A dense medium cyclone is a wet gravity separator that divides crushed and screened solids by particle density. The feed enters with a heavy suspension of fine magnetite or ferrosilicon in water. Inside the cyclone, the rotating flow tends to send denser particles toward the wall and out of the bottom spigot, while less dense particles tend to leave through the central overflow. Plants call these products sinks and floats. Both streams leave as a mixture of solids and medium.
The useful separation is measured on the actual feed, at an agreed size range and density cut. Start a purchase with the washability of that feed, the product grades and recovery the plant needs, and the capacity of the medium and drain-and-rinse circuit. Those inputs determine whether the vessel can deliver its promise after it is connected to the rest of the plant.
Sawmill dust cyclone with tangential entry and a tapered body. Context photo: Encik Tekateki, CC BY 4.0 via Wikimedia Commons.
A credible offer links cyclone diameter and outlet geometry to an inlet head, a measured slurry flow and a specific solids feed. It also explains how recycled medium, contamination and wear will affect the density split over a shift and between changeouts.
Chapter 1 / 06
What a Dense Medium Cyclone Does
The solids entering a dense medium cyclone have already been prepared for separation. A jaw crusher or gyratory crusher may break run-of-mine lumps ahead of a secondary cone crusher. A vibrating screen then defines the size fraction assigned to the cyclone. The crusher choice belongs to the liberation study. Recovering valuable material in a coarser fraction can reduce the tonnage sent to grinding, but only if valuable particles have a density contrast at that size and are sufficiently liberated. Excessive breakage can move clean material out of the cyclone feed and increase the burden on the fine circuit.
The words floats and sinks describe the streams at the separation stage. In coal cleaning the lights can be the saleable product and the heavy fraction the reject. In diamond preconcentration the heavies are the stream that goes forward for further recovery. An iron ore duty may also value the heavy stream, subject to mineralogy and the association of impurities. It is poor practice to label the two outlets automatically as concentrate and waste in the flow sheet. Use the material names for each duty and define what the sample labeling system calls each stream, including any middlings or recirculation streams.
The solid's density is a property of the particle entering the cyclone, including any locked combination of minerals. The density of a pure mineral is therefore only a starting point. A composite grain can have an intermediate density and report to either outlet near the transition. A porous particle may behave differently when wetted. A feed description that names only the mineral and a maximum fragment size gives the vendor little basis for a recovery guarantee. Supply assay and distribution by size and density, representative moisture and expected contamination. State whether the quoted tonnes are dry solids per hour or wet feed received at the belt.
A familiar drawing can obscure the mechanical boundary. The vessel resembles a cyclone separator in outline. Its job depends on the controlled heavy-liquid suspension and on the density partition of the feed solids. A wet sizing cyclone or a gas-solid collector has different duties and design criteria. A spiral concentrator uses a flowing film of slurry. A flotation cell depends on surface behavior. These routes may treat fractions outside the dense medium circuit after testwork. An eddy current separator may recover conductive metal in a dry recycling stage, which is again a different mechanism.
Assignment
Physical separation
What the circuit should report
Coal cleaning
Remove denser stone and other heavy material from the selected coal size fraction
Dry clean-coal yield, product ash and combustible loss to reject
Diamond preconcentration
Collect a small dense fraction for downstream recovery operations
Concentrate mass pull, reconciled tracer response and checks on loss to floats
Iron ore preconcentration
Reject gangue where feed mineralogy gives a workable density split
Iron recovery and grade for each agreed size fraction and feed condition
Retrofit in a running DMS plant
Recover the intended density partition at required solids loading
Before-and-after partition curves, wear state and medium balance on comparable feeds
Economic separation can favor a smaller or a larger mass pull depending on what the stream costs to process next. Rejecting a tonne of gangue ahead of a SAG mill saves the downstream work on that material. Sending an additional tonne into a small final recovery plant can consume capacity needed by richer feed. Set both a minimum valuable-material recovery and the permitted mass or grade sent forward. A good technical comparison uses the total outcome of the separation and downstream route, with both products sampled. Comparing only one shipment grade can reward a unit that quietly loses the value the plant was built to recover.
Chapter 2 / 06
How the Cyclone and Medium Circuit Work
An inlet directs the pressurized slurry into the cylindrical section and sets up rotation. A cone leads to the spigot, where the outer, downward-flowing suspension leaves as underflow. A tube called the vortex finder extends into the upper section and collects the inner upward flow as overflow. The two movement paths are sensitive to pressure, outlet restriction and internal wear. An air core can be present under normal operation, and the factory geometry is developed around a particular flow regime. This geometry explains why running at a convenient pump pressure or choosing a flange-compatible spigot can have a process consequence even when both product launders still contain slurry.
Correct medium is prepared and held at a controlled density in the circulating system. Mixed feed can be delivered by a slurry pump, or the layout may establish inlet head by elevation. A belt feeder can meter screened solids into a controlled feed box. A buyer needs to know where the vendor's operating pressure is referenced, the elevation of that point, and the density assumed when a pressure is expressed as an equivalent liquid head. A pump discharge reading upstream of fittings and a long feed line gives a different value from the pressure at the cyclone inlet. The hydraulic calculation has to connect the two.
Medium tends to classify inside the unit along with the coarser process solids. Underflow medium can be denser than overflow medium. The feed medium density on the plant display and the particle density at which half the particles go to each product are distinct measurements. Their difference is often tracked as an offset. Its size and consistency depend on the geometry, medium properties and the condition of the feed. A change in offset can signal that the relationship between the densitometer and actual separation has drifted. Recording both quantities makes it possible to investigate before an operator keeps moving the medium setpoint to catch a product assay.
Both products normally go onto drain-and-rinse screens. On the drain section, relatively undiluted medium passes through the deck and returns to the correct-medium circuit. Wash water in the rinse section removes more adhering medium. That resulting dilute medium is collected separately and sent to a magnetic separator suited to recovering the magnetite or ferrosilicon. Regenerated medium goes back to the circuit at the appropriate stage. Water and nonmagnetic contaminants have their own exits or treatment loops. Define where water enters and where it leaves. Simply recycling every filtrate can return fine contaminants that change medium behavior even while magnetic solids keep circulating.
The quantity of medium relative to the solids matters because both the flow field and the separation have to accommodate that particle load. The Multotec operating paper describes typical medium-to-coal ratios of about 3.5:1 to 4.5:1 for the coal duties it discusses [2]. It frames sizing in terms of slurry flow and solids feed and describes the effect on separation when higher coal tonnage reduces the ratio. Obtain the supplier's exact ratio definition and units, since plant reports may express solids and medium on different bases. The cited band is a coal example. A new ore or a different size fraction demands an independently justified basis.
Circuit point
Return or outlet
Data to put on the flow sheet
Correct-medium feed
Dense suspension supplied to mixing and cyclone feed
Density, flow, young and aged medium assumptions, measurement location
Drain section
Undiluted or relatively concentrated medium goes back to the correct circuit
Wash-water rate and quality, spray pressure basis, drainage separation
Magnetic recovery
Recovered medium returned, fine contamination and water managed separately
Medium grade, stage recovery assumptions, plant top-up and discharge balance
Product transfer
Dewatered solids to stockpile, disposal or next treatment
Residual moisture, adhering medium, chute elevation and design flow
Fine streams outside the cyclone can still limit the separation. A gravity thickener may handle fine suspended solids where settling tests support it. A rotary drum thickener or clarifier belongs to a site-specific water or sludge scheme with its own feed requirements. Decide how clarified or filtered water affects rinse sprays and the density balance before connecting recycle points. Recycled water flow alone is an incomplete utility description. Suspended nonmagnetic fines can accumulate if the water-treatment route and the medium-cleaning route are evaluated separately.
Chapter 3 / 06
Geometry, Wear Protection and Circuit Types
Catalogue diameter usually refers to a nominal separation chamber size. Ask for actual wetted dimensions and the configuration that produced the vendor's results. A coating or thick lining changes dimensions when fitted, and a part carrying the same family name can have a different throat. Diameter affects residence and capacity, but a scalable family still has a feed size window, geometry set and head range. Several parallel cyclones can give capacity and maintenance flexibility if the feed is split evenly. One large unit can reduce the count of isolation and splitter points. Compare both arrangements with the same feed solids and upstream availability.
The inlet profile establishes rotation and affects how particles arrive near the overflow tube. Multotec lists cast-iron and ceramic-lined families and describes a scrolled evolute head and engineered tiles [1]. Its statements about head or wear improvements belong to its own designs and conditions. A purchasing drawing should identify the feed shape and area, whether a transition piece is supplied, and any handedness or orientation constraints. Any vendor-specific statement about reduced pressure, higher capacity or longer life needs a reference geometry and comparable feed before it has practical value in the bid evaluation.
The vortex finder sets the boundary of the overflow path. Its bore and insertion depth affect the split between outlets and the risk that feed travels directly into the overflow without the expected separation. The spigot controls the underflow opening and must pass the heavy fraction and its share of medium. Test both outlet configurations together. If higher-density material forms a much larger proportion of the feed than assumed, an undersized apex can be overloaded while total feed tonnage appears comfortably within nameplate. Coarse fragments, worn geometry and outlet backpressure can further change product partition. For critical cases request a vendor check at the worst credible sinks mass and top size.
Cast alloy parts, lined shells and individual wear inserts offer different service strategies. High-wear areas can include the feed entry, the vortex finder, the cone transition and the spigot. Compare repair time, spare inventory needs and liner installation practices as well as material selection. A zoned assembly can allow localized replacement if the part can be removed with the surrounding spool in place. A large one-piece lower section can avoid a joint in the wear path but may require a different lifting plan. Ask for a section drawing that indicates material and replacement boundaries on each wetted surface, including parts that the vendor expects the plant to furnish.
Geometry or arrangement
What it governs
What to demand from the bidder
Body diameter and cone profile
Flow capacity, solids size envelope and the residence available for separation
As-lined drawing, approved size fractions and design feed envelope
Feed head and entry profile
Vortex formation and energy needed to handle the selected slurry flow
Pressure reference point, line-loss basis, flow curve and inlet drawing
Vortex finder
Overflow geometry, bypass tendency and medium split
Insertion depth, as-new bore and replacement limit
Spigot or apex
Underflow capacity, blockage sensitivity and outlet partition
Opening range, expected sinks load, spare options and wear checkpoints
Parallel bank
Installed capacity and turndown with one module isolated
Splitter performance, dead-leg provisions and operating cases
Two-stage circuit
Recovery of middlings or production of more than two streams
Stage-by-stage performance, full recycle balance and test evidence
A single duty normally delivers two streams. A two-stage arrangement can process a selected first-stage fraction at a different cut to make a middlings stream or recover material from one side of the first split. Identify whether the second stage shares the same medium sump. Different cut densities can require separate medium control, and recycled middlings increase the circulating solids load. Define the basis for stating stages on the proposal. Two identical machines in parallel are one separation step in hydraulic parallel. Two consecutive separation steps have separate product and efficiency consequences.
At a mineral operation, alternate crushing and grinding routes can change the amount of feed that remains above the lower size limit. A high-pressure grinding roll used upstream can have a different output size and shape distribution from a cone circuit. A ball mill typically serves duties where further liberation is needed and may receive a separated product downstream. A trommel screen may handle early wet scalping or classification where appropriate. Use the resulting measured distributions to establish the cyclone's actual duty instead of assuming that similar throughput from different upstream trains produces interchangeable feeds.
Chapter 4 / 06
Key Specifications and Performance Measures
Washability describes the attainable grade and yield when a sampled feed is separated by density under controlled conditions. The useful report includes mass and assay of the density fractions by size. Near-density material is the fraction within a stated band near the proposed separation density. A wide band gives a different reported near-density percentage from a narrow band, so always state it. When a large part of the feed sits close to the cut, a small shift in cut or a loss of operating sharpness can change product grade significantly. A broad feed distribution may need separate coarse and fine partition data so a convenient average cannot hide weak separation at the lower limit.
A partition curve plots the measured fraction of each density class reporting to one specified outlet. In a sinks curve this fraction generally rises with density. The half-partition density is often called d50 or the cut density. Keep its meaning separate from the particle-size d50 used in sizing duties. A commonly reported sharpness measure is probable error, Ep, defined as half the difference between the densities at 75 and 25 percent partition on the ascending curve. When the curve is smooth and the sample meaningful, a smaller Ep generally indicates a sharper cut. Always provide mass balance and sampling uncertainty with the result. The Multotec operating paper illustrates these concepts and the cost of losing efficiency near the cut [2].
Parameter
How to state it
Reason it belongs in the contract
Dry feed loading
Minimum, typical and maximum dry solids per hour per operating cyclone
Separates realistic feed capacity from pump flow and nameplate
Feed size fractions
Mass held between stated apertures, with oversize and slimes included
Shows actual coarse loading and fine fraction at risk of misplacement
Target cut density
Particle cut with test method, size bands and allowed range
Distinguishes product partition from medium-density control
Partition sharpness
Ep and selected density points on the agreed sinks or floats basis
Exposes loss of selectivity that total product grade can hide
Medium specification
Magnetite or ferrosilicon grade, particle distribution and target feed density range
Connects separation to rheology, stability and magnetic recovery
Medium-to-solids ratio
Defined calculation at each guaranteed case
Protects part-load and maximum-load separation in the agreed hydraulic window
Pressure or head
Required local inlet value and permissible variation, with datum and slurry basis
Distinguishes vessel operation from a remote pump gauge
Outlet limits
Expected overflow and underflow slurry flows and solids distribution
Sizes launders, screens and medium recovery at the actual loaded condition
Wear criteria
New liner geometry, minimum wall or wear indicators by part, expected duty basis
Makes process degradation and shell protection inspectable
A plant can infer sharpness from calibrated density tracers where suitable tracers and recovery procedures are available, or calculate a material partition from feed and product sampling and float-sink analysis. Tracers can reveal behavior at selected densities and sizes, provided they are representative in shape and recoverable in the circuit. They are a distinct measurement from shipment chemistry, product size or valuable-mineral loss. If high-value particles are present in small numbers, test design must address the difficulty of measuring rare losses. Include a product assay method and the requirement for independent verification of the mass balance before acceptance.
Wear life, power and medium consumption should be reported on explicit boundaries. Power can mean the feed pump alone or the entire loop including medium recovery and water services. Medium use can mean make-up to the whole plant or residual medium adhering to products. An apparent improvement in one number can simply move costs elsewhere. A comparison of proposals is stronger if it states energy per dry tonne handled, the measured period over which make-up is tracked, and what grade and recovery were obtained at that time. Ensure the flows listed for the plant's pumps, screens and water circuit are internally consistent with the proposed cyclone setting.
Screen and filter duty farther downstream can govern allowable product moisture and availability. A filter press may handle fine slurry needing a drier handled cake. A vacuum belt filter may be appropriate where continuous cake handling or washing is required and tested. A rotary vacuum filter is another process-water and solids-handling option for a suitably filterable feed. The cyclone's job ends at its two slurry outlets unless the contract expressly includes these services. Avoid using excellent filter performance to infer that the cyclone achieved the intended density separation.
Chapter 5 / 06
Selection, Testwork and RFQ Scope
Start with a sample set covering planned operating conditions. Test the fresh and weathered ore if the two occur in the mine schedule. Separate unusual high-ash, friable or contaminated bands if a blend can put one of them into the wash plant at a material proportion. For a coal project specify clean-coal ash, yield or combustible recovery targets and the disposition of middlings. For a diamond project establish a conservative tracer and recovery proof as well as the required concentrate mass pull. For an iron ore project state the assay basis for both grade and recovery, including impurities that could force a penalty even when the iron assay meets target.
Magnetite is widely used in coal duties. Ferrosilicon can support higher-density suspensions in suitable mineral duties. Medium choice depends on the separation density, particle grading and rheology required for stability as well as compatibility with the recovery equipment. Ask for permitted contamination, magnetic recovery and make-up assumptions at a defined operating point. Identify whether fine medium is handled in bags or bulk and how it is added safely to the preparation system. A screw conveyor or a bucket elevator in dry make-up handling has separate requirements for dust confinement, wear and metering. Confirm the supplied limits for those interfaces before the mechanical layout is frozen.
Following the ore handling flow backwards often identifies how to hold feed conditions steady. A stacker reclaimer can be part of a blending strategy when stockpile planning allows it. The upstream apron feeder may address impact from coarse reclaim. The next belt conveyor has to transfer enough solids without pulsed surges that deprive the cyclone of its design medium ratio. Define the rate for the shortest window that matters to the surge body and the longest window that matters to daily throughput. In a brownfield change, collect operating records from the existing route before assuming average production shows that the instantaneous feed is within the current design basis.
A replacement cyclone project should ask the original designer, plant and bidder to reconcile available pump head, pipe wear margins, magnetic recovery and existing drain-and-rinse screens. Higher feed at the same circuit flow reduces the medium available per unit solids. Additional surface moisture on the feed can dilute the slurry. A bigger pump can place additional duty on an already constrained screen. The Multotec paper gives a case-driven discussion of why these changes matter to coal separation [2]. The useful deliverable is a case matrix with the vendor's predicted pressure, medium balance and separation behavior for the plant feed cases. It is a safer basis for choosing between new wear parts, present-size replacements and a bank redesign.
RFQ attachment
Minimum contents
Vendor reply to request
Feed characterisation
Dry solids rates, size-by-density mass distribution, assay and moisture range
Limits of characterized data and extra test samples needed
Process scheme
Stream destinations, used and new pumps, screened size split, density control method
Circuit balance and permitted constraints with alternatives noted
Separation basis
Target product quality, recovery, cut and performance method
Guaranteed case matrix with sampling and retest conditions
Mechanical layout
Elevations, inlet and outlet geometry, mounting steel, lifting access
Installation drawing, structural loads and required owner-supplied items
Operating envelope
Water restrictions, feed extremes, medium type and forecast hours
Predictive maintenance assumptions, suggested spares and controls I/O
The request for quotation should say whether the chosen vendor owns the complete separation duty or only the cyclone and liners. Put the existing pump curve and line arrangement, upper feed size, expected sinks proportion, medium balance and required cut on the same inquiry. Provide the normal and maximum rates with tests on the contiguous size bands the machine will see. Require the bid to state which results were tested, which were scaled, which are typical and which become enforceable. Ask for worn-configuration limits and operating instructions in the same document set. That makes it possible to compare a low-cost bare shell with a more complete package without guessing what commissioning and site engineering will add.
Chapter 6 / 06
Installation, Acceptance and Maintenance
A good arrangement starts with the manufacturer's orientation, support and discharge requirements. Check removable piping and direct access to the inlet head, spigot, vortex finder and any liner access joints. Put predictable wear spools where a crew and lifting device can reach them without removing the entire cyclone. Keep the pressure measurement accessible and protect instruments from plugging and abrasion as specified by the instrument supplier. A firm mechanical connection can impose loads the body was never designed to carry. The drawing should identify separately supported piping, filled weights, disassembly clearances and the load ratings for approved lift points.
Check free discharge and the intended operating air-core conditions when the cyclone is connected to its launders. A flooded or pressurized connection can change outlet hydraulics. Include the sampling stations and safe means of reaching them in the original layout. A sample taken from an unrepresentative corner of a launder can bias the reported size or density fraction. Plant mechanical and safety personnel should approve the locations for inspection, drainage and isolation before working drawings go out. The connection and isolation plan needs to account for the height of stored slurry, trapped pressure, suspended loads and solids that settle in dead legs.
Commissioning should distinguish the equipment checks from the process proving period. Before qualification with solids, establish correct instrument scaling and confirm that the indicated flows refer to the agreed process points. Then prove stable operation with representative material and otherwise agreed feed conditions. Take coordinated feed and product samples over the qualification window, document the wear parts installed and record any downtime or feed disturbances. Repeat the run at the capacity and difficult-feed cases the procurement plan requires. Put procedures for trial disruptions in the contract before the trial. A shift missing its feed window should retain its raw data and be treated according to the agreed retest criteria.
Operators should trend pressure at the cyclone, correct-medium density, feed rate and any available outlet or product indicators. Pair those trends with periodic samples and a component wear log. A shift in product quality without clear breakage can arise from a different washability curve, a change in medium offset, worn or obstructed outlets or biased sampling. If one cyclone bank behaves differently while feed and medium are shared, compare distribution, pressure, orientation and as-installed geometry before blaming the material. A plant can extend inspection intervals only when the record shows the geometry is still suitable for the required partition and mechanical integrity is being verified.
Maintenance acceptance should include measuring actual critical openings and tagging parts with fit and liner grade. Inspect the feed entry and outlets under the responsible site's isolation and access procedures. Refit spacers, inserts and spools of the approved geometry and record any deviations. A physically interchangeable insert from a previous design can produce a different partition when its bore changes. The spares list should differentiate parts an operator can inspect from complete replacement units that require a planned lift. Tie expected material usage, condition limits and inspection labor to the same cost estimate that justified the equipment, so wear economics can be reviewed after a comparable run.
Documentation normally includes the process and instrumentation drawings for the supplied system, conformity and material documents required by the destination, and explicit instructions for inspection and maintenance. Applicable site and jurisdiction requirements depend on how the assembly is classified and integrated. Ask each bidder to list the governing requirements and its scope rather than copying a standard designation from a different pressure or piping item. The plant owner should establish the legal duties for foundations, slurry containment, guarding, maintenance access and sampling. Final turnover includes as-built drawings and a visitable record of the pressure, medium density, throughput and partition achieved during the witnessed trial.
FAQ
Is cut density the same as the density of the medium going into the cyclone?
Cut density is the particle density at which the two outlets each receive half the particles of that density under test. Feed medium density is measured in the incoming suspension. The offset between them can vary with cyclone geometry, operating conditions and medium properties. Record both values from the same test window when comparing settings.
What are floats and sinks in the discharge?
Floats are the particles reporting to the overflow in the lower-density product. Sinks report to the bottom spigot. The product with commercial value depends on the duty. Coal plants commonly value the floats, while a mineral preconcentration duty may value the sinks. Both streams carry medium that needs to be drained and recovered.
Why is near-density material important?
Particles near the operating cut can end up in either product when separation has finite sharpness. A feed with a large mass in the specified near-density band makes product grade and recovery more sensitive to small shifts in the actual cut or in separation sharpness. State the width of that band when submitting washability data.
Can I size the cyclone from tonnes of solids per hour alone?
Request sizing at the actual medium flow and head, feed size distribution, sinks load and target cut. The solids rate alone omits much of the fluid the vessel needs to process, as well as the capacity demanded from the spigot and downstream screens. Ask for the dry solids and total slurry throughput separately.
What does the magnetic separator recover?
It recovers the magnetic medium solids such as magnetite or ferrosilicon from the dilute stream generated by rinsing product. It is part of the medium return circuit. The cyclone delivers the ore or coal density split. A circuit balance should show how much medium is recovered, returned, lost and replaced with fresh material.
Which parts wear most often?
Inlet, vortex finder, lower cone and spigot are typical areas to inspect, with the pattern affected by mineral abrasiveness, slurry velocity and installed lining. Compare actual dimensions with the vendor's approved wear limits and correlate wear with changes in product partition. Document the fitted geometry each time the cyclone receives a new wear part.
How should capacity and separation be accepted together?
Test the guaranteed feed and medium conditions at the specified rate. Sample feed, floats and sinks on the same basis, evaluate partition by size and density, and demonstrate both product performance and a reconciled mass balance. Record pressure and medium data for the same window. List any unstable conditions using the agreed retest rules.