Washability and sink-float results can give an idealized picture of how product grade and yield change with density. A water jig has real separation error and a size-dependent response. Ask whether the bidder measured a partition curve or directly compared products by density and size, especially if the project uses a design cut in the process model. An overall mass split can look correct while fine heavy grains leave with the lights and coarse light grains contaminate the sinks. When the gate control reports a density-equivalent value, specify how that value will be compared with physical product measurements. A reading that is useful for control still needs calibration and an operating context.
Sampling has to follow both streams and the feed on a common basis. Choose sufficient sample mass and duration for the variability and top size. The test should sample during a documented run at stable feed and utilities. Track mass recovery, sample moisture and assay repeatability. Take additional samples during known transitions if the plant routinely shifts material grades or restarts after brief interruptions. Close the mass balance before interpreting an attractive result from one stream. If reporting a target near a detection limit, define how assay confidence and missing or below-limit values will be treated during acceptance.
Document air quality as well as quantity. Valves and control gear have their own acceptable moisture, contamination and supply pressure limits. The air train can include delivery piping, local buffer volume and isolation appropriate to the offered design. Confirm whether a low pressure large volume pulse duty uses dedicated equipment and how the normal services share supply during a disturbance. Water records should distinguish makeup flow from circulating flow and include fines, temperature or contaminants that affect operation. If a plant has restricted fresh water, the guaranteed performance test should use recovered water with representative quality after the circuit has reached stable conditions.
Weight and civil loading should include the filled machine, supported accessories, operating fluctuations and handling loads. Give the building designer reaction points and acceptable support tolerances, not just the empty shipping weight. The supplier should identify critical deck alignment and stiff support conditions. Request the type and range of local indicators and alarms along with the plant control interfaces. If the control package supports automatic discharge, verify the behavior when the sensor signal is lost or the discharge path has limited capacity. Agree on which abnormal responses will be tested during commissioning without interfering with the site's safety procedures.
Chapter 5 / 06
Selection, Circuit Boundaries and RFQ
A staged test program can start with repeatable batch screening of candidate feeds, then use a continuous campaign if distribution, product handling and sustained loading are uncertain. Capture enough of each feed lot to repeat the original analysis after testwork. Ask the supplier to provide the preparation method, test deck, pulse method and discharge conditions. When results are scaled from a narrow test vessel to a wide plant unit, the scale-up statement should explain how residence, bed load and transverse uniformity are kept comparable. Separate any assumed values from those measured during trials, especially near the fines limit and for the least clean feed blend. An agreement on a repeat test under representative production conditions has practical value when the first data come from hand-selected samples.
An upstream stacker reclaimer can support blended delivery if the feed source and stockyard permit it. A coarse feed apron feeder may smooth intermittent reclaim, and a belt conveyor provides a measured solids delivery path. Record expected feed excursions at a time scale that matters to bed control. A steady shift average cannot establish that a feed surge spends enough time in stratification. The wet distributor and any feed box belong in the RFQ if they affect spreading. Attach the feed trajectory and elevations, and ask the bidder where its load guarantee begins.
Wet recirculation can include a slurry pump sized for solids abrasion and the plant's head requirement. A hydrocyclone in desliming performs a wet classification duty distinct from the jig. The general cyclone separator reference describes the family distinction. A gravity thickener or a clarifier can support water balance when settling tests and site layout allow it. A rotary drum thickener is an option for some separate sludge duties. Draw the circuit with the actual destinations of rinse, fine solids, recovered water and unavoidable bleeds so that operating water quality can be assessed.
Downstream treatment can include dewatering and drying to a handling specification. A vacuum belt filter, rotary vacuum filter or filter press may treat a suitable fine slurry generated elsewhere in the water or product circuit. Verify filtration from actual samples and connect filtrate quality with water reuse. For suitable dewatered solids, a screw conveyor or bucket elevator can handle the transfer where the moisture and particle behavior suit it. Their capacities should use the real bulk condition at the intended discharge, including wet sticky material or short periods of high heavy-product load.
An existing plant can narrow a test by isolating what changed. Compare the earlier feed size and water quality against samples from the current circuit before accepting a replacement jig as the cure for declining product. If screenings deliver excess slimes, correcting the upstream aperture or washing scheme may be necessary to recover stable bed control. If the constraint is equipment width or heavy-stream gate capacity, request defined performance at the available building and utility limits. Model how a bypass or alternative arrangement routes feed while one compartment is offline, especially when the following separation plant is built for steady feed.
Inquiry input
Attach to the RFQ
Require in the quote
Feed
Ore or waste type, assay, size and density distributions, samples and variability
Test program and design feed window
Product
Named sinks and lights, target grade, recovery and reject restrictions
Guarantee at normal, high and difficult feed cases
Utilities
Air and process water available, recovered-water quality and drainage limits
Average and peak loads and all owner-supplied services
Mechanical
Site layout, supports, incoming feed, outlet elevations and handling access
Equipment envelope, loads, deck modules and withdrawal routes
Control
Automatic discharge expectations, available interfaces and data retention
Sensors, alarms, history, permissives and operating responsibilities
Use RFQ wording that identifies the dry solids rate, feed size distribution, material density, target sinks and floats performance, and whether the machine will be installed indoors or outdoors. State whether wet feed arrives directly, and make operating water quality and recovery responsibilities explicit. Specify the level of automatic discharge control expected and how it will be tested. If a dense-medium option is also being assessed, give both bidders the same commercial product and recovery targets. Request installed and operating requirements on a common battery limit so the comparison includes air, returns, fine solids disposal and ancillary equipment.
Chapter 6 / 06
Installation, Acceptance and Troubleshooting
Make sample cleaning and transport part of the acceptance plan. Collect the two product streams so drained water or slimes cannot change a grab sample's apparent mass or grade before measurement. Identify whether the reported loss follows dry solids at the jig outlet or downstream after product rinsing or dewatering. If a dense product has isolated large pieces, sample those as specified by the sampling plan and keep the retained oversize identified. The work should distinguish a genuinely poor separation from a sampling method that consistently misses the coarse heavies or washes fines out of one sample. A reconciled dry-solids balance with separately reported moisture gives the plant a baseline that can be repeated when performance degrades.
Mechanical acceptance starts with an as-built deck and chamber drawing and field verification against the vendor tolerances. Confirm that the feed chute spreads material across the effective width, and that product outlets remain free to drain at peak demand. Water retained during a stoppage or a filled sump can add static load or affect access. An approved plan is needed for isolation, drainage, lifting, entry and restart. Access for inspecting a submerged deck should be established before the machine is placed under pipes and structural members. Replacement of a blocked or worn panel should not require dismantling unrelated production equipment if the design offers a more direct route.
Instrument checks include water and air pressure references, communication with upstream feed devices and downstream product handling, and correct gate indication across its range. Prove the control logic according to the agreed functional tests, using the vendor and site work procedures. The loaded trial should use controlled production samples with consistent test boundaries and verify both steady grade and condition changes the operation expects to see. An unscheduled event that disrupts feed during a trial must be recorded in the signed test record so the acceptance team can identify retest conditions instead of silently excluding a period that affects overall output.
Unstable separation often has several observable causes. One section of the deck that carries a deeper bed can indicate poor feed spread, a different pulse shape or a partial blockage. Heavy material in the upper stream can be due to poor liberation, peak feed load or insufficient heavy-product removal. A marked deterioration soon after a water reuse change can arise from altered suspended solids. Gather feed and product samples, log chamber pressures and discharge indicators, and compare the feed size and assay with the last stable baseline. A single reading of air pressure or a single product sample rarely isolates the cause.
Automatic discharge is useful only if wear and control behavior are kept visible. Inspect gate sealing faces and deck apertures during approved outages. Log the materials fitted and whether wear is uniform across compartments. As valve response or sensor calibration drifts, the same indicated pulse or bed value may become associated with different product behavior. Check the cause against a physical observation or independent sample before changing process targets. Maintenance notes should say what mechanism was found and what part was restored. Over time that record can guide inspection and spare choices for the actual site duty.
For final turnover, obtain maintenance and operations documents, wiring and control descriptions, instrumentation records and the components needed to repeat the acceptance sample campaign. Governing legal requirements depend on where the machine is supplied and how the process, compressed air, water and electrical systems are classified. Have the vendor state the applicable machinery requirements and limitations of its supply. The owner should identify the standards and safeguards it will implement for wet access, isolation of stored water and compressed air, moving material and cleaning. Keep the purchased jig's process proof beside the mechanical and safety documentation so both the measured separation and the conditions supporting it can be maintained.
FAQ
What is the difference between the light and heavy streams?
The light stream leaves the upper layer with more of the lower-density particles. The heavy stream leaves the lower bed with more of the denser particles. The value of a stream depends on the duty. Coal typically values the lights, while metal recovery from slag often values the heavies. Sample both outlets to calculate recovery.
Why does a jig use pulsating water?
Cyclic water movement opens and settles the particle bed repeatedly. The grains can migrate between layers over successive cycles. Air chambers or a mechanical actuator can supply the movement. The pulse shape affects whether the bed is adequately loosened and how stable its layers are. Evaluate loaded operation across the working width.
Can one jig take every size range shown in a catalogue?
A catalogue range describes the scope of a machine family. Confirm feed size bands, the size distribution, the rate, and the separation recovery for the actual offered deck and discharge arrangement. Wider size mixtures and fine slimes can change the result. Ask which size and rate combinations were tested on comparable material.
What does automatic heavy-product discharge control?
It meters removal of the lower layer to keep a useful separating bed. A controller can use a level, density or pressure-related signal together with an adjustable gate or other discharge device. Verify the relationship between that signal and the measured product before relying on it. Check operation when the proportion of heavies changes.
What are the main water and air specifications?
Request average and peak water demand, recovered-water quality and the expected water balance around the products. For an air-pulsed jig obtain average and transient air requirements, supply conditions at the machine and the allowable pressure variation while other users share the supply. Identify the specified utility measurement point and reference conditions for each pressure.
Does a high-density difference guarantee a good separation?
Liberation, grain shape, feed size and how the machine is operated also matter. A coarse light particle and a fine heavy particle can have similar settling behavior. Use a sample from the proposed preparation circuit and require results by relevant size fraction. Include material near the bottom of the specified feed size range.
How is a jig acceptance run scored?
Measure dry feed rate, both product flows, product assays and relevant size and density fractions with stable recorded air and water conditions. Reconcile the mass balance. Compare grade and recovery with the agreed case and document any interruptions and retest rules. Use those same measurements to establish a baseline for future plant checks.