Plasma Cutter Specs for Landscaping Fabrication: 2026 Selection Map
Landscape fabrication work (gate frames, planters, fire-pit rings, rebar assemblies) needs a 30-50 A dual-voltage plasma cutter with 1/4-1/2 in mild steel clean-cut capacity and a 60% duty cycle, matched to a portable 110V/220V supply and a 4-6 CFM compressor.